Planer head and (2) Sanding heads
36" wide capacity
5" thickness capacity
Minimum part length: 15"
Infeed loading area: 14"
Minimum part thickness with planer head: 1/2"
1st head: 6" diameter helical cutterhead with 14 mm carbide inserts - 30 HP
2nd head: 8" diameter spiral grooved rubber contact drum - 20 HP
3rd head: Combination head with 5.5" dia. spiral grooved rubber contact roll and 2.5" platen - 20 HP
Anti-kickback fingers on the infeed of machine
Sectional infeed shoe
Dual infeed and dual outfeed hold down rollers
37" x 75" abrasive belt size
Variable speed feed 15 to 45 FPM
Motorized thickness adjustment with digital thickness readout
"Go-To" set up device
Dial indicators on drum/platens
Infeed stop bar
Load meters
Dust extraction: 4,500 CFM
Compressed air usage: 4 CFM @ 90 psi
Full load amps @ 460 volt: 98.8
Machine weight: Approximately 8,000 lbs.
S/N 31164 Cleaned and Checked with parts warranty
Hours: 10,429