I recently started working for a shop that has a 20" Crescent bandsaw which they recovered the wheels on within the last year or so. The problem is, neither of the tires has a crown to them which in my understanding of bandsaws is that the crown helps keep the blade tracking at or close to the center of the wheel so not to track off the wheel. Am I correct on this point?

1/23/15       #2: Crescent bandsaw tires ...
JeffD

I'm no expert on bandsaws, but what I've seen is while most smaller bandsaws do have crowned tires for tracking, some of the bigger saws do use flat tires. If the blade tracks correctly I wouldn't worry about it. If not the tires can be crowned on the machine with a little ingenuity. With a little searching you'll turn up several methods for doing so.

good luck,
JeffD

1/23/15       #3: Crescent bandsaw tires ...
rich c.

Doesn't need a crown. Minimax band saws use flat tires.

1/26/15       #4: Crescent bandsaw tires ...
David R Sochar Member

Bandsaws historically have crowns, all of them. The way the physics works, the blade wants to run to the high side, contrary to what one might think. It is best practice to let the bald find its comfortable spot on the crown, and then bring the guides up to it. Do not use the guides to 'place' the blade.

I worked in a shop where one guy decided the crown in the wheel was wrong and spent all day sanding a hollow in the wheels. It would throw a blade in seconds - absolutely would not work.

The link has a fairly good dialogue with some good and some fair info. The video is the reason I re-posted it.

See Post # 10

1/27/15       #5: Crescent bandsaw tires ...
Kevin Member

Thank you all for your responses! The 36" Tannawitz I had did also have a noticeable crown on the tires as well as my first big machine, a Yates (pre-WWI). I have always been of the same belief as Mr. Sochar in regards to the physics of it. I will be talking to the boss about another retread in this since it won't track properly the way it is now. Thanks again to all.

1/27/15       #6: Crescent bandsaw tires ...
rich c.

Be sure to tell your boss that other machines don't. I had a 32" Fay and Egan that had no tire on the top wheel when I bought it. In those days, aftermarket tires were next to impossible to find. I bought some 1/8" rubber belting and contact cemented it to the rim, with a skive joint. It ran perfectly for years. There is a lot more to tracking than crown in the tires. I'm not certain of the engineering, but as an example, I would question that a 1/4" blade even sees the difference between a crown and a flat. How much crown in a rubber tire will it contact? 1" blade, maybe different? Just saying it is absolutely not a necessity in every case.

6/17/19       #7: Crescent bandsaw tires ...
Dave Nauman  Member

Website: http://www.dcnchair.com

I have a 20" Crescent and the wheels themselves are crowned. New tires should just take on the crown of the wheels.

6/17/19       #8: Crescent bandsaw tires ...
KCR

It has been a couple of years since I worked for this company but I have never forgotten this issue.
I don't know if the Crescent machine they had, had a crown in the wheel casting or not but I do know that the surface of the tire put on it was truly flat and that no matter how I tried to adjust it, the band would never stay on track. When I took off the guides, the blade wanted to either race forward or backward off the wheel, there was no in-between. Ultimately just so I could move on, I set it up so the blade would track back to rest on the guide bearings while running. Since then I have decided for myself that I would never have a saw without crowned wheels, Just makes sense to me.

  • Post a Response to this thread
  • notify me of responses to this topic
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)