Can CV Drill Hinge Plate Holes

06/11/2013


From original questioner:

Hello All,

Does anyone know why Its possible for CV to drill shelf holes but not hinge plate holes?

Thanks

Steve

From contributor Ad


You need to make sure that the hole diameter for the hinge plates matches your tool diameter exactly or it won't drill them.


From contributor St


Thanks Adam
I figured it out. My interior scribe was set to .031 instead of 0. The plate would have been in dead air..
Steve