Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Please help a newbie by recommending the correct router bit

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Please help a newbie by recommending the correct router bit

8/15/18       
Marc Member

Please help a newbie by recommending the correct router bit shape. Here's some background about the project. Mom has several doors in her house that rotted. It seems that whoever assembled the doors did not paint the edges of the door slabs, and the doors did not hold up to the weather on the gulf coast. Most of the doors that have the problem are fixed French patio doors. They do not move but look exactly like the few doors that do move. For this reason, we feel the they can be repaired without too much worry since these fixed doors will not swing at all.

These painted exterior doors are 30 years old and were made by a company that is no longer in business. Each door has thin rails and stiles with one double glass pane. We've repaired a couple of doors just by using 8/4 fir boards to replace the rotted bottom and top rails. While dowels have been sufficient, we would really prefer to find a router bit with 1/2" shank to make the nice grooves that the original doors had in addition to dowels. The photo shows the door slab viewed from the top so you can see the joint (highlighted by the blue box) between the rail and stile.

We can't seem to find the same bit that the door manufacturer used. We're new at this and don't know which other styles of bits can be used. Can anyone tell which router bit is acceptable for joining rails and stiles of this thickness? Would it be a finger-joint bit? Is there instead a rail and stile bit for this wood thickness (1.75" actual thickness)? Now that you see the joint between the rail and stile, do you think the dowels are enough and perhaps the groove is unnecessary?

[This was also posted at Woodworking Talk.]


View higher quality, full size image (2592 X 1456)

8/15/18       #2: Please help a newbie by recommendin ...
JeffM

I could be wrong, but I don't think you'll find a router bit to duplicate that entire cut. Looks like you'll need a custom moulding head.

8/15/18       #3: Please help a newbie by recommendin ...
rich c.

Too big for a router, you need a shaper.

8/16/18       #4: Please help a newbie by recommendin ...
D Brown

With several cuts on the table saw perhaps

8/16/18       #5: Please help a newbie by recommendin ...
David R Sochar  Member

Door manufacturers do not use router bits.

You will have use your abilities to make do.

Custom profiles for router bits can be made by several advertisers within inches of these words.

What is your budget for the doors - time and materials?

8/19/18       #6: Please help a newbie by recommendin ...
Marc Member

Thank you, JeffM, rich c, D Brown, and David Sochar, for your responses.

Mr. Sochar asked a question about the budget and materials. Since the doors are not readily available for purchase, we've been spending a week or more on each door when using wood dowels to join the rails and stiles. Also, we've been putting around $110 worth of new wood, including red oak for sills and douglas fir for the new jambs. At one time we repaired the slabs with Spanish cedar, but it was expensive at $8 per board foot, so now we buy rough-sawn fir from a lumberyard about an hour's drive from here. Then we fill the knots with epoxy, plane the board, sand it, coat with shellac to prevent resin from coming through, then we paint it. The fir is less that $3 per board foot, so the red oak (~$7 per board foot) is still the most expensive part.

Do you think the wood dowels will be enough to join rails and stiles? Getting the pieces perfectly flush before gluing is a real challenge. Any advice?

8/19/18       #7: Please help a newbie by recommendin ...
Larry

I would use white oak rather than red. More rot resistant! $7/bd ft,!! Way more than we pay.
Notice that the doors were stave core and thick veneered. Usually helps with warpage/cupping on exterior doors.

With a little care you can do those cuts on a table saw. In my shop we would produce the lineal cuts on the molder and the copes on a shaper. Lots of doors are made with 5/8" dowels. You might be able to use a router table for all the cuts but it will take quite a few passes and require making a jig for the copes. I'm guessing you don't have a power feed so your cuts will be less than ideal but that's what sand paper is made for, right?

Clamp the parts together, dry, and through drill the dowel holes.

8/20/18       #8: Please help a newbie by recommendin ...
The Cajun Craftsman Member

There are exterior door router sets to be had. You need a beefy router in a table to use them. Infinity, Freud, Whiteside, etc. all have them. Just search for "Entry & Interior Door Router Bit System".

Click here for Search Link

8/30/18       #9: Please help a newbie by recommendin ...
Steve Member

You might find an alternative productive source of info. in the Canadian WWing forum, https://forum.canadianwoodworking.com/forum?_ga=1.38950241.3131736.1427465266

I
say productive only in that while the members there, many are professional/commercial and all sorts of others will simply have more available time to go back and forth and discuss your issues, since you say you are learning.

There are of course domestic U.S. forums also to post on. Feel free to send me a PM if you wish to discuss.

8/30/18       #10: Please help a newbie by recommendin ...
Steve Member

Check Whiteside router bits, download their catalog.
https://www.whitesiderouterbits.com

9/1/18       #11: Please help a newbie by recommendin ...
Steve Member

Marc, I may have a solution for you. Whiteside for example has the same profile bit set but the proportions won't match as they are for ¾" or 1" stock.

Save the expense and labor of trying to match and cut router bits, particularly since the doors won't be opening. I have used RSS structural screws for a half dozen such doors I made for use as patio architectural gates/doors. Google GRK fasteners, RSS structural screws (#30 bit), and they are carried at Lowes, Depot, and other fine concessionaires. Use a 5/16" x about 6" or 7" drilled and countersunk from the side edge. You can then countersink a &#8541;" or 3/4" head and fill it with a piece of dowell rod cut as plugs.

Far easier than the routed attempt. I'm a little slow this morning to try to take and upload pics but if you want them I will., if ? let me know.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery