Determining Vacuum Holddown -- 3 -- 
11/16

I am in the process of purchasing a moving gantry CNC with a 5x10 table. I am trying to determine the proper vacuum pump. Typical cuts include a nested 4x8 sheet of 3/8" baltic birch plywood maxed out with 9.5" x 3.5" and 2" x 3.5" pieces. Currently we use a smaller CNC and leave an onion skin and then route it off. I absolutely want to avoid this. Another typical job is a nested sheet of 3/4" baltic birch plywood maxed out with 8" x 3.25" pieces. Typically I am either maxing out the sheet of plywood with small parts or it is all custom work with some smaller parts. I attached an image of an example. I am being suggested Dekker, Busch, Becker, and Travaini. This will be my first experience with vacuum pumps and I want to make sure I make the proper decision. I have been reading a bunch and understand the difference between HP, CFM, and IN HG but my unanswered question is how much do I actually need. Looking for suggestions and help please.
Click the link below to download the file included with this post.
CNC_Cut_Sheet_Example_01.pdf
11/16 #3: Determining Vacuum Holddown ...

As much as you can afford and it's never enough.
I started with a 10HP regen blower. Did OK, but wanted more. Got a 10HP Becker. Better but wanted more. 18HP Becker. Better but wanted more. Now have a 30HP Sullair rotary screw. 430 CFM @ 25". Pretty good when masked off to 4X8 but some days I really wish I had more.
Tool bit choice will make a difference as well. Unless I need good edges, I have gone to a 3 flute down spiral roughing bit on my ply. Less cutting pressure moving the parts sideways.
11/16 #4: Determining Vacuum Holddown ...

We have a 5 X 10 with a 40hp Quincy. We can't hold parts that small. Tab or onion skin! If they are just rectangular parts stack cut them on your beam saw. Much faster.
11/16 #5: Determining Vacuum Holddown ...

Dropout - That is the exact situation I see myself getting into. I want to get the right one from the start.
Larry - I was afraid of getting this response! lol
11/17 #6: Determining Vacuum Holddown ...

2 CNC here, one with 25hp and one with 15 hp regen blowers, Both nest very well yet I trust neither with the parts you have sized,
If they are a common produced part consider a dedicated vac jig with sealed pucks
11/17 #7: Determining Vacuum Holddown ...

We have a 40hp on a 5x10 table.
The cut sheet you show would be no problem, but I might cut the little ones in two pecks down if the table was getting snarley.
Get as much as you can afford.
It won't look so cheap if you have to upgrade because what you bought doesn't cut the mustard so to speak.
11/17 #8: Determining Vacuum Holddown ...

I probably should have looked at your pdf,, Mine will cut that all day long yet it is best to OS the small long parts,, the list you gave in text is too small for me,, courious though why 2.5" are they nailers / stretchers ?
11/17 #9: Determining Vacuum Holddown ...

James - I am realizing that there may be no way around onion skinning the smaller pieces. The PDF with the 2.5" pieces is for our main product line. We make road cases. There will be additional routed holes for latches and hardware but I just wanted to make the drawing as basic as possible.
11/17 #10: Determining Vacuum Holddown ...

Snaglpuss - what model vacuum do you run?
11/17 #11: Determining Vacuum Holddown ...

Website: http://www.allstaradhesives.com/
What type of router are you looking at? What ideas do you have for a vacuum table grid? If you like you can contact me at gbradley@allstaradhesives.com I think we can help.
11/17 #12: Determining Vacuum Holddown ...

I'd like to see someone actually hold "9.5" x 3.5" and 2" x 3.5" pieces" or for that matter 2.5 x 14" without a dedicated gasketed board or onion skin. A nest with a bunch of those small parts is going to have lots of leaks due to all the cut lines.
If you are going to be production routing the same pattern over & over, the gasketed board is the way to go. You just have to be careful when loading it to not snag the gaskets. Allstar is a good place for gasket.
Plywood adds another level of problems. Sometimes, as small or longer but narrow parts are cut, they want to pop up due to the release of tension in the material.
As for one brand or another of pump holding better, I doubt that within types there is much difference. Different types do have different flow VS vacuum curves.
11/17 #14: Determining Vacuum Holddown ...

