Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Solid Wood Plank Entry Door

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Solid Wood Plank Entry Door

5/16/14       
Jeff Brown  Member

I have been asked to copy a weird plank door by a contractor who can't wait the 8 week lead time from the factory (for a very expensive door that he probably underbid and stalled on while he schemed to minimize his losses).

http://www.simpsondoor.com/door-products/search/detail/?BaseSpecificat
ionID=3127

The door is standard entry dims., 1-3/4" x 36" x 80". The weird part is that it has a 6" top rail and a 12" bot. rail that run the full width of the door. There are an odd number of planks allowing for the center "plank" to be recessed, clear, 1/2" glass that runs from top to bot. rail. It will be painted both sides. I will probably use 8/4 sapele.

Location is N.W. CT., very humid summers, fairly low humidity in winter. Always comfortable inside. The door will never see direct sunlight or rain being on a very large, raised, covered porch.

I have been given a fair amount of leeway to alter the design. I may even be able to run the stiles full length as well. Maybe that may help the joinery.

Other threads suggest a floating tenon glued to each stile, and allowing the planks to float freely about the frame but this door has a piece of glass in the way.

I am concerned that without the intermediate tenons (hidden rails) the door will be weak, but am not sure. If so, I'd like to design the structure a little bit differently to overcome this weakness, maybe by joining the planks nearest the glass to the rails with a tenon. There will be ~15" wood to either side of the glass - 1 stile and 2 planks.

Any ideas? Suggestions?

Thanks

5/17/14       #2: Solid Wood Plank Entry Door ...
Jeff Brown  Member

Sorry, I can not figure out how to post a link in-line or edit my post. The link got wrapped so it was not easily pasted. Here is a drawing of the door, and here I will try to post the link again.

Click the link below to download the file included with this post.

Clark_Entry_Door.pdf

link to door

5/17/14       #3: Solid Wood Plank Entry Door ...
Brian T

Edge glue verticals. Cut slot in top and bottom plus rails for a spline stopping before the outside edges. I would not use a mortise tenon for this application.

You will want to make spline stock at least .75 x8''long x width of each outside style. Make sure to cut small grooves to allow for better glue surface adhesion.

The splines will receive 4'' into style and rail. Don't mortise all the way to the outside edge of the rails and styles. Similar to a haunched mortise and tenon. This will hold glue in and hide the joint.

Next make splines for the inside styles or panels. They can be smaller. Only need to go 2'' into both pcs. Glue splines into top and bottom of inner styles. Next glue outer splines into both top and bottom of styles leaving roughly .5'' of space between the 2 tenons. Make sure to clean all glue out of joint. The next day I would do final assembly. Only glue the 4 outside splines Let the 4 wider inside splines float in the joint to allow for expansion and contraction.

You may also want to put a micro bevel on both floating panels tops and bottoms where the joints are to hide expansion and contraction.

Sapele will work well and I would also use epoxy like west system for the glue joints.

5/17/14       #4: Solid Wood Plank Entry Door ...
Jeff Brown  Member

Thanks,

Here's a drawing of what I think you meant. Is this right? The dark rectangles are the splines.

Would the splines be sapele also?

For sure on the West.

Click the link below to download the file included with this post.

Clark_Entry_Door_splines.pdf

5/17/14       #5: Solid Wood Plank Entry Door ...
Brian T

Yes that is exactly what I meant.

Sapele will work well for the splines.

We have used marine grade ply for large splines in the past hoping it would negate any opposing swelling between the two joints and floating members. I really can't say if it makes a difference though as I have never put a solid spline joint side by side with ply spline joint for any period of time.

Neither joint has ever failed. Most of our custom doors are mahogany species glued with west and are all solid styles and rails. They are almost all directly on or near the ocean from the cape to N.H.

We even have doors on Buzzards Bay that actually get submerged in high water and storm surf that have not failed in 17 years. 8 doors in total.

5/17/14       #6: Solid Wood Plank Entry Door ...
Jeff Brown  Member

Thanks Brian,

I am really concerned that there is not enough holding this door together by only gluing at the 4 corners. This door will be very protected by cover and paint.

