Solid Wood Machining

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Thicknessing glue-ups: planer vs. wide-belt sander

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Thicknessing glue-ups: planer vs. wide-belt sander

4/22/17       
Sam A. Member

Hoping for some advice. Sorry for long post.

In the last few months, we've started doing solid casework (dressers and sideboards, mostly). Some of the designs have mitered corners. Though maybe not strictly necessary, mitered casework is much easier for us to execute if we sand the panels that compose the sides, top, and bottom down to exactly the same thickness. It's hard to do this on our stroke sander (and near impossible to do this using a belt sander), so we've been gluing up the panels in our shop and then taking them to larger shops in the area so they can be sanded to uniform thickness using their wide-belt sanders. As orders for our dressers/sideboards have increased, so have the costs associated with outsourcing the sanding/thicknessing on these panels. We're now paying hundreds of dollars a week to get these panels thicknessed, and we're realizing it's time we invest in a planer or a wide-belt sander so we can thickness the panels ourselves in-house.

Which one is more appropriate? We have 10-20k we're prepared to spend, although we expect in the next 6-12 months to be able to invest in additional equipment (maybe something to complement whatever we purchase now). One of the outfits to whom we send our panels has a massive, 3-head wide-belt sander (Timesavers). They're telling us we should invest in something similar, but those things are at least 30k (new), if not significantly more. If absolutely the right decision in the long run, we can probably get the money together. But wouldn't it make more sense for us to buy a 24" wide planer with a helical cutter head? Something that will flatten the panels down to uniform thickness. And then, if necessary, we can get a smaller wide-belt sander with a higher grit belt for finishing sanding? (Though I doubt we'll be able to get both a planer and sander for <20k; maybe we just pad sand by hand after running the panels through the planer). Grizzly has a 24" wide planer (new) that looks promising, though I'd love to hear other brand/model recommendations. It's possible to use wide-belt sanders for thicknessing panels, obviously, but I would have thought it non-ideal, if only because you end up wearing through the belts quickly. Here's one more consideration: we're beginning to do solid dining tables. Would be great to be able to use the planer for table tops, as well, just so the table top surface is even to the touch. But most dining tables are too wide to fit in a 24" wide planer. Do we necessarily need a larger wide-belt sander for these tops?

Other relevant information: our glue-ups are usually pretty flat. Very rarely need to take off more than 1/8", and usually it's closer to 1/16". This is all 4/4 surfaced by our lumber supplier to 29/32". Panels are only ever 21-22" wide (since our casework is a standard 20" deep). With the way orders are coming in, we need something that can comfortably thickness 5-10 glued-up panels (again, ~22" wide x ~65" long, max) per day. Not especially interested in buying used. Rather spend more on something we won't have to dump time into repairing in the future.

Thank you for your suggestions in advance!

4/23/17       #2: Thicknessing glue-ups: planer vs. w ...
Pete D

I do very similar work with solid wood panels and mitered edges and I process the panels using a 24" planer and single head wide belt with platen. My setup is efficient and works well for me however, I do less volume and use my planer for dimensioning lumber as well.

If your sole purpose is flattening panels I would focus on a multiple head wide belt or possibly one with a planer/sander configuration. These are expensive machines, but not really...For example, if you're spending $500 a week outsourcing this task, that's ~$20k in one year! And that doesn't involve the time to transport the panels between shops. If you think about a purchase like this over a few years the machine will pay for itself very quickly.

Wouldn't be too concerned with belt life, if you follow a recommended sequence of grit to stock/scratch removal they will last a long time. Adam West of surf prep has written informative articles about this.

4/23/17       #3: Thicknessing glue-ups: planer vs. w ...
Pete D

Btw, I used a conservative estimate at $500 for 40 weeks/year. If you plug your numbers in and add the transportation time/costs you may find your spending substantially more every year for outsourcing.

4/24/17       #4: Thicknessing glue-ups: planer vs. w ...
Hen Bob Member

If you have the space you should really have both, I would pass on the grizzly planer and look for a used more industrial machine.

Having the widebelt in house will quickly pay for itself, We recently purchased a 2 head timesavers and are very pleased with our decision.

4/24/17       #5: Thicknessing glue-ups: planer vs. w ...
Sam A. Member

Thank you both (Pete D and Hen Bob) for the suggestions. Immensely helpful.

Pete D-- I think your calculus is correct, and that making the investment in a planer / sander combination will pay for itself pretty quickly given our needs. (Doesn't make it easier to cut the check, though! This will be the most expensive equipment purchase we've made in a long time.)

Hen Bob-- Is your reservation with the Grizzly brand related? Or you just don't think it can handle production-shop volume? I guess it makes sense to spend a little more and get something we can grow into, so to speak...Would you mind saying a little about how your Timesavers has paid for itself? (Don't know what sort of work you do, so may not be relevant, but I'm curious nonetheless. Want to see what sort of value a two-head wide-belt could add to our operation beyond thicknessing panels.)

