The Dotul 10’ Fixed and Adjustable Platen Stile Presses are constructed from the ground up with a heavy duty “I” beam construction and tube stock, welded securely for continuous and long duty. Thirty thousand (30,000) lbs. of air pressure are applied to the platen by six (6) air bladders at 100 psi. Continuous air pressure does not need to be applied after the initial charge. The platen applies pressure to the outsides of the stile blanks ensuring tight glue lines.
Model AT-1202 will adjust to 85% of the opening size. The press must be filled to 1 ½” from the top of the stack to the bottom of the top platen.
In accordance with the Site User Agreement, WOODWEB, Inc. assumes no responsibility for the accuracy or content of, or any transaction resulting from, listings posted at WOODWEB's Machinery Exchange. Please use caution, common sense and prudent commercial practices when utilizing WOODWEB's Machinery Exchange.