Safety Speed Cut Thermwood Corporation ECabinet Systems

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Manually applying PVC edge banding

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Manually applying PVC edge banding

9/21/20       
Mark B Member

We have an odd situation where we need to apply some 1 3/4" .018" PVC banding to some parts we cant run through the bander. Running a few test with contact the adhesion is not great at all. You can peel the banding off with moderate force and while the contact stays on the banding a bit it peels off consistently to where the back of the banding is just as clean as it was off the roll. Banding supplier doesnt have much to add stating that contact should be fine. Wondering if anyone has any input. All the standards, even application both surfaces, plenty of dry time (to the touch), warm, new material.

9/21/20       #2: Manually applying PVC edge banding ...
TonyF

Mark B:

I'm guessing that you can't use the bander either because the piece is too big or the edges are not straight, or have some kind of angle.

You don't say how much of this you have to do, but what you might try is to have one person put down a bead of hot melt glue (craft store type) ahead of another person who follows with the edgebanding and a roller. It would be tedious (and messy), and might take some trial and error to get the right pace, but it might work.

They used to sell a pvc banding that had double-sided tape applied to it, and you peeled off the barrier paper as you rolled the edging onto your piece. I wonder if a strong double-sided tape like was on that banding might not work in your situation.

Hope this helps.
TonyF

9/21/20       #3: Manually applying PVC edge banding ...
Mark B Member

Thanks Tony,
And yes to the bander issues with these parts.

Hadnt considered a hot glue option but without trying it it sounds like something that would be pretty iffy and most definitely messy as you say.

Doing a bit of head scratching as we've rarely had to contact PVC before and never an issue. Never thought it would be a problem and even calling banding supplier they say "its done every day" and dont know what the issue would be.

We could have brought this banding in peel and stick, which in hindsight may have been a better option, but Ive used peel and stick many times as well as Fastcap's fastedge tape or whatever its called and Ive never been impressed which was why opted to just lock it down with contact.

Thanks

9/21/20       #4: Manually applying PVC edge banding ...
Brian Clancy

Website: http://clancywoodworking.com

Mark
we use a hand held glue pot for curved or radius surfaces by Virutex. Works great.

https://www.virutextools.com/hot-melt-portable-edgebander-peb250-pid291

9/21/20       #5: Manually applying PVC edge banding ...
Mark B Member

Thanks Brian,
The angles on these were the reason didnt use a contour bander.

9/21/20       #6: Manually applying PVC edge banding ...
TonyF

Mark B:

Don't know if you are using water-based contact cement; if so, you might try the solvent based instead. If the glue pulls off of the substrate, you might try double-coating that. Perhaps aggressively sanding the back of the pvc edging before gluing might help as well.

Sorry if I have stated the obvious, but I know I have been in situations where the obvious sometimes gets overlooked.

Good luck.
TonyF

9/21/20       #7: Manually applying PVC edge banding ...
Mark B Member

Tony, stating the obvious to me is perfectly fine. Im thankful for your input.

No water-based. All solvent.

Substrate seems to be fine. Banding so so. Supplier stated to not in any way sand or abrade the banding that its primed. In tests we cut one back hard and cpntact anyway, not much better. We wouldn't deviate from manufacturer spec regardless.

9/22/20       #8: Manually applying PVC edge banding ...
james e mcgrew  Member

Website: mcgrewwoodwork.com

use a laminate or phenolic paper first then apply the PVC with contact

9/22/20       #9: Manually applying PVC edge banding ...
Tom Gafgen

Two thoughts , try a very light first coat on the banding with a very long dry time before a not too heavy second coat to re activate it and or maybe try some other brands of glue .

9/22/20       #10: Manually applying PVC edge banding ...
Jack Mazzuchelli  Member

https://edgecoinc.com/peel-stick-edge-banding-pvc-wood-veneer/. They have this in all brands,matching mica, wood u stain etc

9/22/20       #11: Manually applying PVC edge banding ...
Al

Years ago I did laminate doors that had a cove finger pull. I would put masking tape on the edge of particle board then run it through edgebander. The glue did not stick very well to the masking tape but adhered to the pvc banding. I would just peel the banding from the board and then heat gun it to the cove on the door. Some masking tapes work better for this than others. Maybe this would work for you.

9/23/20       #12: Manually applying PVC edge banding ...
Mark B Member

Tom,
Thanks, Thats pretty much what we had wound up doing. Doubling up helped. We also switched to a steel roller instead of rubber. Bigger job I'd ditch our old contour bander and buy a new one that would run angles.

Jack,
Appreciate the tips. We have run EdgeCo's peel and stick as well as Fastcap in a couple situations and Ive just never been impressed with the bond which is why we opted for contact. Even at the bond that caused me to post, the contact was tougher than any peel and stick we've used but keep it in my for sure.

9/23/20       #13: Manually applying PVC edge banding ...
Mark B Member

Al,
Thats a pretty impressive tip/trick that I will definitely keep in mind. Not sure it would have worked on these lengths but man that would sure be handy in some spots to be able to use the bander as a hot melt applicator. Im going to give it a try just for fun on some test pieces. Seems like it may be tricky to get enough heat for the bander glue but not foul the PVC.

Great tip.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • Veneer Systems Inc.
      Specializing in Veneer Equipment and Veneer Supplies
    • SAMES North America Corporation
      Precision Spraying Solutions From Pumps To Complete Application Systems-Design and Manufacture of Process Equipment Including Airspray, Airmix, Airless, Rexson Dispense, Electrostatic and Powder Coat
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Limtech Industries, Inc.
      CNC Routers, Machinery for Woodworking, Plastic and Other Non-ferrous Metal Machining Applications
    • CP Adhesives
      Supplying Quality Adhesives to the Woodworking Industry
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • Southeast Tool, Inc.
      High Quality Tooling at Competitive Pricing
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • O'Shea Lumber Company
      Merchants of Fine Woods
    • ULTI-BOARD
      The Ultimate Spoilboard - ULTI-BOARD - Specifically Engineered and Formulated for the Ultimate in Spoilboard Performance - Not Your Ordinary Sheet of MDF.
    • Onsrud Cutter
      Router Tooling for Woodworking, Plastic and Non-Ferrous Metal Manufacturers
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • Wood Doctor's Rx, LLC
      Wood Processing Seminars, Kiln Operators Seminar & Training, and Advanced Drying Evaluation & Training

    Become a Sponsor today!