Description
Used Baker model ABX band resaw w/ return roller conveyor and thin roller guide package installed on the saw that lets the saw cut as thin as 1/8" thick
Specifications:
Number of heads: 1
Guides: Baker low-profile flat guides with steel guide plates with rear backup roller guide wheels
Dust output: 6" x 6" (15.24cm x 15.24cm) square outlet with a 90 degree adapter chute with a 4" (10.2 cm) diameter outlet, which can be rotated to serve four directions of discharge. 600 CFM recommended.
Dimensions & weight: Length 84" (2.13m), Width 72 1/2" (1.84m), Height 68" (2.03m) Weight 2000 lbs (907 kg)
Power:
Main drive motor: 30 HP, 480 V , 3 PH
Electrical: Completely prewired. NEMA 12 enclosure with starter and overload protection standard
Feedworks/Conveyor hydraulic pump motor: Driven by main engine. Hydraulics has 14-gallon reservoir, flow control valve for variable feed speed, filter, start/stop valve
Feedworks: Rough-top belting and hold-down wheel
Feed speed: Fully variable 0 to 95 fpm (0 to 29m per minute)
Conveyor width: 12" (30 cm)
Material Capacity: 12" x 12" (30 cm x 30 cm)
Hold-down system: Hydraulically powered hold-down system with a 4 5/8" diameter urethane wheels
Blades:
14'2" x 1" x 0.035" hardback or 14'2" x 1 1/4" x 0.035" hardback
Blade tensioning: Mechanical Spring
Kerf: 0.072" (1.8288 mm)
Specs are not binding and subject to error.