HELP....I am trying glue cedar to metal outside

12/23/14       
machshnell Member

I have possibly a foolish project i am starting. I have a bunch of old cedar 3/4" boards, red cedar, that i have planed to 7/16" and i am wanting to glue to metal garage doors. i have three metal skinned baked on paint smooth insulated garage doors. I want to veneer the half inch cedar to the face of the doors. i was planning on using some 1" (stainless) finish nails and a ?mastic or glue that i could trowel out with small grooves and attach cedar. I have read about just caulk (3m 5200) and pl products but i thought a trowelled out mastic or glue that covered the metal door would add a layer of protection for the metal as well. I have also heard about the cedar moving and the metal moving differently? Not sure if an issue to have some flexibility between substrate. Not sure the best approach to this. i have a lot of time in planing and joining and want to do this once and not deal with delam. Any advice would be greatly appreciated. thank you

12/28/14       #2: HELP....I am trying glue cedar to m ...
Adam

Some people might call this a "fool's errand".
However, luck seems to like fools from time to time. You might be the one.

3M 5200 is one of the best adhesives for bonding totally different materials. I would use this as the adhesive. More is not better. The trowable adhesives that I know are pretty average compared to 5200.

I would use as few mechanical fasteners as possible they may cause problems. What type of joinery were you planning?

12/28/14       #3: HELP....I am trying glue cedar to m ...
machshnell Member

thanks for reply. I have planed all the boards to 7/16" and i am going to slot or "groove" all the edges with a 5/32" slot cutter and make 1/2" splines. and i guess glue one side of the spline into boards and let the other move?? not sure on that. any advice? I would rather not use mechanical fasteners for the difficulty added to the process and the ability to rust.


View higher quality, full size image (747 X 1328)

12/29/14       #4: HELP....I am trying glue cedar to m ...
David R Sochar Member

All the local 'custom' houses have had garage doors made with cedar ticky-tackied onto them by site carpenters, laborers, and even some overhead door companies. PL400, a circular saw and a drill/driver were the tools used. The favored/required design is to mimic carriage house styles.

Then, in anywhere from a week to a year later, one or two or three boards fall off, get lost or driven over, and new cedar goes in. Then a few more. Some seem to last a few more years than others, but most get replaced with a new plastic or metal doors.

Failure is inevitable.

Besides ignoring the basics of wood construction, The doors weigh 2-3 times the original weight, and the .49 cent hinges bend and deform, causing misalignment and further problems. Tracks and motors are not sized for the additional weight and fail early. The lack of drainage consideration at panel joints allows water penetration, and a freeze thaw cycle then pries them loose.

It is better to redesign so the doors can be made sectionally in solid woods, and then use approved construction methods for building. Water must be dealt with at every point.


View higher quality, full size image (2592 X 1944)

1/3/15       #5: HELP....I am trying glue cedar to m ...
Steiph Zargon Member

Hmmmm... so the doors in question are "Man" doors like the one in the background of your photo... NOT the big "car" doors that open up with a mechanical contraption???

Seems to me you are certainly on a fools errand. I would rather just paint those robust metal doors with a nice oil based epoxy or poly. and save the wood for a deserving project. Making nice boxes or a blanket chest comes to mind.

If you want to make a fabulous wooden door then buy some 8/4 Cedar and fabricate the frame and use the wood you already have to make the panels. WOW that would be awesome!

Not sure what it would look like if you attach it to the face of the existing door(s)?. ;-{
And just how would you attach the door handles and locks, given the added girth you giving to the door?

So, if you are determined to do this.. I think a combination of high performance glue and mechanical fasteners would be best. If you don't want to see the fasteners... countersink the holes and make plugs of a contrasting wood and give it some extra flair.

Good luck!


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)