5' x 14' Douglas fir & aluminum conference table for a local publisher. The client drained a couple of mill ponds on their property and discovered a number of 8' to 10' diameter Doug fir sinkers. Probably been underwater for over 50 years. Not the penultimate tight vgf stuff but still pretty nice.