sanding/polishing

11/17/14       
Mike Auger

I find using Velcro sanding discs with an interface pad polishes the wood. We use 150 and 180 on oak. You can look at the wood at an angle and see a shine. It also feels like it has been sanded down to 320. I am concerned about adhesion issues. I also feel like the interface pad contours too much and doesn't really flatten or remove glue . Has anyone else experienced this?

11/17/14       #2: sanding/polishing ...
chris

150 on oak is enough.
It is easy to switch out the pad on an orbital sander and get a harder one if needed.

11/17/14       #3: sanding/polishing ...
Daniel Shafner  Member

If you're seeing a shaine then you are burnishing the wood rather than sanding it. You're right to be concerned with adhesion.

Are you pushing down on the sander? The sandpaper should do the work of sanding with no downward pressure from the person holding the sanding machine.

I would also consider a switch to peel-and-stick discs because these are flatter to the surface than a cushioned abrasive.

Friction from sanding can turn the glue gummy. That's one more reason -- avoiding heat buildup from friction -- to avoid bearing down on the sander.

Get a cabinet scraper for glue spots. Cabinet scraping is a good first step.

11/17/14       #4: sanding/polishing ...
Mike Auger Member

Thanks for the responses. I encourage more people to respond.I pretty much assumed what I was going to get for response. I have been saying this all along to the company I work for. When we sand oak their process has been 150 and 180. In reality it feels like 320 grit. I have used the Velcro and pad for leveling out finishes on could ter tops. It is soft enough to level without burning through the finish. Another issue that I have encountered is sanding painted maple. Again, the same tools are use. I feel like the pad is too soft and does not even CUT but just polishes..... We see lines on glue ups of draw fronts. They seem to disappear using traditional hard pads with sticky abrasives. Again, with velcrpo, it feels polished. Using sticky back indasa 120 cuts so much better and actually looks more uniform with first coat of primer.

11/17/14       #5: sanding/polishing ...
Adam West  Member

Website: http://www.surfprepsanding.com

I'm not entirely sure I have the whole picture.

You use an orbital sander with an interface pad and velcro disk in 150/180 to white wood sand?

Then you use that same pad to sand in between coats with the same grits?

Have you just tried removing the interface pad and sanding with the straight disk?

Velcro does not contribute to polish in any significant way. I use it daily. Velcro just gives a slightly better finish. It cuts just as flat.

The interface pad sounds too soft for the job.

11/17/14       #6: sanding/polishing ...
Mike Auger Member

Yes I had to agree.....the sander is using the interface pad on everything..... Just seems to much. It won't even sand missed glue. It just contours the glue.

11/18/14       #7: sanding/polishing ...
Brian T

Are you talking about a pad protector or and actual .25'' or .5 interface pad?
There's a big difference.

If he's using a .5 interface pad on raw wood he will not be able to cut glue. If it's a standard pad protector then there should be no issues.

11/23/14       #8: sanding/polishing ...
Andrew Kelsey

If you are burnishing the wood, you are using the disc for too long. A 180 disc isn't going to last as long as a 120. Keep the paper sharp and you won't burnish the wood. You will also have less issues with even stain application.

  • Post a Response to this thread
  • notify me of responses to this topic
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Carter Products
      Band Saw Guides, Blades, Wheels, Tires, Line Lasers and 2D Projectors, Wide Belt Sanding Accessories, Vacuum Holding Systems and More
    • SAMES KREMLIN formerly EXEL North America
      Precision Spraying Solutions From Pumps To Complete Application Systems-Design and Manufacture of Process Equipment Including Airspray, Airmix, Airless, Rexson Dispense, Electrostatic and Powder Coat
    • Apollo Sprayers Inc.
      High Volume Low Pressure Spray Systems
    • EX-FACTORY
      Importer and Dealer of New and Used Woodworking Machinery
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Supergrit Abrasives
      Industrial Quality Abrasives Manufactured by Leading US and Foreign Companies
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production

    Become a Sponsor today!