Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Hand Hewn Fronts

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Hand Hewn Fronts

2/14/20       
Orin Zelenak  Member

Website: apg10.com

We need to reproduce a hand hewn look on cabinet fronts. Would prefer to gouge into engineer fronts with 6mm solid layer (front and back for balance) instead of solid.

Finish is opaque lacquered (off white) with black ceruse on Plain Sliced white oak.

Don't want to reinvent the wheel. Thoughts?

See image below

Click the link below to download the file included with this post.

Hand_hewn_fronts.pdf

2/15/20       #3: Hand Hewn Fronts ...
james e mcgrew  Member

Website: mcgrewwoodwork.com

Like this,, Done in Aspire using a fluting or texture toolpath


View higher quality, full size image (1024 X 683)


View higher quality, full size image (1024 X 683)

2/15/20       #4: Hand Hewn Fronts ...
Thomas Gardiner

Certainly Wood sells special thickness veneers up to 1/8". I would be surprised if the texture you want to achieve would be deeper than 2mm. It would be awfully convenient for you to lay up balanced panels of existing veneers as opposed to resawing your own.

Certainlywood.com

You might be able to find or purchase a 3d model of the texture you want by searching for "hand scraped wood texture" or something like that. I definitely would do this with a cnc.

2/15/20       #5: Hand Hewn Fronts ...
David R Sochar Member

I do not think the word 'engineered' is a meaningful word - it is just a marketing term that has overgrown its use. Show me the calculations an engineer did for the drawer fronts.

If you have a source for real wood, and have the equipment and know how to work solid wood, then what is the fear of using solid wood? There is more 'engineering' (of the real kind) that has gone into solid wood than you can imagine. Making wood more useful can probably be the root cause for engineering to become the science it is. State Universities like Purdue have long studied wood as an agricultural component, and the Forest Products Laboratory has a huge amount of information - real science - available to US citizens.

Will those cuts into the wood somehow cause it to warp or twist? Is 'imbalance' inherent in solid wood? How could wood ever have attained its usefulness if we cannot trust a piece of properly dried wood to just lay there and not move around like some feisty 2 year old?

2/15/20       #6: Hand Hewn Fronts ...
james e mcgrew  Member

Website: mcgrewwoodwork.com

We did hdf on the large divider panels and solid cherry on the doors in the lobby. I did a balance relief on the backs of .25 equal to the " Gouge" on the face

2/15/20       #7: Hand Hewn Fronts ...
pat gilbert

Other options


View higher quality, full size image (1166 X 493)

2/15/20       #8: Hand Hewn Fronts ...
rich c.

Hand hewing with a broad ax involved scoring perpendicular to the grain, then splitting off between the score lines. Definitely not all parallel lines to the grain. Research the broad ax on youtube. I'd do the texture on both sides of a piece of stock, then resaw it off and laminate to the manmade sheet goods.

2/15/20       #9: Hand Hewn Fronts ...
Keith Newton

I agree with Rich c. I would however add that if you are thinking of trying that method, that most hand hewing is done on green wood. It is MUCH harder x2 if the wood is dry.

Dr Wengert has pointed out several times that drying thin wood is a different creature from drying lumber, in that you will likely have sagging between normal spaced stickers. However Ive had pretty good results stretching a cable high enough across my parking lot to just hang some 1/8 planks like laundry.
Some soft wood will dry in a day on a hot day.

2/15/20       #10: Hand Hewn Fronts ...
TonyF

Orin Zelenak:

The example in your link has larger "flats" and is much more random than the example shown as produced by CNC.

I agree with David that this would best be done on solid wood, as the depth in your example might exceed the thickness of any applied veneer that I would feel comfortable using, and you don't have to worry about going through the veneer to the core material below.

I don't know what kind of square footage you are talking about, but if it were me, I would use the King Arthur "Lancelot" chain carver on an angle grinder, and then hit it with a flap sanding wheel.

This will give the randomness that your example has, and you don't need to kill yourself trying to use an adze on kiln dried hardwood.

Its quicker than you think, and somebody has already invented the wheel in chain carver form. Been there, done that.

Hope this helps.
TonyF

2/16/20       #11: Hand Hewn Fronts ...
Mark B Member

The problem with the angle grinder or any abrasive method is that it really can tend to rely on the operators artistic eye and their ability or willingness to chase the grain and keep it looking natural. Same with the CNC. The beauty of true hand hewing is you split material off with the grain so the hewing tends to look more natural and follow the contours of the material better.

