8/4 x 8' african mahogany, old stock good widths, heavy to ribbon grain 1 bundle 500;BF $3.50 bd ft. 8/4 x 10; Walnut FAS old stock good widths 1 bundle 630 BF $3.50 bd ft 5/4 x8; african mahogany old stock good widths heavy to ribbon grain 1 bundle 725 bf $3.50 bd ft 4/4 4/4 SYP 7" width 8;, 7; 5; 4; long This is second growth material heavy to vg, very square clean lumber from a mill that does export timber.mostly clear, these are drops off the timber mill. generally 15-20 rings per inch. Price ? 1020 bd ft total...Make offer for entire lot...I need to clean plant it's sold
In accordance with the Site User Agreement, WOODWEB, Inc. assumes no responsibility for the accuracy or content of, or any transaction resulting from, listings posted at WOODWEB's Lumber Exchange. Please use caution, common sense and prudent commercial practices when utilizing WOODWEB's Lumber Exchange.