Quick turn around adhesive
3/18/22
I do a lot of work on architectural grade wood doors, they are made of a particle core with a veneer of choice.
I do many rerails in height and restiles in width, I am looking for a glue or some other adhesive that sets up and is workable in a very short time.
I usually use a yellow wood glue and leave them clamped up overnight but I am looking to do a quicker turn around.
3/24/22 #2: Quick turn around adhesive ...
One hour or even faster curing epoxy comes to mind.
John
3/30/22 #3: Quick turn around adhesive ...
Formica exterior grade golden glue, that's all we use and it is excellent glue. We make furniture and qw have components in an air clamp for under a minute and then set aside. Very good glue.
4/4/22 #4: Quick turn around adhesive ...
I suggest you do a few tests to convince yourself that yellow glue sets in less than an hour. Many shops glue panels for width, and an hour later are sending them thru a planer. You need intimate contact (for the glue joint) and good clamping.
4/26/22 #5: Quick turn around adhesive ...
I was using an urethane glue that came in a calking tube. Misted water on the parts, applied glue and clamped. Cured in ten minutes. Can't remember the name (off internet) Shelf life on a case of glue wasn't that good. Lost tubes so we quit buying it. I'd like to have it again if I could get a few tubes at a time. Cured glue said it was waterproof. Look around on the internet, guessing it's still out there.