4/24/17       #6: Thicknessing glue-ups: planer vs. w ...
Hen Bob Member

As Pete D has mentioned your already spending the money to have another shop surface the panels and add the labor time to transport. Once you have it the uses for the machine are numerous , you will wonder why you didn't get one sooner

I have had quite a few Grizzly machines, they really don't compare with the true industrial versions. We have a 24" planer from the late 40's that will out run a Taiwan made one any day. That planer cost us less than grizzles 15" model.

4/24/17       #7: Thicknessing glue-ups: planer vs. w ...
Pete D

I'm not discounting the value of a large planer, but if short term finances are a concern and you're contemplating a multi head wide belt vs compromising to add a planer and single head wide belt I think you're better off adding the multi head first, especially since you commented about adding dining tables.

This is one of the articles I mentioned:

http://surfprepsanding.com/2014/02/28/the-ultimate-primer-on-single-
head-wide-belt-sanding-2/

If you look at the table in the article showing min/max stock removal per grit you'd be able to surface one panel down to 150 grit in one pass per side on a three head machine considering you need to remove 1/16"-1/8". The larger machine can keep up with your demands as you grow and can handle dining table widths as well.

I have no experience with the planer/sander wide belt configurations so I can't comment on the pros and cons vs a multi head sander.

My planer and single head setup works for me because 99% of what I do fits in the 24" planer and usually only takes one or two passes on the wide belt. I have the capacity to surface a 36" wide dining table top when necessary, but it's a lot slower with multiple passes and belt changes. Considering I rarely build dining tables it's not a big deal.

4/25/17       #8: Thicknessing glue-ups: planer vs. w ...
Woodworker Member

I bought 32" Industrial planer... and i think sander is more useful than planer in huge width like 32". U don't need planer more than 16".

4/25/17       #10: Thicknessing glue-ups: planer vs. w ...
Woodworker Member

For glue-up, why not 32" jointer ;). I use jointer for glue-up to ensure 100% straight.

4/27/17       #11: Thicknessing glue-ups: planer vs. w ...
Tom Gardiner

I would take a step back and fine tune your glue up process. I glue panels for doors 72 x 30 x 5/8" five to ten at a time that require minimal sanding after gluing. My process is long bed jointer planer then a saw tooth profile on the shaper that when set correctly will align boards within .005" . I stroke sand the excess glue. If you were to glue up with say .010" to come off each side then you could consider a single head sander. I wouldn't be without a big jointer though.

5/3/17       #12: Thicknessing glue-ups: planer vs. w ...
Adam West  Member

Website: http://www.surfprepsanding.com

The biggest trick to planing with a wide belt sander is keeping heat to a minimum. You can do the surfacing you desire with a single head wide belt.....all it takes is time. I would suggest you invest in a 36 grit belt to take the parts down to flat using only the drum on a single combi-head machine. Once you arrive at a flat surface you can change to an 80 grit, then 120 using only the drum, then do a finishing pass with a 150 or 180 grit with the drum and the platen. Use the chart in the article mentioned above and you can achieve a very satisfactory result. You are talking about 8 passes through the machine per panel. Taking the correct amount of material off per pass/grit is critical.

Think carefully at this point. Each pass, done well, will take 30 seconds to 1 minute per grit per panel. If you do them all at once it will go faster, but make sure you are not robbing yourself by saddling your shop with enough labor to pay for a nice 3 head planer sander.

4/2/18       #13: Thicknessing glue-ups: planer vs. w ...
Karel

Good day, More than 30 years ago we started by paying to have our sanding done at a larger company also. Getting our first sander (used Sandingmaster 2 head) was a financial stretch at the time. In the first week we had it we wondered how we went so long without our own. I think any solid wood furniture shop is making a mistake not to have a sander. If you buy a quality brand even a used 2 head or single head combination one, will suit your purpose. you will find that you will put almost everything you make through the machine. I have a planer in my shop now but I did not have one for more than 25 years it was unnecessary. We purchased premilled lumber like you and edge glued it.
When I still lived in the states we could sand 150 tops a day with the old sandingmaster. If you can, purchase new for the warranty and service, but buy from one of the well known makers. but do not be afraid of an older good running machine after all a used sander is sanding your panels now. One of the most useful accessories you can get for your sander is a roller conveyor to return the sanded panels for another trip through the machine. Also do not forget you will need proper dust collection. I do understand a new machine can be optimized for your particular work but even one not 100% optimized for you is so much faster than any other method its still worth having. I seem to remember reading in one of the trade magazines years ago that one hour in a wide belt is worth 30 hours by hand. happy sanding

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)