Cabinet and Millwork Installation

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Wood Shower

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Wood Shower

5/25/16       
Mark

Was finishing up some work at a customers house when she asked me about using wood to cover the walls in her shower instead of tile.

My first thought was hell no, but said I would give it some thought. Figured I would get some opinions here. Tell me if this is an awful idea.

Was thinking of using Ipe, with the boards running top to bottom, and a ship lap or tongue and groove joint between. Would fasten the boards along the center with a water proof construction adhesive, and use a clear waterproof silicone in all of the joints, and to seal the perimeter. Should allow expansion and contraction.

Everything would be pre-finished, front and back, with an epoxy and spar varnish, essentially like finishing a boat. The varnish would need to be touched up every once in a while, but I think it would otherwise be pretty resilient.

Thoughts?

5/25/16       #2: Wood Shower ...
Jared Emery

I've seen wood bathtubs, but they were wetted out with fiberglass. If they can be done, why not a shower? Although I can hear Jeff Goldblum now: "they were so preoccupied with whether or not they could that they didn't stop to think if they should."

5/25/16       #3: Wood Shower ...
rich c.

Do they have hard water? I see a disaster trying to remove lime and soap scum off of wood. I sure wouldn't do it in my house. I hate cleaning the shower way too much to think about making that more difficult! Also the way wood works when it gets wet all the time, is to incorporate a way for it to dry out. Design a way for air to get all around it. Only expose it on one surface, and attempt to seal it, and somewhere water gets behind it and makes a mess.

5/26/16       #4: Wood Shower ...
Adam

Perfect project for faux wood grain solid surface

5/28/16       #5: Wood Shower ...
peTe Anderson

Website: http://petesfloors.wordpress.com

I have a wood shower that our family has been using for the past 30 years. I used a polyester/fiberglass pan. I pre-finished three sheets of one-half inch luan plywood
for the walls by staining with spice brown
Duraseal stain and three coats of moisture-cure poly-urethane. Installed the panels and used an inside corner mold in the back two corners, with a natural colored quarter ply ceiling. I have a fan/infra-red light/incandescent light fixture on the ceiling.
I have a Koa Jamb that mounts a glass door. After each shower the walls and floor are squeegeed, so no water spots, even though our water has 29 grains and 10 grains is considered hard.
The caulking for sealer is NP-1, at joints and behind the corner mould.
Some hard water/soap scum removers can damage the finish. Don't use a cleaner with carbolic acid , or phosphoric acid to remove scum.
Mc poly is extremely abrasion resistant, and water-proof. Water-proof silicone will prevent any type of finish from sticking if you ever need to add more coats of finish.

7/26/16       #6: Wood Shower ...
Mark  Member

I did a couple of showers in cypress some years ago, they sprayed a penetrating waterproofing on the walls and the owners seemed happy with the results

7/1/21       #7: Wood Shower ...
RobHRN

We did a lot of wood walls in bathrooms. Due to our practice, it's really hard to make high-quality waterproofing, depends on sort of wood first of all

7/2/21       #9: Wood Shower ...
RobHRN

Website: https://yournewtubs.com/

If you got any related questions, feel free to contact me anytime

9/19/21       #11: Wood Shower ...
SharpFrank Member

Hey, I understand what you feel. To my mind, using wood walls in a shower looks like madness. It's really hard to find a decent water-resistant wood. Another thing, it's impossible to clean it completely using a basic showerhead. In modern systems, high pressure is generally not available. So the option is to replace it to high-pressure showerheads. Review is below

https://bathroomer.org/best-high-pressure-shower-head/

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Elias Woodwork & Manufacturing
      Solid Wood Cabinet Doors, Furniture, Dovetail Drawers, Mouldings, and Related Items
    • CabMaster Software
      The Easiest Custom Cabinetry Software
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • Parts Cutter CNC
      CNC Cabinetry and Closet Parts
    • Steve H. Wall Lumber Co.
      Quality Hardwoods and Softwoods, Exotic Wood, Furniture Quality Plywood, and Hardwood Flooring
    • KCD Software
      Powerful 3D Cabinet/Closet Design Software with Built-In Touchscreen Mode for Mobile Use with Best Production Practices Including Direct to Cut List, Cabinotch and/or CNC Machining
    • WalzCraft
      Custom Doors and Wood Products
    • Cabinetshop Maestro
      Web-Based Project Management Software for Custom Cabinet Shops - Manage Jobs from Prospect to Punchlist Through Scheduling, Task Management, Time Tracking and Communication

    Become a Sponsor today!