0.4 - 12 mm (1/2") Edge cap; 8 - 55 mm Panel thickness; 160 mm (6-3/8") min. panel length and 65 mm (2-1/2") min. width; line control (NO limit switches) for workstation function; 14 MPM Feed Speed (11 MPM automatically when corner rounding)
Quick heat-up glue system w/overhead hopper feed, "quick change" glue tank for maintenance & glue color change.
Automatic magazine for strip & coil stock, 3 mm PVC guillotine, (1) drive plus (3) idle roll "pneumatically controlled" pressure sections.
Workstations:
Double motor end trim (0.5 HP - 12,000 RPM motors), automatic chamfer from control panel 0° - 15°.
Top & bottom flush/Fine trim (0.75 HP - 12,000 RPM motor) bevels 0° - 25°, with insert knives for 3 mm PVC radius; (4) position turret stop for electro-pneumatic axial movement of flush trimmer.
2-Motor Corner Rounding unit for leading and trailing edges of panels; either radius or chamfer cutters can be mounted; (0.5 HP - 12,000 RPM motors); 3 mm Max. edge thickness.
Top & bottom scraping for 2 - 3 mm radius,
Top & bottom buffing (0.125 HP - 1,400 RPM motors).
End trim & flush trim stations have HF motors w/electronic brakes.
*** Please click the link for full description***