Are we designing in too much allowance for wood movement at the expense of too little strength? This door will be heavy. Won't it sag and pull itself apart with such a small glue surface where the bottom rail is essentially hanging off of the stile? Had the bottom rail been tenoned into the stiles like usual with wide tenons and shoulders I think I would be much less apprehensive, but its not.

Can you please explain what would be wrong with gluing the 2 planks adjacent to the glass to the rails and not edge gluing the planks in order to allow for wood movement? In that case I would still allow the center plank on either side to float. In fact, I am so ignorant in this type of construction, that thinking about it, I do not understand what would be wrong with gluing the center plank into the rails also (but not edge gluing it to allow for expansion). To me that would allow for more strength as well as keep the plank centered.

I am definitely in need of an education here.

5/17/14       #7: Solid Wood Plank Entry Door ...
rich c.

Everyone one of those boards is going to expand in width, not length. Glue all of them solid to the top and bottom rail, and the wood can't move. Those rails will attempt to hold it solid. Unless you have some kind of wide tongue and groove that will show gaps in the winter and be tight in the summer. If you don't give enough room for it to expand around the glass, and it might blow it up. Quartersawn wood moves a lot less. Slab doors went out of favor in colonial times since they stick in the summer and you can see light in the winter. Veneer is the way to go. Make it look like a slab, don't make a slab.

5/17/14       #8: Solid Wood Plank Entry Door ...
Brian T

Gluing the doors in the 4 corners is more then adequate. With splines of this size and epoxy properly applied in the joints the door should not fail.

You could glue the entire length of spline into the top and bottom rails however it would add considerable strain to the joint with seasonal expansion and contraction mainly of the top and bottom rails.

Using quarter sawn stock as Rich pointed out will help and almost always does with doors. Ribbon grain Sapele is in my opinion the proper selection.

Leave adequate room for the glass and glaze with silicone after finishing.

We have made numerous doors 9' and taller with only top and bottom glue joints and no center rails. Joinery is the key.

You could go with a slab door but as Rich said they have seasonal issues. I would steer clear of veneers. Your adding unnecessary labor to a rather simple design and build.

It may seem like a difficult door to produce but if it was Simpson would not be making it.

5/17/14       #9: Solid Wood Plank Entry Door ...
Jeff Brown  Member

Got it. I'm kinda embarrassed that I actually said I could glue all of the planks to the rails without detriment. What was I thinking?

Sapele is available at my local mill. He said I should have no problem picking through it for the quarter sawn. I was planning on that.

The splines will definitely help with getting the shoulders perfect quickly. And the West System is readily available here on the Hudson.

I appreciate the reassurance on the joinery, Brian and I do feel better about it after your response but I'm still a little leery. Since the contractor has given me some latitude to modify the design, do you think it would be significantly stronger to build the door with full length stiles so that the rails run into the stiles instead? Or are there other problems I am not foreseeing using that method?

5/17/14       #10: Solid Wood Plank Entry Door ...
Shaun

In using a solid sapele spline does grain direction matter considering the size of the splines?? Several years ago I had a redo job of ipe "rings" that came apart due to the splines easily breaking along the grain lines. I think those splines were 3/8" thick x 5" wide. I fixed the job by simply turning the grain of my splines and re-glueing. Made the rings plenty strong enough to handle for installation.

5/17/14       #11: Solid Wood Plank Entry Door ...
Brian T

You could run the styles into the depth of the mortise. The main reason for not doing this in this application is simply to glue each style up in one pc and apply splines after. If you want to add the labor to run tenons on the styles then glue sand then glue all other pcs after then that will also work..

Shauns question about the splines is a good one.. You should always run the splines grain in the direction the most resistance will occur. Which in this case would be vertically.. In the case of a standard door would be horizontally and in the case of a Barrel door would be horizontally.

5/17/14       #12: Solid Wood Plank Entry Door ...
Brian T

I forgot to mention I would never use Ipe for anything like this. Its not an architectural building material but it does look great on decks.