I regularly cut pieces as small or smaller that what is suggested. I use a 10 hp regen pump for vacuum. I am cutting 3/4 mdf, 1" apple ply and 3/8 maple ply.
I do not onion skin nor leave tabs. I do it by using 2 ft wide masking tape and covering the board on the bottom side. Then I cut to the tape but not through the tape. Just pull the pieces off of the tape and ready to go.
11/17 #15: Determining Vacuum Holddown ...

Jim - that sounds pretty good. Thank you.
11/17 #16: Determining Vacuum Holddown ...

George - Thanks, I am going to consider gasketing the pieces that are standard production runs.
Larry - Thanks for the input, I clearly have a lot to consider
11/19 #17: Determining Vacuum Holddown ...

Website: http://www.NEMI.com
Hi Chris -
It sounds like a dedicated fixture might be a good solution for you. I would be happy to give you some information about NEMI's offerings.
Andrea
ap@NEMI.com
763-856-2044x208
11/19 #18: Determining Vacuum Holddown ...

Website: http://www.allstaradhesives.com/
Chris
As far as the vacuum goes and what to use you can research AXYZ routers in Canada and I do not think that they use a vacuum as great as mentioned above but AXYZ buys and uses our "pegboard tiles" if used precisely you could do nested based manufacturing and cut small parts like the stretchers on your cut list,we have a video on cutting cabinet doors https://www.youtube.com/watch?v=jN0wLRa3tQM
Let me know how you make out.
View higher quality, full size image (432 X 301)
11/19 #20: Determining Vacuum Holddown ...

Website: http://www.cnccustomservices.com
Companies that machine plastic and aluminum nests encounter this alot. One technique if you have a tool changer -
1.) Route the 2.5" parts first with the same tool you would normally use to route through leave a .015 to .02 skin
2.) Select a smaller diameter cutter (1/8" to 1/4") Cut the smaller profiles through with the smaller cutter - may have to back the geometry "off" a few thousandths in X and Y - .004~.008 (.1~.2mm) will insure the small cutter is cutting the skin only and leave an almost imperceptible "lip". Talking about 1/128 in or less!
3.) Re-select your primary tool and route through the larger parts of the nest where vacuum escaping through the cut swath will be less influential on hold down
Works great in alot of instances and can eliminate post secondary operations yours looks like a very good candidate.
Hope this helps
Mark T
11/19 #21: Determining Vacuum Holddown ...

Mark - Thank you for the advice! Sounds great!
11/20 #22: Determining Vacuum Holddown ...

Mart-T
we use same method for long time
but added some point:
i create script that decide the parts to 3 types:
small- as you mention ,first 12 mm leave 0.5 then overlap 0.1 with 6mm
medium- same but second time with 12 mm
big- only one pass
the only thing is that i add also script for the tool order ,because you must order in 2 lists
one for all machining ,second only for nesting machining(that go throw 0.1mm)
and then order by ,first the part in the corner then by size
in this method ,i run all my parts in the the fast way
thanks
Yaakov
11/20 #23: Determining Vacuum Holddown ...

We cut parts that small and smaller every day with no problem. It appears your two small parts come in pairs. Onion skin them together. We have a router table on the out feed table of the CNC with a flush trim bit. Cutting parts like that apart is part of the secondary operation that is done when the next sheet is running.
The part shown is total 10" x 10 the small squares are 2 x 2". I pull a 3/8 bit through 2x's to make the groove 1/2" sp a 3/8 flush trim bit will go through and leave a .01" skin.
Good luck!
View larger image
11/22 #24: Determining Vacuum Holddown ...

Like others said you just have to be more creative with your programming. I have a 10 hp becker and there isn't a lot that I haven't been able to do.
I don't have an unlimited electrical service, so I couldn't run a 40 hp even if I wanted to.
11/22 #25: Determining Vacuum Holddown ...

