Ahora tienes dos piezas con forma de campo de béisbol. Coloque uno en la cuna y trabaje con el otro. Si eres bueno con la sujeción, puedes equilibrar la pieza, pero para empezar quizás quieras hacer una plantilla para sujetarla a 45 grados. Corte todo lo que pueda antes de golpear las abrazaderas o la plantilla, luego déle la vuelta y termine de cortar de principio a fin.



| Common Lumber Name | A | B | C |
| Hardwoods | |||
| Alder, Red | 9.9 | 19.2 | 2506 |
| Apple | 10.9 | 31.7 | 4132 |
| Ash, Black | 9.3 | 23.4 | 4132 |
| Ash, Green | 14.3 | 27.6 | 3590 |
| Aspen, Bigtooth | 10.3 | 18.7 | 2439 |
| Aspen, Quaking | 10.3 | 18.2 | 2373 |
| Basswood | 6.2 | 16.6 | 2174 |
| Beech, American | 8.9 | 29.1 | 3793 |
| Birch, Paper | 8.8 | 25.0 | 3260 |
| Birch, Sweet | 11.9 | 31.2 | 4065 |
| Birch, Yellow | 9.2 | 28.6 | 3723 |
| Buckeye | 8.9 | 17.2 | 2235 |
| Butternut | 11.3 | 18.7 | 2440 |
| Cherry | 13.8 | 24.4 | 3184 |
| Chesnut, American | 11.6 | 20.8 | 2708 |
| Cottonwood | 8.5 | 16.1 | 2102 |
| Dogwood | 6.8 | 33.3 | 4331 |
| Elm, American | 10.2 | 23.9 | 3116 |
| Elm, Rock | 12.2 | 29.6 | 3860 |
| Elm, slippery | 11.5 | 25.0 | 3251 |
| Hackberry | 11.8 | 25.5 | 3319 |
| Hickory, Bitternut (Pecan) | 14.7 | 31.2 | 4062 |
| Hickory (True) | |||
| Hickory, Mockernut | 9.1 | 33.3 | 4332 |
| Hickory, Pignut | 9.3 | 34.3 | 4332 |
| Hickory, Shagbark | 10.9 | 33.3 | 4333 |
| Hickory, Shellbark | 6.6 | 32.2 | 4195 |
| Holly, American | 8.3 | 26.0 | 3387 |
| Hophornbeam, Eastern | 7.9 | 32.8 | 4266 |
| Laurel, California | 15.1 | 26.5 | 3456 |
| Locust, Black | 21.2 | 34.3 | 4470 |
| Madrone, Pacific | 7.8 | 30.2 | 3925 |
| Maple (Soft) | |||
| Maple, Bigleaf | 12.8 | 22.9 | 2980 |
| Maple, Red | 13.1 | 25.5 | 3318 |
| Maple, Silver | 12.4 | 22.9 | 2981 |
| Maple (Hard) | |||
| Maple, Black | 12.3 | 27.0 | 3523 |
| Maple, Sugar | 12.3 | 29.1 | 3793 |
| Oak (Red) | |||
| Oak, Black | 11.7 | 29.1 | 3792 |
| Oak, California black | 16.4 | 26.5 | 3455 |
| Oak, Laurel | 6.3 | 29.1 | 3791 |
| Oak, Northern red | 13.6 | 29.1 | 3793 |
| Oak, Pin | 13.0 | 30.2 | 3928 |
| Oak, Scarlet | 13.2 | 31.2 | 4065 |
| Oak, Southern red | 9.6 | 27.0 | 3520 |
| Oak, Water | 10.4 | 29.1 | 3793 |
| Oak, Willow | 6.4 | 29.1 | 3790 |
| Oak (White) | |||
| Oak, Bur | 15.4 | 30.2 | 3928 |
| Oak, Chestnut | 10.1 | 29.6 | 3858 |
| Oak, Live | 17.5 | 41.6 | 5417 |
| Oak, Overcup | 10.7 | 29.6 | 3860 |
| Oak, Post | 11.0 | 31.2 | 4063 |
| Oak, Swamp chestnut | 10.7 | 31.2 | 4063 |
| Oak, White | 10.8 | 31.2 | 4062 |
| Persimmon | 7.0 | 33.3 | 4332 |
| Sweetgum | 8.9 | 23.9 | 3115 |
| Sycamore | 10.7 | 23.9 | 3115 |
| Tanoak | 9.0 | 30.2 | 3926 |
| Tupelo, Black | 10.4 | 23.9 | 3116 |
| Tupelo, Water | 12.4 | 23.9 | 3115 |
| Walnut | 13.4 | 26.5 | 3454 |
| Willow, Black | 8.6 | 18.7 | 2438 |
| Yellow-poplar | 10.6 | 20.8 | 2708 |
| Common Lumber Name | A | B | C |
| Softwoods | |||
| Baldcypress | 13.2 | 21.9 | 2844 |
| Cedar, Alaska | 14.4 | 21.9 | 2844 |
| Cedar, Atlantic white | 10.9 | 16.1 | 2100 |
| Cedar, eastern red | 16.4 | 22.9 | 2981 |
| Cedar, Incense | 13.1 | 18.2 | 2371 |
| Cedar, Northern white | 11.1 | 15.1 | 1964 |
| Cedar, Port-Orford | 12.6 | 20.2 | 2641 |
| Cedar, Western red | 12.2 | 16.1 | 2100 |
| Douglas-fir, Coast type | 12.3 | 23.4 | 3049 |
| Douglas-fir, Interior west | 13.2 | 23.9 | 3116 |
| Douglas-fir, Interior north | 14.0 | 23.4 | 3048 |
| Fir, Balsam | 9.9 | 17.2 | 2236 |
| Fir, California red | 10.6 | 18.7 | 2437 |
| Fir, Grand | 10.7 | 18.2 | 2371 |
| Fir, Noble | 10.1 | 19.2 | 2507 |
| Fir, Pacific silver | 10.4 | 20.8 | 2711 |
| Fir, Subalpine | 10.5 | 16.1 | 2101 |
| Fir, White | 12.2 | 19.2 | 2506 |
| Hemlock, Eastern | 12.6 | 19.8 | 2573 |
| Hemlock, Western | 11.5 | 21.8 | 2847 |
| Larch, Western | 11.3 | 25.0 | 3251 |
| Pine, Eastern white | 12.3 | 17.7 | 2303 |
| Pine, Lodgepole | 11.5 | 19.8 | 2576 |
| Pine, Ponderosa | 12.6 | 19.8 | 2573 |
| Pine, Red | 12.2 | 21.3 | 2777 |
| Southern yellow group | |||
| Pine, Loblolly | 12.9 | 24.4 | 3183 |
| Pine, Longleaf | 15.0 | 28.1 | 3658 |
| Pine, Shortleaf | 12.9 | 24.4 | 3183 |
| Pine, Sugar | 12.6 | 17.7 | 2302 |
| Pine, Western white | 10.0 | 18.2 | 2370 |
| Redwood, Old growth | 14.9 | 19.8 | 2573 |
| Redwood, Second growth | 13.2 | 17.7 | 2302 |
| Spruce, Black | 11.3 | 19.8 | 2575 |
| Spruce, Engelmann | 10.0 | 17.2 | 2234 |
| Spruce, Red | 10.6 | 19.2 | 2506 |
| Spruce, Sitka | 10.8 | 19.2 | 2506 |
| Tamarack | 12.0 | 25.5 | 3318 |