Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Maintaining 1/8” gap on exterior t&g siding

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Maintaining 1/8” gap on exterior t&g siding

4/17/19       
John L

What type of tongue and groove mil specification and installation method would you suggest for exterior vertical tongue and groove edge matched genuine mahogany siding?

Customer is looking to maintain a clean minimum 1/8” gap without it closing up due to seasonal expansion. The mahogany is 3/4” flat sawn 4” wide which will be prefinished all sides & edges. I determined the tangential expansion worst case scenario to be .06” from its kiln dried state of 6% MC to a worst case MC of 15% during peak humidity, 10% being a more realistic number.

Would you mill the tongues 1/8” deeper than the grooves to provide an expansion stopping point and space the boards an additional 1/16 or .0625” to compensate for seasonal expansion? Or would you rebate the face above the tongues and space accordingly? Or is there another way?

How would you fasten them to allow the boards to expand and contract to maintain a consistent gap and what type of fasteners would you recommend? I’m concerned with panelization and an uneven gap when contracting during the dry season. Any ideas? Buckling is also a concern, but if my math serves me correctly, the 1/16” spacing “should” be fine.

Thank you in advance for any responses.

4/18/19       #2: Maintaining 1/8” gap on exterior t& ...
Haroldd Pomeroy

In doors, I pin the tongue and groove panels in the middles to average out the wood movement. Having narrow wood will help.

Some education on wood movement ahead of time will calm the customer's anxiety when the wood moves, because it will.

Finally, a set of feeler gauges measuring 1/32" to 1/4", all labeled as 1/8", would help.

4/18/19       #3: Maintaining 1/8” gap on exterior t& ...
John L

“Finally, a set of feeler gauges measuring 1/32" to 1/4", all labeled as 1/8", would help”...haha...good one...forgot the dark pair of sunglasses..lol.

Yes, averaging out the wood movement is what I’m looking to achieve and wondering if face fastening vs blind fastening is the better approach.

4/19/19       #4: Maintaining 1/8” gap on exterior t& ...
Chris H.

Website: https://www.csaw.com/lamello/

Love Haroldd's idea of the 1/8" spacers!

Agreed, laws of Nature apply to all customers, so there WILL be seasonal expansion and contraction. However, you mentioned flat-sawn material. Is quarter-sawn available? That will shrink less across the grain than flat-sawn. And as Haroldd mentions, fastening in the middle of each board is a good best practice too, like fastening a breadboard end on a farmers table. Acclimatization of the material is also a good idea. I found a pretty detailed link below about seasonal movement for you. Good luck on this one! When I had my shop and would field requests like this (which fly in the face of the laws of wood science) I would exempt that part of the project from my warranty. Just saying.

Wood Movement

4/19/19       #5: Maintaining 1/8” gap on exterior t& ...
John L

Thanks Chris. I did consider quartersawn but the difference in expansion across the width for flat vs quartesawn was only .0163” based on the expected MC change. The shrinkage calculator resource on this site was very helpful.

It would probably be a good idea to sticker the material in a garage or covered location to allow it to acclimate as you mentioned so any dimensional changes will be less drastic, although time is of the essence...you know how that goes.

I did decide to have the material sent back to the mill and have them rebate the board faces above the tongues 1/16” in the event the boards do compress, so at least the gap won’t totally disappear.

The existing siding being replaced was supposed to have a nickel gap and was spaced 3/32”, yet compressed, not looking too attractive. Subsequent refinishing resulted in bridging of finish at the non-existent nickel gap, water getting trapped/not shedding, resulting in finish failure at edges. I’m hoping to avoid a repeat scenario.

I’m not the contractor doing the installations, the client and architect deferring to me for sound advice. I’m guessing the installers will be utilizing wire nails, toe nailing above the tongues. I’m wondering what options there might be for fastening. The installers were concerned with buckling. Although science dictates that 1/16” spacing would work, I just bumped up the spacing specification to 3/32” to appease their concerns.

Thanks for the link!

4/20/19       #6: Maintaining 1/8” gap on exterior t& ...
Adam

Think of it as flooring. It will not buckle.

My mind of expansion was completely changed by a massive water leak in my old carriage house workshop. The floor is 32’ x 32’. 6” wide x 16’ southern yellow pine was installed with typical Bostich flooring staples. No face nailing.

There was a massive water leak on the 2nd floor. It had 1” of standing water on the floor for 1 week. The pine floor only buckled at 2 location(4 boards) across 32’. The rest looked perfect.

1st thing regardless of how you mill it would be to leave it outside for 2 weeks to acclimate to the outdoor moisture content.

I would assume the wood is going to expand rather than shrink. Depending on your location the gaps may change during the seasons.

Think of this project as vertical flooring. Making the groove any deeper(1/16” typical) achieves nothing. The shoulder matches the tongue.

I would gap it with 1/8” spacers and be done with it. The gaps may close to a 1/6” and expand to 3/16” throughout the year.

It’s wood it moves end of story.

4/20/19       #7: Maintaining 1/8” gap on exterior t& ...
Russ

Website: http://www.mr-moulding-knives.com

Is this blind nailing joint an option? We offer many other siding designs you may want to review and consider. Happy Easter Russ @ MR

tongue-and-groove

4/20/19       #8: Maintaining 1/8” gap on exterior t& ...
Pat Gilbert

Adam

Floors buckle all the time?

4/21/19       #9: Maintaining 1/8” gap on exterior t& ...
Adam

Pat ,

What?

4/21/19       #10: Maintaining 1/8” gap on exterior t& ...
Pat Gilbert

You state "It will not buckle."

I'm saying that floors do buckle

I'm trying to understand your take on this

4/22/19       #11: Maintaining 1/8” gap on exterior t& ...
Walter Member

All six sides of the siding should be finished to reduce the movement of moisture in and out of the wood.

Knowledge Base Article

4/22/19       #12: Maintaining 1/8” gap on exterior t& ...
Gerry

This floor never got wet but the space under it flooded. The floor gained a lot of moisture. I calculated in the 40' of width it moved between 3 and 4 feet.


View higher quality, full size image (1280 X 960)

4/22/19       #13: Maintaining 1/8” gap on exterior t& ...
LJ

I'd tell the customer 1/8" is too tight a reveal to maintain consistently throughout the year. Even an extra sixteenth would make all the difference visually. I would mill it with an 1/8" groove when pushed together hard and have the installer use a 3/16" spacer. Room to grow and room to shrink.

4/22/19       #14: Maintaining 1/8” gap on exterior t& ...
John L

Thanks LJ. We finally settled on milling it 3/16” and spacing it an additional 3/16”....very close to your suggestion.

Will settle for a 3/16” vs” 1/8” minimum gap. Should be good.

4/22/19       #15: Maintaining 1/8” gap on exterior t& ...
BH Davis  Member

How much time to you have to let the wood acclimate to the outdoor air. In most situations the wood will begin to take on moisture as soon as it comes out of the kiln.

If you don't already have one pick up a moisture meter and find out the MC of the wood at the time of the install. The 3/16" is overall a good idea but if the wood has acclimated to 9% to 10% when installed you could likely have good results with the 1/8" gap. Depending of course upon your location and real summer max. moisture levels.

Most mahoganies (real or substitute) will be fairly stable. Quarter sawn would be better but as you implied might not be worth the extra cost. I'd think the numbers you got for expansion would more likely relate to each 12" of width vs. 4" of width. I could be wrong on that though but thought I'd bring up the point.

BH Davis

4/22/19       #16: Maintaining 1/8” gap on exterior t& ...
John L

Correction, the final spec was 3/32” milled gap and 3/32” additional spacing...

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory