Safety Speed Cut Thermwood Corporation ECabinet Systems

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: MDF for cabinet doors

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

MDF for cabinet doors

3/4/20       
Mark  Member

I've always used solid stock for stiles and rails and would use MDF for flat panels. It's been years since I've used MDF for raised panels, and remember using a glue size on the hips before assembly.
Anyway, I made some shop doors the other day out of 100% MDF. Very coarse sticking and hips. Like I'd never sell to a client, even if they asked me to.
My question is, what is a good grade/brand/weight of MDF to use for raised or machined panels that won't take hours to fill and sand smooth?

3/4/20       #2: MDF for cabinet doors ...
Oggie Member

From my limited experience with MDF doors, door grade MDF panels tend to look a bit yellowish and those that are not suitable for door machining tend to be on the brownish side. Maybe it has something to do which type of wood is used to make it from. But I'm not sure it's a general rule.

Anyway, you need to google it for "door grade MDF", or "moulding grade MDF", "MDF double refined",... or something similar. I'm not sure there's a standard name for this things, looks like every MDF manufacturer has his own idea about the name, or you could ask your local suppliers for more details.

Two of my local sheet suppliers have no idea what I'm talking about when I ask about that, but the third one carries those boards, made by McEwen and the description of the product says this:

================================
MDF, Double Refined (Door Grade)

Door grade MDF is designed specifically for painted and bladder pressed doors for the cabinet door industry. Quality standards on this product ensure better machineability with no raised fibers. This is achieved by a more uniform density throughout the board with a flatter profile. 1/2&#8243; – 49×97, 61×97 5/8&#8243; – 49×97, 61×97 3/4&#8243; – 49×97, 61×97
================================

Some time ago Home Depot in my area used to carry those yellowish MDF boards that machined pretty good (smooth finish, no fibers) and they were also cheap. I don't know what happened but they don't have them any more.

3/4/20       #3: MDF for cabinet doors ...
Leo G Member

Plum Creek is one of the better double refined MDF out there. If you have sharp cutters (as you should) it will mill up nice and I usually don't even sand before I put the primer on. If you are using the MDF for a bevel panel then you need to preprime and sand the bevel with a high build primer, my choice is Clawlock.

After you prime just the bevel you scuff it hard and then assemble and then prime as usual.

If you are doing flat recessed panels and the bevel is on the back side of the door then you don't have to preprime it.

For what its worth, I preprime all my panels before they are put into the door so the tongues have color on them. For the most part it's just white, but if they get a paint color other than white or off white I'll tint the primer to the color. This is in case there is a bit of shrinkage you don't see raw MDF.

Same with stained panels, the tongue gets stained before assembly.

3/4/20       #4: MDF for cabinet doors ...
D Brown

Plum creek is the best for raised panels I have used. What you are wanting is called " high density" mdf , it machines much better .

3/4/20       #5: MDF for cabinet doors ...
Leo G Member

I consider HDF not suitable because I have issues with priming. It doesn't like to dry nicely for me. Plum Creek is a high double refined MDF and I wouldn't call it high density MDF.

Maybe you are talking about another product I haven't heard of D Brown.

3/4/20       #6: MDF for cabinet doors ...
Adam

We likewise use plum. We sand the cut area with 240. Spot prime with either BIN or Clawlock. You need to use a sealer type primer to harden the fibers. Sand with 320. Prime the whole door. There is no grain. It’s better than wood.

3/4/20       #7: MDF for cabinet doors ...
Jim Herron

I prefer the 5/8" Plum Creek for raised panels.
We spray the machined areas with 50% reduced precat lacquer prior to profile sanding and assembly to harden the fibers so the machined areas are as smooth as the face.

3/5/20       #8: MDF for cabinet doors ...
Hen Bob Member

We also use Plum Creek

3/5/20       #9: MDF for cabinet doors ...
Mark  Member

Thanks for the replies all, looks like Plum Creek is the common denominator here and now I know to look for double refined material. Don't have an immediate need but I do want to be able to offer it for paint grade.
Leo G., I hear you on the sharp cutters- I didn't want to run what was essentially drops from over the years past my "good" C&P heads so I used a no name set I got who knows where. I did run a piece of poplar through first, looked ok so off I went. I even set the rpms to 10k and fed slow. Just a bad cut all around.
Lessons learned........
Again, thanks to all.

3/5/20       #10: MDF for cabinet doors ...
Leo G Member

If you are running MDF you have to have carbide cutters. I mostly by Freeborn cutters and the carbide are orange bodies. They have tangtung which is good for solid wood and shaper than carbide but they don't do well at all with MDF, they have yellow bodies. HHS will dull very fast with MDF.

Probably telling you all stuff you already know. LOL

3/5/20       #11: MDF for cabinet doors ...
Mark  Member

Oh yeah, they were carbide- just s**t carbide no names. Painted blue
Most of my C&P sets are Freeborn carbide, very reliable product with great support.

3/5/20       #12: MDF for cabinet doors ...
Adam

Likewise Freeborn except for raised panels. Many years ago I bought one of those Freud ones off of Amazon that has the two raked top cutters. They are better in my opinion. My Freeborn has been delegated to cherry only, where they must be really sharp to avoid burning.

The Freud regular blades & router bits are no good. Their industrial blades and shaper cutters are decent.

5/8” plum for raised panels. 3/8” mdf for flat panels. The faces of plum are also smoother and harder.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • ULTI-BOARD
      The Ultimate Spoilboard - ULTI-BOARD - Specifically Engineered and Formulated for the Ultimate in Spoilboard Performance - Not Your Ordinary Sheet of MDF.
    • Parts Cutter CNC
      CNC Cabinetry and Closet Parts
    • GreCon
      Spark Detection and Extinguishment Systems and Quality Assurance Measuring Equipment
    • ECabinet Systems
      Free, Fully Functional Cabinet Design Software and Kitchen Layout Software
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • American Fabric Filter Co.
      Provider of Custom Made Filter Bags and Transfer Sleeves
    • W. Moore Profiles, Ltd.
      Supplying Knives and Cutters to the Woodworking Industry - Standard and Custom Profiles Available
    • MachineryMax
      New and Used Machinery for the Professional Woodworker
    • Tooling on the Web
      Tooling and Tooling Accessories - Free Re-Sharpening for Qualifying Tools
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • T-Tool USA LLC
      Quality Tool-Holders, Tooling Supplies and Accessories for Numerous Cutting and Grinding Applications
    • Felder USA
      High Quality Woodworking Machines and Tools

    Become a Sponsor today!