Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Finger joint clamping

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Finger joint clamping

5/7/20       
Mark Member

Gentleman,

I have to do some low volume finger jointing. I have good tooling and a tenoning table on a shaper to produce the joints.

Does anyone know of an off the shelf solution for some clamps that can clamp or attach to both pieces and then pull them together tight in order to get a good glue joint?

I am open for any ideas.

Thanks,

Mark

5/7/20       #2: Finger joint clamping ...
rescraft

Couple of small wood blocks, hot glued to back, on each side of joint, pull together with clamp; rubber faced clamp over joint to keep flush?

5/7/20       #3: Finger joint clamping ...
BradS

I bought a finger joint clamp off Mac Campsure years ago. It is basically a two way acting clamp. Hold stock tight on each side, and it has another lever that clamps the two pieces tight. I do not have a picture, but I bet Joe C will.

5/7/20       #4: Finger joint clamping ...
Dustin orth

I went to my local plumbing supply house and got some 20' length of 3/4 black iron pipe and then just use the regular pipe clamp heads. I put mine on dunnage on the floor, can do 6 at once at the end of the day, that way your not tripping over them!

5/7/20       #5: Finger joint clamping ...
BH Davis  Member

Website: http://www.bhdavis.net

Take a look at the Gartop press in this thread from the Woodweb archives.

These are great machines for small batch clamp ups. However I can find no indication that they are still being made.

BH Davis

Gartop Press on Woodweb

5/7/20       #6: Finger joint clamping ...
BH Davis  Member

Website: http://www.bhdavis.net

It looks like it may actually still be in production.

BH Davis

Finger Joint Press

5/7/20       #7: Finger joint clamping ...
BH Davis  Member

Website: http://www.bhdavis.net

Oh...........I just noticed the date on that Youtube video. 2010. Sorry.........not looking promising after all.

Perhaps you could find a used one.

BH Davis

5/7/20       #8: Finger joint clamping ...
Bill

You have not said what you are making. If any of the material is going to be removed you might be able to go old school and use pinch dogs.

5/7/20       #9: Finger joint clamping ...
Mark Member

Bill,

I am making butcher block. Pinch dogs would requirer that I would have to run my staves much thicker to account for the holes.

BH, that is exactly what I am looking for. I have done a google search and they don't show up as still being in business. If I could find a used one, that would be the ticket.

Watching the video has given me some food for thought.

Mark

5/7/20       #10: Finger joint clamping ...
BradS

I attached an image of the clamp I tried to explain. No finger jointed stock handy. Not as nice as the air clamp by BH, but maybe give you an idea.


View higher quality, full size image (1200 X 1188)

5/8/20       #11: Finger joint clamping ...
chris

Here is an inexpensive option. Unknown how well it works.

https://rangate.com/products/arch-clamps

5/8/20       #12: Finger joint clamping ...
BH Davis  Member

Website: http://www.bhdavis.net

I'd forgotten all about that segment clamp from Rangate. I had one with my business and it did come in handy occasionally. It was a bit of a pain to use but it did work. There was no room to get the Workrite glue zapper in though so it was clamp up and leave to dry whereas the Gartop press had room for the Workrite head to get over the joint.

Thinking back a lot of years though Rangate may have been the US distributor for the Gartop press. I'd at least give them a call. If they were then they might know of a used one somewhere.

BH Davis

5/8/20       #13: Finger joint clamping ...
Joe Calhoon

I have the Gartop. They are no longer made. Soukup has one and a German company Lower makes a stationary one also.
The German hand clamp Brad shows is a good one. In semi retirement I would consider selling my Gartop if I could find a couple of those. I don’t know if they are still made. I have looked at the shows.

Pinch dogs work well if the back side does not show. Especially in softwoods.


View higher quality, full size image (1280 X 960)


View higher quality, full size image (1280 X 960)

5/8/20       #14: Finger joint clamping ...
Mark Member

Brad,

Thanks for posting a picture of your clamp, it's an elegant solution.

Joe, the Soukup preforms just like the Gartop. Do you have an idea of how much they run approximately?

Mark

5/9/20       #15: Finger joint clamping ...
Joe Calhoon

Mark, the Soukup arch clamp is about 9K.

It’s more industrial than the Gartop and has a feature that allows for assembly of premachined arch segments. This is a desirable method with some CNC machining centers.
The Gartop worked fine for me, I always do profiling and tenoning after the segments are joined.

11/30/24       #16: Finger joint clamping ...
Jim Lewis

Website: http://icarusfurniture.com

Yeah, this is a way old thread, but in case anyone else like me is searching the web for finger joint clamps, Felder makes a more reasonably priced Maxifix Mitre Clamp. You have to spell it that way to find it on their website. It requires you to drill 8 mm blind holes in the back of your stock to insert the clamp.

Not as elegant as the Gartop, but under $100.

Maxifix Mitre Clamp

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!