Solid Wood Machining

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Widebelt Sander Help Needed

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Widebelt Sander Help Needed

6/30/19       
Larry

Website: http://www.superiorcabinetryandmillwork.com

Hi,
I have a 1984 model A.Costa (not Costa and Grissom) 43" widebelt sander. This sander has "fixed" pinch rollers on it. It doesn't have spring loaded pinch rollers. The issue that I'm having is that sometimes the sander will leave a slight dip on cabinet doors that I run through the sander. The slight dips will be either on the leading or trailing ends (Im not sure which). Do you guys have any idea what is causing that and do you have any ideas about how to fix it? Do you think it might have something to do with the adjustment of the pinch rollers? Or, do you think it's caused by the fact that the rollers are "fixed" and not spring loaded? If the problem is caused because the pinch rollers are not spring loaded, is there a way to possibly convert my "fixed" rollers to spring loaded rollers? Thank you for your help.

7/1/19       #2: Widebelt Sander Help Needed ...
rich c.

Don't you think it is past time to retire a 35 year old machine? You aren't saving any money if you have to rework product!

7/2/19       #3: Widebelt Sander Help Needed ...
Larry

Nope. Not planning to retire this machine. It's still a great machine with plenty of life left in it. It just needs some adjusting. I have plenty of older industrial machines. I prefer the older equipment.

7/3/19       #4: Widebelt Sander Help Needed ...
David R Sochar Member

Logic. Just a bit of applied logic.

First, what you are seeing is a snipe. Not like chasing one in the woods, but a snipe - fore or tail. You run moldings, so you have seen snipes before on moldings, usually tail snipes. Planers will also snipe, fore and or tail.

Second - determine for certain what you are seeing on your doors - fore snipe is the first leading edge of the panel. Tail snipe is the last.

Now, for logic. Measure how long the snipe is. Not how wide, but how long. Lets say 5" tail snipe. Now go to the machine and open it up (power off, 100%) and visualize your panel feeding thru the machine. Take a thin stick, mark 5" on it and 'feed' it thru. Where the 5" mark is on the abrasive wheel (the sanding cylinder), you will see the end of the stick coming out from under the holdown roller. This allows the tail of the panel to rise into the abrasive.

Careful observation will tell you what is happening. Careful analysis of these events will help tell you what to do.

It ain't simple, but it is a good exercise in logical thinking. The age of the machine would lead me towards a bearing problem/solution, but that is not a given.

7/3/19       #5: Widebelt Sander Help Needed ...
rich c.

Snipe on a planer comes from the stock moving around until it hits the chip breaker or outfield roller, or both. I'm having trouble visualizing how a pinch roller would work without a pivot and springs. How would the infeed pinch roller work when you have it all set to remove 1/32" and then move the bed to remove 1/64"? Doesn't that mean you now have 1/64" clearance under the roller? Also what happens when you change grit? An 80 grit belt is much thicker than a 120 grit. Are you constantly changing the roller positions? How long have you owned it? Has it always done this?

7/7/19       #6: Widebelt Sander Help Needed ...
Larry

Thank you, David. I'm going to determine whether it's the leading end of the trailing and of the doors that has the snipe when I run my next batch of doors. And, I will do what you suggest about using logic to determine when and where the snipe is occuring. Apparently, this sander was built before they started putting spring loaded pinch rollers on wide belt sanders. I have wondered if not having spring loaded pinch rollers has been the main problem with the snipe issue. I have thought that the spring loaded pinch rollers would easily let off the tension as the door passes through. Whereas a fixed pinch roller is not going to easily let off the tension. I have wondered if it's possible to convert my fixed pinch rollers to spring loaded rollers. Have you ever heard of anyone doing that? Thanks again for your help.

Rich, it's been a while since I set the pinch rollers. I can't remember if I set them to be inline with the contact drum or not. I will find out soon though. I don't move the pinch rollers once I have them set. The pinch rollers are on a cam. You just loosen a set screw and then you rotate them to make them go up or down. I usually am only using one grit size belt. I typically use a 100 grit belt. I have had a long history with this machine. My first boss bought this machine at the IWF show in Atlanta. I used to use this machine when I worked for him. I ended up buying the machine when my old boss's shop got sold to another fellow. I've owned the machine for the last 22 years or so. My old boss did not do maintenance on it like he should have. I had Black Brothers recover the contact roller and I replaced the conveyor belt. I am thinking of having the pinch rollers recovered too, but I'm trying to decide if I should do that or if I should try to modify it to make the pinch rollers spring loaded (if possible) Thanks for your help too, Rich.

7/24/19       #7: Widebelt Sander Help Needed ...
Adam West  Member

Website: http://www.surfprepsanding.com

Costa sets the pinch rollers 0.05mm below the shoes from the factory. This causes far more problems than they would ever admit. I've seen multitudes of issues that would easily be fixed by simply using softer rubber and a bit more pressure. I've seen hundreds of sanders with sticks used to push parts through.

I would pull the shoes and set the rollers to 0.3mm below the shoe. I like to mill a step into the middle of a piece of aluminium that I can set across the shoe while it is inverted on a table.

The shoe itself would be set to the same height as the head it follows. The roller will give much better drive this way without causing a snipe from the roller itself.

This will help with drive issues through the machine.

If you would like you can private message me and I can walk you though it or help directly.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)