It all depends on the customer and their budget. Laying up a balanced panel and then hewing away one face is not going to be balanced and Im not sure how you'd handle the edge grain/banding. Would seem a nightmare. Though my guess is the vast majority of todays consumers would never know the difference between one of McGrews CNC surfaces (we do them all the time) and a true hand hewn surface.... Its the makers call as to what they can get away with.

If the customer will pay for true hand hewn I would run the fronts in solids and do it right. If on the other hand the customer is in the 99.9% majority of today consumers who likes "the look" but likes that it can be done cheaper more, than the CNC is the way to go.

I feel Davids pain having watched it unfold for many years less than he has but unfortunately its a hard existence beating yourself against the rocks of changing times.

2/16/20       #12: Hand Hewn Fronts ...
TonyF

Mark B:

I would agree that irrespective of ones tooling choice, having a good eye, and the ability to coordinate that eye to a process and skill set, is a good thing to have.

I look at the sample shown by the OP and it looks more like a hand process rather than a machine one, although I imagine if one took the programming time, it could be produced by a CNC with a repeat side to side offset of 12", 18", whatever one feels would produce the desired result and look "random enough".

If the OP's customer has that brochure in hand, and is set on "that look", then one might have to rule out a CNC for the project. That also depends on how deep the customers pockets are.

The one time I needed to do something like this I used the angle grinder because at the time, CNC machinery was only owned by mass producers of RTA furniture, and I wanted something faster than hand hewing.

The angle grinder was cheap, allowed it to be done in-house, and one could go back to fine tune the "hewing" to make it look "more random", if needed, using one's eye to make that determination.

If I had a CNC, or ready access to one, I would sell the customer on the CNC look, if it is not too late. Especially if I had a lot of square footage of this to produce.

Its funny about the advancement of tooling and processes, and how some can think that they are detrimental to the purity of the craft. Craftsman who cut a curve using a hand saw and a compass plane probably think less of those who swing a curve with a router and trammel, who in turn think less of those who use a CNC.

Years ago I used to think that lumber core plywood was the pinnacle of sheet goods, and yet at the time I worked with guys who thought that all plywood was junk; no telling what those guys would have thought of MDF. Everything has its place and its purpose.

Dinosaurs like me should not get so calcified in our own thinking that we don't see ourselves being surrounded by the amber.

Sorry for the rant.
TonyF

2/17/20       #13: Hand Hewn Fronts ...
Mark B Member

No arguments from me Tony.

I dont honestly see how anyone could cost effectively vector any hewing on the cnc that would take into account the actual grain direction/flow in solid wood fronts. Would involve importing images of each part and applying toolpaths accordingly. At that point your better off in the handwork as the job clearly has the budget for it.

I would think the vast majority of customers would take the "sell" on the cnc option based on cost and with high quality textures like James has shown many times with his work. That said, even with cnc texture toolpaths, randomization, and gadgetry, the textures can still appear plainly as man-made to some (less and less seem to care about such details though).

Im asked fairly regularly to reproduce a live/natural edge on parts that are S4S and our best solution has been a dense/heavy wood mallet and to pound down the edge material until you collapse the wood fibers to a point you can simply strip them off by hand. They follow the grain contours of the part as they peel off and leave all the natural dips, twists, and fissures, youd see in a "live edge" part. They tear around pin knots and so on. Something that would never be possible with a draw knife, spoke shave, etc.. And its fast.

As you say, the economics of the project pretty much dictate the possibilities.

2/18/20       #14: Hand Hewn Fronts ...
BradS

The trick with the CNC will be creating the artwork. Someone good at sculpting can create a much more random appearance. It is not that difficult to put in your piece size and manually sculpt the pieces to achieve whatever appearance you want. It still will not be quite the same as a skilled craftsman that can look at the grain patterns, but you can get close. It all depends what they want to pay or what resources you have.

2/25/20       #15: Hand Hewn Fronts ...
jonathan mahnken

Website: http://www.mahnkencabinets.com

http://www.oberflex.com/textured-wood-collection.html#references

2/25/20       #16: Hand Hewn Fronts ...
james e mcgrew  Member

Website: mcgrewwoodwork.com

One may be surprised at how easily this can be done with a CNC and Vectric software, there are two toolpath methods, one is random vectors using a fluting tool path and the other using the texture tool path feature. I have made some real Hay with this here and there, along with room dividers carved doors, name plates on sailing vessels etc. we are holding a "Camp" at my shop april 23-25 where Vectric and others come to present how to do much of this work. I think the VCPro software is like 5-600.00 and does all of what i do, i do not use #d toolpathing on textured work.


View higher quality, full size image (800 X 534)


View higher quality, full size image (1024 X 683)


View higher quality, full size image (800 X 619)

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!