5/17/14       #13: Solid Wood Plank Entry Door ...
Joe Calhoon

We did a house full of this type door a few years ago. We used square edge cope and stick, Splines, not glued between the planks, loose tenons glued on the interior planks and dowel joinery glued at the corners. Any type of joinery done right should work. Material should be well seasoned or engineered.
This allowed the planks to expand or shrink a little. In my area wood usual shrinks but the opposite might be true in CT.
I was worried about this job holding up especially the exterior door with the wide members. Last time I looked everything was fine. 6 or 7 years old now.
Joe


View higher quality, full size image (680 X 907)


View higher quality, full size image (680 X 907)

5/18/14       #14: Solid Wood Plank Entry Door ...
Shaun

I agree that using ipe when glue is required for joining is not a good idea. I fixed a job on a yacht that had ipe decks, handrails and accent pieces (large trim rings that decorated ceiling fan recesses) The previous builder used gorilla glue and glued the rings together with splines and edge glued the handrails together. All met with failure! I cut strips and face glued all the ipe up and around all the curves with TB3 and except for one handrail in back that they tried to tie the boat up with they all remain intact 4 years later.

5/19/14       #15: Solid Wood Plank Entry Door ...
David Martin Member

I think you must consider all the aspects whether positive or negative to get best possible outcomes.

5/19/14       #16: Solid Wood Plank Entry Door ...
David R Sochar Member

I have built many doors like this, but my methods are somewhat different, and based on historical doors that have survived decades.

I would build this as a three ply 'ladder core' door, with the center ply being a mortise and tenoned frame the full width and height of the door. Two stiles 5" wide or so, and about 6-8 rails with 3" tenons into the those stiles a very rigid core. All from jointed stock at 3/4" thick. This is simplified - yours will be more complex with the glass in it.

Think of the two faces as laminations. I would join the two vertical stiles to the rails with long, open tenons the full width of the rails, again, all at 3/4" thick. The filler boards would each be tongue and grooved into each other and the stiles and rails, glued to the core, with a gap between the t&g boards. The gap will be about .050 if v-jointed, and about.075 if square edged. Do not glue the T+G except at the ends of the boards. The idea is to let each board move in it place, while the outer perimeter is rigid. Ct is like Indiana - if anything, these boards will swell if the lumber is at 6-8% now. Fill the voids in the ladder core with rigid foam insulation before adding the second face.

Use quarter sawn stock - especially on that wide bottom rail. I would even consider making the bottom rail a five ply rail - face at 1/16", cross band at 1/16", core at 1/2" of quartered solids, then cross band and inner face. I see quartered Honduras Mahogany at 12" that hasn't moved, but I still would loose sleep over it. Other species I would not trust.

As stated to an earlier query about planks in a door, things are not always what they appear to be. Joe Calhoun builds a good door, and don't overlook his comment on "engineered" stock. Stable stock will eliminate all the movement issues and allow total freedom for reveals, joints, etc.

5/20/14       #17: Solid Wood Plank Entry Door ...
Jeff Brown  Member

Thanks for detailing your method for building this door, David.

I need to acknowledge that you, Joe and Rich all would not build this door solid. Having never built an exterior door, this is a daunting task for me, not only for the methods and materials, but for the size of the joinery and the parts. Your suggestion to through mortise the outer boards might be beyond my capabilities.

Some questions:

First, does the core mimic the outside in that the core rails run the full width of the door?

You said 5" stiles for the core. What should the widths of the other members of the core be in this case, especially the bottom rail?

It sounds like you mean to apply 3/4" T&G on the face. Would 1/2" work or is that too flimsy and subject to warp, as I assume? Are you proposing to build a 2-1/4" thick door? I was going for 1-3/4".

I understand you to be saying to glue the perimeter rails and stiles to the core, and let the other boards float. Could you clarify what you mean when you say not to glue the T&G except at the ends of the boards?

