I've bid on a few curved jobs that would have used this board and I finally got one of the jobs. I know the basics of using the material. Make a dado and a horizontal rib with the shape of the project and combine them. What is the best way to attach the FlexBoard to the rib? A few ways I suppose, nails, staples, screws or just glue and clamps. I was figuring slather on the glue and attach it with staples. I'm using 3/4" FlexBoard and making a 5/16" dado/tongue for alignment. Normally I'd think of just using a full width dado (3/4") for the rib but the ribs will be flush with top and toekick. Just to make things simple I did the center with the same 5/16" dado.
So, has anyone used this stuff?

Click here for higher quality, full size image

"Photo by Leo G "

Forum Responses
(Architectural Woodworking Forum)
From contributor S:
I have used this material many times and glue and staples work well.

From the original questioner

Click to View Member Profile Shop Gallery Project Gallery Categories

Every 2-3" sound like a plan? What about filling the holes, is it required? I'm using vertical grade laminate and a 20 mill paper backed sapele veneer.

From contributor F:
You want staples, nails will pull right through that stuff! You just need enough to pull it into place until the glue dries, that's where the real strength comes from. You won't need to fill the holes for laminate. For veneer Iím not sure.

From contributor K:
Staples? I can't understand why people are advocating the use of such methods as they surely won't withstand the test of time.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Architectural Millwork

  • KnowledgeBase: Architectural Millwork: General

  • KnowledgeBase: Cabinetmaking

  • KnowledgeBase: Cabinetmaking: General

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2017 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article