Yaakov, Bill, Scott - Thanks for the advice guys. Once I get the machine in I will be able to test out all these methods for my parts.
11/22 #26: Determining Vacuum Holddown ...

Have you considered a pressure foot in addition to the vac. there are some who discuss this on a machine forum with some success
11/22 #27: Determining Vacuum Holddown ...

Im not familiar with this. I am looking into it now. Thanks!
11/22 #28: Determining Vacuum Holddown ...

I have not used one but there are some who swear by them with a bracket they can be adapted to the mid smaller machines
CNC Pressure Foot
11/22 #29: Determining Vacuum Holddown ...

Pressure feet and ply don't play well together. In my experience, unless you use a roughing but ply can come off in slivers and strings and they can get caught in the foot.
11/22 #30: Determining Vacuum Holddown ...

Dropout - Thanks for he input. I don't plan on trying to go down that line until I max out the other options.
11/22 #31: Determining Vacuum Holddown ...

one thing about vacuum that very important
that i saw all the time ,and i think many people mistake about it
vacuum is not like pressure
if you add 1000HP you always have limit
because you just create vaccum ,
the pressure is the Atmosphere
max max 1 ,but this is Theoretical, the real
is 0.7-08 not more, so more pumps you add is just Compensation for the leaks from the cut ,its cant add more pressure...
from my experience 500 kph its very good for up to 2.8*1.2 m plywood
and we cut all size ,from drawer back(70*400mm) up to...
thnaks
11/23 #32: Determining Vacuum Holddown ...

Website: http://www.qingonggroup.com
Chris, a 10HP Becker for your CNC with a 5x10 table is ok. 5x10 vacuum table with 6 vacuum area, A B C D E F area. if the small parts in E F area, when cutting small parts, you can close A B C area, so E F area vacuum suction power become bigger to hold the small parts.
If the small parts is too small, you can try a CNC pressure foot.
CNC pressure foot
11/24 #33: Determining Vacuum Holddown ...

Thank you for all the input. Right now I am leaning towards a 25hp 455 CFM Busch pump. I think this, coupled with the advice I have received here, will give me a great start. If anyone else has any input, it is still greatly appreciated.
11/26 #34: Determining Vacuum Holddown ...

We run a Quincy 15hp rotary screw vacuum pump on a 5x12 with no issues, and uses very little power compared to a 40hp dekker
12/16 #35: Determining Vacuum Holddown ...

Website: http://www.allstaradhesives.com
There is an interesting product developed by CNC Automation of Canada (Peg Board Tile) which allows Nested Base Manufacturing to be used on a CNC Router without the necessity of "onion skin" or "tabbing" as the means of holding the finished parts on the table.
YouTube: https://www.youtube.com/watch?v=jN0wLRa3tQM
If you have any questions you could contact George Bradley (800-878-7827 / Ext 202) at All Star Adhesive Products, Inc.
12/16 #36: Determining Vacuum Holddown ...

The foam works well sort of.
I have tried it with melamine and found it to be unsuitable.
The idea is to just touch the foam without cutting it. The problem is that a sheet of dead flat material such as melamine will crush the foam more than something with a grain in it. Also, you may have a problem with chip out on the bottom of the panel because the foam gives a bit, unlike an MDF spoilboard.
Also, while it's a cool video, the crush will change on how much of the table is covered.
It could work well for use as a dedicated fixture/spoilboard for a specific job, but be prepared for the setup time.
12/16 #37: Determining Vacuum Holddown ...

The foam will compress. How much it will compress is a factor determined by the strength of the vacuum system. The "new" thickness and density of the foam will be consistent, rather than being "crushed" and losing all compression set, which is the key physical property in reducing v-i-b-r-a-t-i-o-n and improving both the quality of the finished edge and the life of the tooling.
Peg Board Tiles are adhered to the surface of a virgin sheet of MDF or LDF. The smooth surface allows the pressure sensitive adhesive to remain in place and not shift or slide.
Longevity > current users claim 4 to 6 months.
3 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|