End grain gluing

2/3/20       
Stefano

I wonder if someone have suggestion for end -grain joint. Yellow glue or white glue?
Any brand?
Thank you
Stefano

2/4/20       #2: End grain gluing ...
Adam

More information.

2/4/20       #3: End grain gluing ...
Stefano

Adam, I'm jointing hard maple picture frames. I'm using white glue instead of yellow because the white have some flexibility and seem to me absorb more the movement of the wood during the change of the weather. 10 minute before I joint the frames I apply 50/50 mixed water/glue to the mitered joints to avoid the wood absorbing too much glue, after 10 minutes I apply the glue and I joint the frames. Doing like so I have strong glued joint but some time after few months some of the joints show a little separation and I wonder if there is a better technique or glue
Thank you

2/5/20       #4: End grain gluing ...
Adam

Simply use Titebond1 yellow glue. Do not water it down. Put enough glue on so you need to wipe it off after assembly. Depending on the moulding size you can use a biscuit or spline to help keep it together.

2/5/20       #5: End grain gluing ...
Stefano

Thank you Adam but the wood need to prepare in some way otherwise the pores of the end grain will absorb part of the glue

2/5/20       #6: End grain gluing ...
David R Sochar Member

Stefano is following the instructions for miters from when white glue was the primary wood glue in use. Pre - Titebond, when Elmer's was it. He probably learned it from the same old codgers I learned it from back in the 60's.

It is good practice - I still use it with TBI when gluing miters, but I omit the water.

Spread a thin bit on each half of the miter and let it sit for a few minutes. Then add a bit more to one side or the other and assemble then clamp, wiping off excess with damp rag.

Be sure the clamping does not distort the frame members. Be certain your wood is the proper moisture content. 6-8% for most of the US is where you need to be.

CSI - Wood:
How wide is the cross section of the frame members?
Species?
When you inspect the joints and find separation, is it always on the inside (heel) or the miter or the toe? This can indicate wood movement from drying.
Is there any visible dried glue in the open joints? Inside edges or outside edges, both or neither?
Are the miters themselves perfect? Test frequently and rigorously, by dry clamping 3 corners. The fourth corner should just touch - not open, not hitting hard. If you don't have that right, no amount or type of glue will correct it.

2/7/20       #7: End grain gluing ...
Stefano

Thank you David for the beautiful technical informations. I use hard maple and the frames are thin, from 1/2 to 3/4'' faces. Usual separations is from inside, but it's noticeable mostly when I paint the frame white and more that obvious separation is a thin line
Stefano

2/10/20       #8: End grain gluing ...
David R Sochar Member

If inside miters are opening, then your wood is too wet, or your miters are inaccurate, or both.

Normal, seasonal wood movement will never be a factor in a 3/4" wide frame. Maple will move about 0.010" with a 12% to 7% change in MC. Use the "Shrinkulator", check your moisture content, and revisit how you miter, and proof the miters rigorously.

2/10/20       #9: End grain gluing ...
Stefano

Thank you David for your amazing suggestions. I will buy the moisture meter and check the wood. Do you have idea what will be the best moisture level to glue the wood or much depend of the variation of the moisture once the joint are done?
Thank you

2/11/20       #10: End grain gluing ...
David R Sochar Member

It depends upon your location. In the US Midwest, we use 8% as the Equilibrium Moisture content of hardwoods for interior use. Coastal areas are higher, desert lower.

Bruce Hoadley's "Understanding Wood" is the best book for this type of info. Strongly suggested. It will help you understand the basics, so you don't have to worry about the wrong things.

2/11/20       #11: End grain gluing ...
Stefano

Thank you David I ordered the book. I'm in New York were there are some climate variations . Humid in the summer and dry during this season. I really want to thank you for all those suggestions
Stefano

3/19/20       #12: End grain gluing ...
Marty Member

We've always used white glue on end grain as its often more forgiving when it comes to movement. If theres a mechanical fix you can use harder glues.
We also tap lots of dents into the ends with the corner of your chisel to give the joint some teeth.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Vacuum Pressing Systems, Inc.
      Vacuum Pressing Equipment - Including Bag and Frame Systems
    • Excel Dowel and Wood Products Inc.
      Plain and Pre-glued Dowel Pins, and Wood Parts - Servicing Small Hobby Shops to Large OEM's
    • ULTI-BOARD
      The Ultimate Spoilboard - ULTI-BOARD - Specifically Engineered and Formulated for the Ultimate in Spoilboard Performance - Not Your Ordinary Sheet of MDF.

    Become a Sponsor today!