Safety Speed Cut Thermwood Corporation ECabinet Systems

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Biesse vs Holzher vs Time Saver

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Biesse vs Holzher vs Time Saver

6/17/16       
Mike M Member

We’re currently looking into buying an edge bander and a 43” dual belt sander. Beyond the particulars in specs, which I think we’ve narrowed down sufficiently, we’re really having a hard time choosing a manufacturer.

Some concerns aired here and elsewhere state that both Time Saver wide belts and Holzher edge banders have not lived up to their former glory in recent years and that is obviously a huge concern for us, that and their ability to satisfactorily support us with maintenance and repair in the future. Our concern with Biesse, for both an edge bander and a wide belt is that there is very little in the way of any feedback, all-be-it the little feedback here is good.

FWIW, as an aside, Stiles has been, shall we say, aloof in their sales approach as I have yet to get even a phone call after my contacting them on two separate occasions. Needless to say, we’ve lost interest in them.

We purchased a CNC from Biesse a year ago and are very happy with their support. While our machine had some major hiccups, they kept at it and fixed the machine which has been working for 10 months now without so much as a squeak. So I know their support is good, they stand by their product, but is their product up to snuff.

I understand that it’s in the manufacturers to scrub bad press from the internet, with that, please send me any feedback you have via the contact link that is linked to my email address.

Thank you in advanced for your time.

6/18/16       #3: Biesse vs Holzher vs Time Saver ...
Derrek

Had a holzher bander and hated from the day I got it. People love them or hate them.
Now have a biesse and have zero issues (other than its an edgebander that requires that you love it by keeping it clean and maintaned)

6/18/16       #5: Biesse vs Holzher vs Time Saver ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com

I don't know squat about edge banders.

There's a company out of Minnesota that sells a widebelt almost identical to what Timesavers sells. Their website sucks, but I've had a dual head 43" machine from them for about a year and a half and I'm very pleased with it and their customer support. It was substantially less money than the Timesavers model. I'm in Minnesota, that played a huge part in what machine I bought. Proximity to parts and technicians is important to factor in.

http://apexmachinegroup.com

I dealt with Jon Hill. Decent enough guy. My machine got caught up in the labor strike at the ports on the West coast and took a while to show up. Not their fault though.

I would recommend going with the longer belts. 103" vs. 75". The way I run mine is pretty hard on abrasives, but burning up paper is still cheaper than more machine time. I think the longer belts would improve that.

6/20/16       #6: Biesse vs Holzher vs Time Saver ...
Matt Krig Member

Website: http://www.northlandwoodworksinc.com

We purchased a new sander late last year and had some great advice from a trusted fellow shop owner I'd like pay forward. Buy a big sander, huge infact. 53"-3 head and you'll never look back ( I know it seems crazy and way too expensive right?). The footprint is negligibly larger, the extra capacity pays dividends. A year ago, I would have laughed at the reasoning for anything over 43. We are running the occasional full sheet through, large face frames, all kinds of parts, plus with a larger belt width we all get a lot done in less time.
We do frame, Euro, laminate, whatever as well as make a lot of doors.
There was a lot of jargon I really didn't understand until we had the machine in place, that's where I'm grateful to have had a very helpful friend introduce me to a machine class and a rep that changed our approach to sanding.
Here are a few considerations and things learned-
1) constant pass line- feed table/infeed belt never moves- machine frame adjusts up and down. Much more accurate and predictable as well as infeed and outfeed tables always work.
2) Drums/ platen combo. Steel on the first drum- it's bombproof and will make your second rubber contact drum last much longer meaning better sanding. Finally a combi head- this means belts running on a segmented platen which means customizeable sanding if you are ever doing veneer, sealer sanding (huge time savings) and finally prep sanding for finishing with a light hit from the rollers and platen combo.
3) Get a machine that reads and adjusts for the parts coming in- this is gold and will pay for itself in belts and machine abuse and wear avoided.
4) Use a digital caliper to set up the sander, don't mess with the onboard measuring thing unless you have smaller parts that are pre- calibrated. It's foolproof this way.
much less costly and more consistent paper belts with air blasts to cool them and good calibration sanding or tight specs on incoming solid wood will make the belts last a ridiculous long time. Most of our belts fail from edge tears from loading and unloading.
The quality of the parts coming out of this machine means significantly fewer labor hours to the point where I believe in a 8-10 guy shop we will safely cover the extra cost for a machine larger than what I originally set about to purchase.
Lastly, the creature comforts are just an added bonus- a saved program for nearly everything in a very custom shop, a practically dummy proof system, and finally, it's super quiet to run.
The down side is the large amount of compressed air and dust collection needed if you're not already set up for it.
The initial cost creates some initial reservation, but money is cheap right now and labor is scarce and our biggest expense, so it makes sense to invest in equipment that will get more done.

6/27/16       #7: Biesse vs Holzher vs Time Saver ...
Adam West  Member

Website: http://www.surfprepsanding.com

Choosing a wide belt sander correctly can save your company the cost of the machine per year, for every year you own it. You pick the wrong one and it will cost you more than the cost of the machine plus some.

I cannot advocate for one machine company over another as it would alienate my friends at each of the machine manufacturers.

If you would like to email me I can give you a very solid understanding of how you will actually utilize your machine for the best results possible, and this will undoubtedly help you understand which machine will work the best for your requirements.

I can state publically that you defintely want a machine with dead shafts and air exclusion on each sanding position. If you buy a two head make sure it has a drum and combi-head. The machine weight has absolutely nothing to do with how "heavy duty" it is.

Avoid salesmen who promise that a machine will do every single job perfectly and do not let them sell you what they have in stock rather than what you actually need.

My job is to travel the country for my employer and teach people about sanding. I specialize in wide belt machine and have personally worked on over 1500 wide belt machines in my career.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello