Sawing and Drying

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject:

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Wood movement across large widths

2/25/15       
Vic

I wasnt quite sure under what heading to post this question, but thought I would start here, Maybe Dr Gene will chime in.

I've been asked to build some rather large raised panels from KD Butternut lumber. And in these will be several 3/4" or 4/4 glued up panels up to 5' wide. I'm a little concerned about the stability of 5' wide panels as or if the EMC changes.

So, I thought I would send the GC an email with my concerns saying that I would make them, but that I'm concerned about the stabilety. My question for this forum is: Is there a specific movement in wood in relation to a specific EMC change??

For instance: We know Red Oak will shrink 7% from wet to KD. So what can I expect wood to move (shrink or swell in %) per X in EMC change??

Does this make sense to anyone and is it a fair question, or a legitimate concern??

Thanks,

2/26/15       #2: Wood movement across large widths ...
Gene Wengert-WoodDoc

Great Question. Your question is legitimate and fair...."extremely legitimate" indeed. (Not sure if there is a phrase "extremely legitimate" or not, but you know what I mean.) Is this the right place to post it? Yes, but it is so important, it should be posted on five or six other boards too

#1. Wood shrinks and swells across the grain when the moisture content (MC) changes...swelling if the MC goes up and shrinking if the MC goes down. Wood seldom shrinks lengthwise. (The limited lengthwise shrinkage is why plywood, with the lengthwise direction being at 90 degrees in each adjacent sheet of veneer, is overall so much more stable than a solid piece of wood.)

There are two directions for across the grain- -TANGENTIAL (meaning parallel to the annual growth rings; the width of a flatsawn piece) and RADIAL (meaning perpendicular to the growth rings or the width of a quartersawn piece). The values for tangential movement would be the maximum movement; the values for radial movement would be the minimum. In practice, a perfectly flatsawn or perfectly quartersawn piece is not common, so we will likely have a bit less than the maximum for most flatsawn pieces and a bit more for most quartersawn or rift sawn pieces.

When dealing with oak, the highest shrinking commonly used species in North America, there are twenty species of red oak and twenty species of white oak that will show up in the commercial market. Each species within the grouping of red oak or white oak does move different amounts, as shown in the figure attached below.

#2. When dealing with shrinkage, green means 28% MC and 0% means 0% MC. Shrinkage from 28% to 0% (or swelling in the reverse) is a straight line with MC, so you can divide the total number by 28 to get the movement for each 1% MC change. Example, northern red oak is 4.0% radially and 8.6% tangentially. So that is (4.0 / 28 =) 0.143% size change radially for a 1% MC change, and (8.6 / 28 =) 0.307% tangentially for a 1% MC change. (Actually, the numbers are for thin pieces of wood; the thicker the wood is, the movement will be somewhat less, but not a whole lot less.

The values for every commercial species can be found in the WOOD HANDBOOK, Table 13-5 at www.fpl.fs.fed.us/documnts/fplgtr/fplgtr190/chapter_13.pdf

Two more points to go, so hang in there.

#3. The moisture content of wood changes about 1% for every 5% RH change... 0% RH = 0% MC = 0% EMC 30% RH = 6% MC = 6% EMC 50% RH = 9% MC = 9% EMC 65% RH = 12% MC = 12% EMC 80% RH = 16% MC = 16% EMC

Note that EMC (equilibrium moisture content) refers to the moisture in the air. It is the connection between humidity in the air and the MC in the wood.)

So, as a rough approximation, you could use the 0.143% and 0.307% size change for 1% MC change numbers above as the predicted size change for a 5% RH change as well.

Of course, the change is not instantaneous...the surface and ends change quickly (unless coated with a vapor resistant coating); the core may take days, weeks or months to change. (In fact, the core MC is often the MC that the lumber left the kiln at, as it takes quite a while for the core MC to change.) This slow change or movement of the core is also why thicker pieces of wood have less movement than thin pieces.

#4. Here is a minor point, but do read it please. If wood has been shrinking and the RH is lowered by 5% RH (or 1% EMC), then the wood will continue to dry by 1% MC and continue to shrink, as predicted. However, if a piece has been shrinking, but now is exposed to a humidity increase, there will actually be a lag in the response to the RH and a lag in the change from shrinking to swelling. (Technically, this is called the hysteresis effect.) This effect is why, if we have lumber that has been drying and then this lumber is a bit too wet, but we use it anyway and then the wood is put into a dry environment so that the wood dries more, the size change can be fairly significant, resulting in gluing issues like open joints, size changes, warp, etc. On the other hand, if we have dry wood and then it goes into a summertime humid environment, the swelling change will not be as big as we calculated. Knowing this fact is why we often specify an incoming moisture of 7.0% MC, as we know the wood might dry to 6.0% MC in use during the wintertime or increase to 9.0% MC use in the humid summertime, but the 9.0% EMC will actually behave more like 8.0% EMC. Then the next winter when the wood dries again, it will be 6% EMC, but due to hysteresis, it will seem like 7.0% EMC. Again, that is why we almost always see moisture problems the first year the wood is put into use because the wood is often not quite dry enough, etc. So, maybe hysteresis is not a minor point after all.

If you want even a bit more practical stuff, consider two items: A. First. Wrapping in plastic will prevent any moisture change, even if the someone stores the product you make poorly (bad humidity). A big roll of Saran type wrap from the big box stores is not expensive and can really pay off.

B. Second. Do not humidify your shop above the humidity that your customer will have. If I humidify my shop to much, I am pushing the undesired shrinkage to the customer. But, I would rather have a defect show up in my shop (where I can repair them more easily) than in the customer's home or office. Of course, if I get the correct MC in my lumber initially, then I will not have to worry. Of course, some kiln drying operations do not dry all the pieces dry enough, as it is too expensive for them (shortsighted)- -it is actually not too expensive from your point of view.


View higher quality, full size image (1338 X 1505)

2/26/15       #3: Wood movement across large widths ...
Vic

Gene, thanks so much for this info. It is exactly what I was looking for.

My plan (partly to CYA) is to send a email to the GC with this info. I will ask him to have the house humidifier working and in place before installing the panels. After finding what the house EMC target will be, I wlll make sure my wood MC is at that target.

So if the house RH is 50% and I recieve, process and deliver my panels at 9% MC, then the world will be a better place, right?? If this is constant, all will be well...

2/28/15       #4: Wood movement across large widths ...
Gene Wengert-WoodDoc

I noted three typos that you might want to correct before you share with the customer.

In #4, "tot he" should be "to the"

In A, "to much" should be "too much"
and "bog box" should be "big box"

Hopefully that is all of them. (Note that this info is from a column "Ask the Wood Doctor" that I wrote for FDM magazine, but the article has not been published yet. Actually, I write articles way ahead, so that sometimes it takes a year to appear. It makes my job stress free as I never get a cal that says "We need a column by tomorrow!")

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)