I do have a lot of questions on how to glue the outer boards to the core. But maybe just one for now:

If the core rails are not the full width of the outer rails, will there be an issue with cross-grain movement where the outer rails are glued to both the core rails and stiles at the corners? Or should the core rails be the same width as the outer rails for this reason? Would your suggestion to build 5-ply bottom outer rails allow for a narrower bottom core rail?

Thanks

5/20/14       #18: Solid Wood Plank Entry Door ...
David R Sochar Member

I neglected to mention that this would be a 2-1/4" thick door. Pretty much the standard thickness exterior door around here until after WW2.

You can make thinner faces - 1/2" - but the 3/4" allows for a t&g joint along their length. You should have something to plug the gap, since a gap has top be built into the door. 1/2" can allow for shiplap, but then one edge can curl - the t&g holds everything parallel.

The core rails can be narrower than the faces. I would use stock about 3-4" in width, and about 6-7 of them from the top to bottom. You want to lay them out so a rail - second from the bottom - catches the ends of the floating faces and the upper edge of the wide rail. Same at the top. I'd have to think and draw to figger out the glass....

Think of those floating face boards as 'semi' floating - they are glued to the core rails, and to the horizontal face rails where they meet, but not to each other along their length. Let each one move in its own little place is the guiding principle.

Cross grain movement will be most threatening in that bottom rail. I'd do several things: redesign it to 10" max, with quartered materials. The 5 ply is foolproof, though, and makes for a better long-term solution, in my opinion.

The pictures show a plank door with a small window going together: core, faces, and second face, with spacers.

My other recommendation is to sub this out to a pro shop so you can do what you are good at, and lessen your exposure. It sounds as if you are capable, but there are lots of things about doors that are not anticipated until after they are made. Also to be considered are the jamb, sill, weather strip, finish and hardware.


View higher quality, full size image (2592 X 1944)


View higher quality, full size image (2592 X 1944)


View higher quality, full size image (2592 X 1944)

5/20/14       #19: Solid Wood Plank Entry Door ...
Jeff Brown  Member

Am I understanding you correctly that each outer board is glued to every inner core surface it contacts? In other words would the entire face of the core be covered in glue? I have to ask because I am not used to gluing anything but veneer cross-grain so I am not sure if you are telling me to do this. Also, what glue do you recommend?

And yes you are right, I should not be building this door. Of course, "I'll look into it" has turned into, "where's my door?". But this contractor knows I am inexperienced building exterior doors and I have kept him informed of the options and risks. He wants it yesterday and so he is taking all of the risk. I will do my best but I also will not build it if I don't think it will be satisfactory.

At this moment, I want to build the ladder core door, even though Brian, who lives closest to my climate has assured me that it can be done solid. I just feel that the 3 ply door is less risky as far as stability and strength.

At this time, I have the lead carpenter checking out the existing hardware to see if it will fit the 2-1/4" door. Its expensive and the contractor said if it doesn't fit its back to 1-3/4".

Maybe I could get the hardware to stretch to 2"? Do you think 5/8" T&G would work? I'm guessing that you are recommending 3/4" T&G because any thinner might leave too thin of a wall around the groove and possibly snap off under stress?

5/20/14       #20: Solid Wood Plank Entry Door ...
Joe Calhoon

Jeff said
"I need to acknowledge that you, Joe and Rich all would not build this door solid.

Jeff, we did do this job solid. The exterior door totally solid because we had some exceptionally good wood. Not always the case. The interior doors were only 1 3/4" thick and we used a stave core stile on the long edges.
We do plenty of ladder frame plank doors pretty much as Dave describes only using LVL for the ladder frame. What he describes would also work here. His method will be more costly and ladder frame doors lend themselves to 2 1/4 or thicker doors.
But you have a stile and rail door here with just a little different arrangement of the stiles and rails. The location of the window actually makes this pretty easy to construct solid with stave cores. As I said in our area wood shrinks. You will need to calculate worst case expansion and contraction for your area. Even if doing the ladder frame.

Joe

5/21/14       #21: Solid Wood Plank Entry Door ...
rich c.

