Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Machining small parts

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Machining small parts

7/25/20       
Mark Member

Gentlemen,

I've got a very interesting job that's being presented to me and I'm rolling it around in my head on how to produce the parts. I've signed an NDA but I believe I can talk about the parts without disclosing the product.

I have to machine 80,000 strips of oak that will be a 1/4 x 3/4 x 78" long with about 8 holes drilled and countersunk, one end with small radiused corners, the other end with a 12 degree bevel and the top edges eased all the way around.

No problem producing the blanks, it's radiusing, the bevel and easing the top edges in an efficient manner.

I have a pod rail router and could make numerous holding fixtures and machine the parts one at a time, but I don't want to tie the machine up just to run that job.

I've considered ganging parts together and beveling the ends in lots of 10 or more on a shaper and doing the same for the radius's on the other end, then drilling all of the holes on a drill press set up with stops. Not excited about that process.

I'm not opposed to buying another machining center to run this job either. The money is quite good.

I've never run a flat table router and am thinking that maybe I could put a lot of pieces on the table and let the machine do the work and have a guy just sit and load.

Is this a possibility? Will a vacuum pump hold those pieces if I put them on an 1/8 or a 1/16" wider then needed and let the machine do the final sizing and all of the drilling?

What are your thoughts? I am open for suggestions.

Thanks

Mark

7/26/20       #2: Machining small parts ...
BH Davis  Member

Website: http://www.bhdavis.net

Could you do all the machining on the CNC on a single board and then rip the board into your strips? This would solve the hold down issue plus take a lot less CNC time.

BH Davis

7/27/20       #3: Machining small parts ...
Mark Member

BH,

I can't.

I'm starting to think that I can cut out the shapes in a piece of 1/8" tempered hard board to act as a locator and place multiples on a flat bed router and machine them like that.

What do you think?

Mark

7/27/20       #4: Machining small parts ...
Tom Gardiner

I have used wedges to hold multiple pieces into fixtures on a flat bed router (1 1/2" x 7/8" x 96"). I wasn't concerned about keeping the pieces absolutely flat on the table though. You could use a thin sheet of hardboard to accurately place the parts but you will have to devise a method to hold them flat to the table. Vacuum alone will not be reliable for so small a surface area and thinness. It could be a series of spring loaded aluminum dogs that can turn 90° to release the work or Destaco clamps as long as you can assure yourself that you won't run the router through them.

7/28/20       #5: Machining small parts ...
BH Davis  Member

Website: http://www.bhdavis.net

Mark,

I think you mean you could cut out spaces for the strips to sit in the sheet of 1/8" hard board.....correct? I think that's a good idea with the caveat of how you're going to hold them down. Just sitting in openings I think is going to let the parts move as soon as the bit hits them. Plus the parts would have to be dead flat. Even so I doubt a spoil board vacuum is going to hold them down. Easy enough to try though.

A modified plan along those lines might be to cut part shaped recesses into the surface of a 3/4" sheet of PVC. Then cut a 3/16" channel all the way around the part near the perimeter of the recess for a 1/4" round gasket to press into. One end of the part recess would be near the end of the sheet of PVC so that you could drill an access hole into the recess from the edge. Then you could run tubing from the edge holes to a rotary vane vacuum pump and pull say 18" to 26" of vacuum on all the recesses. The combination of the recess and the full vacuum suction should hold the strips.

Your 1/8" hard board idea gives good perimeter support but poor suction while the PVC method would give the same perimeter support while adding a sealed vacuum suction to the bottom of the part.

BH Davis

7/28/20       #6: Machining small parts ...
Mark

BH,

Thanks for your suggestion. I'm going to run a test. I can build the fixture and try it on my rail and pod machine.

Without having any experience with a flat table router, I don't/didn't know if the vacuum pumps could hold those parts while being machined.

Mark

7/28/20       #7: Machining small parts ...
BH Davis  Member

Website: http://www.bhdavis.net

Mark,

Right......I forgot you said you had a pod and rail machine. So you already have a true vacuum source through the pods. That makes it a lot easier as you can just through bore from the center of each PVC part recess down into the center of a pod location. Makes for a very easy setup.

Thinking about it a 24" x 96" piece of 3/4" PVC would give you easy access from one side to all the parts and simplify height uniformity issues that might arise with a 4x8 sheet.

BH Davis

7/28/20       #8: Machining small parts ...
Mark Member

BH and Tom,

Thanks for both of your your responses. I was wondering if there was enough vacuum that could be pulled through a spoil board to hold those thin parts down while being machined. And it sounds like that won't work, so I'll quit barking up that tree.

BH, I'll start tracking down some 3/4" PVC and and give that a test. This job could be large enough to merit a second, maybe used, rail and pod machine to keep up with it.

Mark

7/28/20       #9: Machining small parts ...
BH Davis  Member

Website: http://www.bhdavis.net

Mark,

If your regular panel provider doesn't have it you might find it at a lumber yard. We have one around me that carries it. Also Home Depot and Lowes might be a source.

The reason for the PVC is that it is a relatively inexpensive non-porous sheet good product. It can expand and contract but not significantly in relation to what you are doing. I actually used it to make the grid work hold down system on my retirement home shop 4x8 CNC. If you used MDF for this purpose you would have to seal all surfaces and edges after cutting in the recesses.

BH Davis

7/29/20       #10: Machining small parts ...
Scott

I used to work for a company years ago that did thousands of lineal ft of 6mm or 1/4 inch solid birch edging for birch cabinets for schools and institutions.
To make the 6mm we would run solid boards through the shaper with a multi cut or gang style blade set up, then we ran the strips through the widebelt sander to get the finished thickness. It was very fast.
I think once you had your blanks done you could set them in a hardboard jig like you mentioned and drill all the holes and some of the machining on a flat bed cnc. You could tape poly on the hard board and then all your vacuum would be at your pieces. I think you are going to have to do some handwork on every piece with the ends of the pieces though, use a laminate trimmer maybe?
1/4 inch thick is going to be delicate to work with.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!