Tansu Media Cabinet

Listing #1557 Listed on: 11/11/2008 Company Name: DeWitt Woodworking
Name: Paul DeWitt

This Media Cabinet was made of Cherry and Bubinga. The top has a Maple inlay border and the handles were shaped from Walnut. Everything visible on the outside is solid wood; the panels are all resawn and bookmatched. The back is a frame-and-solid panel design with ventilation and cord cut-outs. Finger joints on the drawers. I used hidden barrel hinges on the doors.