"But this contractor knows I am inexperienced building exterior doors and I have kept him informed of the options and risks."

Don't kid yourself Jeff. If it goes bad, you will be number one on the hit list.

5/21/14       #22: Solid Wood Plank Entry Door ...
David R Sochar Member

The more I look at this, the more I can see it go as solid wood, per Joe C's suggestions. I think this is an example of how two different methods can meet each other and both be equally sufficient.

Perimeter parts tenoned and rigid, with floating panels/boards within. The only part that I would obsess on is that lower rail - that would definitely be made as a 5 ply rail. Something has to be done to keep it from cupping. The two boards that flank the glass should tenon into the horizontals, and the other two boards should float as panels.

The best advice I ever got was from a mentor of sorts that would assign me work many years ago in my first real wood job. I asked how to build the project, and he would say that I would figure it out. And I would. But after a while, when I was done, he'd mention 2 or 3 other ways of doing this or that.

When I asked him why he didn't give me those suggestions before the project, he said that the best thing I could do was to come up with 3 good solutions on my own and then select the one I want. This has kept me from rushing along with the first thing that came to mind, only to find myself painted into a corner of some sort.

5/22/14       #23: Solid Wood Plank Entry Door ...
Jeff Brown  Member

I guess I was using the term "solid" to refer only to "solid wood", not engineered. I suppose I am constructing this door solid after all, in what I now would describe as as "solid stave core construction". Hope my terminology is right.

It is going to have 4 pine stave core members with mahogany veneer and edges for a 1-3/4" thick door: 1\ 5-1/2" Top Rail, 1\ 10-1/2" Bottom Rail, 2 side stiles at 14-1/2" wide each. The ends of the rails will be edged.

The plan is to spline or tenon and glue the stiles to the rails along the entire width of the stiles using west system and leaving a gap in the center for the glass which will be stopped on both sides, the outside stops being glued.

After the glue up, I will route the v-grooves into the door. It was proposed by the stave core manufacturer to build a stave core slab, veneer the entire thing and then v-groove.

I don't have the means to build that way and he wanted too much to rush it and need to get this thing done. Also, I wasn't so sure about that idea. So I made the quick decision to have him rush the parts as I think I know how to do this, with the stave core modification to Brian's proposal. I thought this mod would allow me to add the extra strength to the joints I want by allowing me to glue the entire length of the joint instead of floating most of it. I also thought it to be a much more stable material and significantly decrease the likelihood of warping. Lastly, I like that there will be no expansion and contraction between the v-grooves.

The v-grooves will be narrow, the specs call for 1/8" which I will probably increase slightly because of the paint. My main reason for choosing to build and v-groove in this manner was time, knowing that it will be painted and is under very good cover.

I did consider the ladder core in depth. But the time I thought it would take to build as well as not being comfortable with my understanding of the method stopped me in my tracks.

Thanks for everyone's input. You guys helped me a lot. I appreciate all of your generous time and wisdom.

5/22/14       #24: Solid Wood Plank Entry Door ...
Joe Calhoon

Jeff,
Be careful with all this advice. My method requires a small gap in addition to the v joint between each board. This is to allow the member to expand a little. As it shrinks the gap will get bigger. Based on experience in my climate this works. As I said most everything shrinks here more than grows.
Stave core with solid pine for the core will still expand and contract. The idea of stave core construction is to keep the members from bowing, cupping or twisting.
If you don't want any gaps then you would need to do the entire door with some type of substrate that does not move, veneer to the design and route in the Vs.
I have seen this done with light weight honeycomb cores with 1/2" or so MDF faces inlayed with solid material where the Vs are routed. I do not like building exterior doors with thin veneer but is the only solution if you cannot live with the gaps.
Joe

5/22/14       #25: Solid Wood Plank Entry Door ...
Joe Calhoon

Jeff, Have a look at this UK door.

Not sure of the exact construction but it looks like he has allowed for movement of his solid cladding. It is a interesting form of ladder frame. Joe

Door

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory