Mike

We are getting more and more calls for flat slab exterior doors as this seems to be the design of choice currently. We seems to be having good results using two part poly coatings but I'm wondering if we should start using an epoxy barrier coat followed by a varnish.

5/12/14       #2: Epoxy barrier coat on exterior door ...
Jim

Lot's of information in the finishing knowledge base. Also contact west system for information about epoxy.

5/12/14       #3: Epoxy barrier coat on exterior door ...
David R Sochar Member

After 40 years of building exterior doors - and recommending finish programs for same - I know one thing: The door will eventually need to be refinished. Not recoated, but old finish removed and new applied.

Therefore, I recommend products that can be removed and recoated easily. Epoxy does not fit that category. I cannot imagine removing an epoxy finish - the cost and time would be prohibitive. I do recommend Sikkens or spar varnish, and it is very easy to recoat every few years. If it ever does need to be removed, then it also is easy.

The old IWP exterior doors had a catalyzed finish that looked great but was very difficult to refurbish. I do know of one incident where a local finisher tried to charge a customer $35,000 to strip and refinish a paired entry. He had tented the area and was in there for 2 months!

5/12/14       #4: Epoxy barrier coat on exterior door ...
Adam

You need to wait a minimum of 7 days to topcoat epoxy resin with oil/solvent based products. Spar varnish will not harden if put on before the epoxy fully cures.

Do not thin epoxy. It adequately penetrates wood fibers at its normal viscosity. The determining factor of finish failure is the adhesive bond between the epoxy and wood. Thinning does not increase the adhesion. It actually lowers by waterproofness of the epoxy.

Problems of refinishing are caused by interlayer failures between the coats. This can be a problem between the varnish and epoxy. The epoxy is much harder than the varnish and the varnish can be scuffed off of the epoxy. The other scenario is gouging. This is where the damage goes down to bare wood. In this event the door will be unrepairable without showing some blotchy spots .

Doors should be protected with a homogeneous repairable product like spar varnish or Sikkens or a extremely durable solvent system.

Solvent system can be a problem in the future if the guy fixing it doesn't know what product was used, also they are often designed for spray application, spraying solvent in the field is not available.

If you ask in the finishing forum you should get some long term experience with the newer solvent systems like Ml Campbell Eurobild exterior. Its been around for atleast 10 years.

Most people who try the Bristol finish are happy with the final product. Cost is higher; however, it would be similar to an epoxy/varnish solution.

Bristol Finish

5/12/14       #5: Epoxy barrier coat on exterior door ...
Jim Baldwin

David has said it plain enough and I'll add my 2 cents.

If allowed to deteriorate to any significant state, epoxy wood finishes will have to be removed with a heat-gun and scraper (one small spot at a time). Sand paper won't cut it. It's significantly more difficult to remove than varnish. In truth, it's hell on earth to even consider.

Epoxy coatings are capable of lasting for years and years but proper application is the key. We're talking about penetrating epoxy primers and a half-dozen or more coats of Bristol. After that you'll still need to meticulously maintain the finish since wood moves and cracks the coating.

In my opinion, epoxy coatings over wood are almost always a mistake. Varnish is a close second. Both involve herculean stripping efforts.

Most every boat owner knows this stuff...
If you're not willing to live your life with sandpaper and brush continually and habitually in hand, you're better off with traditional oil or cetol.

Oil though, will inevitably look unfinished and dirty but at least it won't kill you to restore it.

Cetol eventually flakes off with a stiff brush or disappears on it's own. A yearly re-coating with a light scuff will maintain it. Cetol will never be a "show-quality sheen" but gets my vote for uncommon good sense.

I'm a wood boat owner and I've been to hell and back, time and again.

5/26/14       #6: Epoxy barrier coat on exterior door ...
Gene Wengert-WoodDoc

Regarding epoxy, there are different types. The standard epoxy is quickly deteriorated by uv light, so you need one that has uv stabilizers or absorbers. But, my understanding is that such absorbers do not last forever.

My sail boat is epoxy coated with several coats of paint on top. I built it myself and it is 8 years old and doing well. I used Zimdars 123 first on top of the epoxy.

5/26/14       #7: Epoxy barrier coat on exterior door ...
Jim Baldwin

Pigmented epoxy paints are great and virtually indestructible, especially over epoxy resins and fiberglass mat but clear-coat epoxy over raw wood is an entirely different subject.

7/21/17       #8: Epoxy barrier coat on exterior door ...
Old Pinky

I made the mistake of leaving an Epoxy coated table out in the sun. The finish turned yellow. I would not epoxy any wood exposed to outside.
Hope this helps.

9/1/26       #9: Epoxy barrier coat on exterior door ...
irtubes  Member

Website: https://irtubes.com/

Epoxy barrier coats can provide good moisture resistance, but exterior wood finishing also depends heavily on UV stability, adhesion, and compatibility with the topcoat. The recoating issue is worth considering too, since a system that performs well initially may become difficult to repair later. Testing the complete coating system is important.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!