Adhesives

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Beginners edgebanding questions

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Beginners edgebanding questions

12/9/19       
Bill Kugler Member

Hey everyone,

Long time lurker in these forums, first time poster.

New to the industry (sort of... long time carpenter, built my own kitchen, impressed people in my circle of friends, now attempting to branch out into cabinetmaking as a side business to my day job).

I've been fortunate enough to pick up an edgebander at a steal of a deal (Virutex eb-135), and it works well for my purposes, but it came with very poor documentation, and I have some questions, not really about the machine, more about banders in general.

1.) How often should I clean the glue pot/replace the glue? Obviously as this is a side job, I am mostly working with small batches of banding (a few cupboards at a time, maybe a kitchen).
How do I know when it's cooked?

2.) I've read about the stick method for cleaning the pot, but how do I clean the tube that feeds the roller? Do I just remove the glue (with the sticks), heat it up again and let the bit that's in the tube run back into the pot? Again, the instruction manual is fairly... abbreviated when it comes to cleaning and maintenance.

3.) The bander came with a bag of glue which is coming up on it's expiry date in Feburary of 2020. It had been stored in the bag which was open to the air (I assume, because that's how I received it). Should I just toss it and start a new bag? Are there any visual indications in the pot or on the panel to indicate the glue is done? Or will the banding stick initially and end up failing down the road, causing me hassles?

4.) How hard should the banding be to pull off the panel when I do a pull test to check coverage? Should I expect it to destroy the panel edge when I pull it? Or just pull some fibres out of the chipboard core? I'm just not sure exactly what I am looking for, being used to iron on banding that seems to fall off when you look at it the wrong way.

And can anyone suggest a good resource for these sorts of queries? A website or reference manual or something? Unfortunately edgebanders aren't really part of the DIY or hobby woodworker scene, so it's not like there's a tonne of websites out there with advice or guidance.

Just looking to get the most out of the bander and make sure it lasts (the glue pot, roller and tube have all been replaced from the dealer I bought it from, because the last owner was fairly hard on the machine).

Thanks!

Bill

12/11/19       #2: Beginners edgebanding questions ...
Mark B Member

No bander aficionado here but from my brief knowledge,

1. It will be difficult to say how often to clean. How often do you use, do you keep the bander covered/clean/dust? It would seem with very little use you'd have to clean when the glue in the pot hits expiration, hard to tell.

2. No idea

3. From everything I have ever been told/read, if the glue is kept covered/clean its likely good. Open bag, dust, not sealed up, probably best to trash it.

4. We run a cartridge bander and you will struggle to pull the banding off with vise grips though a lot of that depends on many factors. Substrate, how your cutting your parts, how quickly you band after cutting, and so on. Again, there is no single rule. MDF core hangs on like crazy, PB less, VC a bit more.

It would seem to me starting out you'd ditch the old glue and start new unless you feel very comfortable about the unused pellets you got with the machine.

If you want to cut some teeth and burn up some free material while you work out the kinks build a bunch of shop cabs. Melamine is about as cheap as it comes. If the glue is getting crispy best to burn it in your own shop as a test.

Good luck.

12/12/19       #3: Beginners edgebanding questions ...
Jeff Member

1.) Clean it out now and start with what you know to be good clean glue. Take note of the color, it will darken if its cooked.

2.) Stick method works well to get the majority of the glue out. I usually scrape what else I can out when the glue is at about 150C. Cooler than that and its too hard, much warmer and it just falls off the scraper. Only use wood to scrape the gluepot.

3.) Old glue will perform with sporadic results. Sometimes fine, some will just not stick. Go ahead and get a new bag. I've had much better luck with Dorus than with Jowat.

4.) It should peel fibers off the panel. 99 percent of what we do is pvc on particleboard core. This may vary based on what youre running.

12/15/19       #4: Beginners edgebanding questions ...
Bill Kugler Member

Thanks everyone who replied! I seriously appreciate the time taken, as I'm sure you're all busy people.

My bander is a fairly low speed, low temp deal (4 m/min, 392F max temp). Jowatherm 280.30 is the recommended glue from Jowat... anyone have any idea what the corresponding Dorus glue would be?

I think I am going to throw out the glue that came with the machine, as it's not even on the recommended glue list, and does not fit the specifications of the bander (Jowat 288.60). It works, but the bond is not as strong as I imagine it should be (nor as strong as I'd like it to be on something I'm selling to someone else, and hoping to not have to service).

Also, for anyone in Ontario, Canada specifically (if there is anyone), where do you get your glue?? All of the suppliers I have used for melamine sell the two common types of Jowat (288.60 and 280.30), and that's it.

Will

12/19/19       #5: Beginners edgebanding questions ...
Mark B Member

Not sure your low temp. We are only about 10 degrees higher. I would think the Dorus 217 is the standard mid all around. We run Jowat (but cartridge) and never an issue.

Wurth has Doellken 217 if you have access to them.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)