gary

I have a client who used a competitors raised panel door where the panel is showing the glue lines after they have applied an extremely high gloss finish. I have no idea of M/C or type of glue but I do know the doors are solid Maple throughout. I suspect they may have just biscuited the panels together whereas I use a glue joint knife. They want me to fabricate a new door that has panels that will remain as a perfect base for the high gloss finish. So I am wondering if anyone has had any luck using a raised panel with solid wood edges with an MDF face ? or something similar? I would be most worried about the movement of the wood/MDF marriage. The client has suggested solid MDF panels but I don't know how you can ever sand them smooth enough for the high gloss finish ( it looks like plastic) Perhaps a solid wood panel fabricated properly is the obvious choice but want to open to others experiences. Thank you

2/9/15       #2: Interior Door Panels ...
JT

Solid wood moves, and no two pieces the same. It could be the original panels where sanded to quickly after glue up and the joints have sunk but I suspect it is just natural movement. You don't say if they are interior or exterior but if they want high gloss sounds like veneers over a flat substrate like mdf, but that makes raising a whole other problem.

2/9/15       #3: Interior Door Panels ...
Geoff

You can make the door with solid mdf panels, no problem. Prime and sand the raised portion before assembly. In my opinion making a panel with a solid wood, mitered edge is extra work for a interior paint grade door.

And, dare I say, neither a biscuit joiner or a "glue joint knife" will make the edge glue joint any better.

2/10/15       #4: Interior Door Panels ...
Gerry

I agree with Geoff. Use MDF sand the profile well and prime with a heavy base primer MLC Clawlock or the like. I think you are going to continue to have problems using solid under a high gloss finish.

FWIW
Gerry

2/11/15       #5: Interior Door Panels ...
David R Sochar Member

Rimming stable panels with solid wood that is later raised is a premium way to make raised panels. The stable core can be framed, sanded smooth, veneered, then raise like solid wood. The resulting panel is stable, and can even be lightly glued into the frame. Save the gawd-awful MDF for the core, where it belongs, and let the wood show.

2/11/15       #6: Interior Door Panels ...
Gerry

I was assuming a pigmented solid color finish. If this is a clear finish I would agree with David.

Gerry

2/11/15       #7: Interior Door Panels ...
Leo G

Likely the panels were processed to quickly. Glued up, taken out of the clamps, sized and widebelt sanded within 2 hours.

If you don't want sunken glue joints you will need to wait 3 days after gluing before you sand them. That gives time for the water in the water based glue to evaporate out of the wood cells and have them return to their normal state.

Other options are use a non water based glue such as epoxy or polyurethane.

2/12/15       #8: Interior Door Panels ...
Kevin Jenness

Sanding and priming moulded mdf edges is indeed laborious, as is rimming an mdf panel with solid wood. We have found that using Medex reduces the effort of prepping edges for paint considerably.

2/15/15       #9: Interior Door Panels ...
Adam

Kevin,

You can also use ultra refined mdf. You can't see the porosity after priming and sanding to 320. It costs alot less than medex.

2/16/15       #10: Interior Door Panels ...
Gene Wengert-WoodDoc

In addition to the common reason for visible joints...sanding too soon after gluing...having the wrong MC at the time of gluing is another reason--as the wood eventually dries and shrinks, the glue joint is a bit more rigid than the wood, so it does not shrink as much. And a third reason is that the joints are inferior because there was too much time between surface prep and gluing, so that some shrinkage occurred and the surfaces were not flat enough. Finally, with some PVAs, heat from sanding or even finishing ovens can soften and melt the adhesive, causing the glue to be slightly squeezed out of the joint. The bottom line is that without examination, the cause is not clear.

On the other hand, millions of panels have been made with no problems, so using MDF, which is certainly a good idea, is not essential if the panel is made properly.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory