Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Building plinths for load bearing wood columns

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Building plinths for load bearing wood columns

11/5/20       
Dan Member

Cheers All, I am replacing fake concrete plinths with wood. The challenge is the columns are grouped together in sets of 3, so they are appear too close for individual plinths.I have 2 ideas for a design:
Laminate 2x4’s on end to make a single plank or use 4x4’s and a half lap mitre.
Plinths need to be 31/2” tall 18” wide.
What’s the best method?
Pic files are too large?

11/5/20       #2: Building plinths for load bearing w ...
rich c

Will the plinth be sitting on concrete? Historically accurate design required? Exterior I presume?

11/7/20       #3: Building plinths for load bearing w ...
Dan Member

Yes It will be sitting on concrete with a sheet of epdm underneath.. I don’t think the half lap mitre is historical but I don’t know of a better 45 degree joint to use..

11/7/20       #4: Building plinths for load bearing w ...
rich c

So you suggesting pressure treated 2x4s and 4x4s? No way a miter stays together on that stuff. Tons of shrinkage and movement on PT 4x4s

11/9/20       #5: Building plinths for load bearing w ...
Dan Member

I agree... what would a better choice?
I can’t find 4x4 stock in exotic hardwood. What hardwood laminates well using west system epoxy?

11/9/20       #6: Building plinths for load bearing w ...
dan Member

here is what i am working with... about 3.5" tall and 18" wide..

11/9/20       #7: Building plinths for load bearing w ...
rich c

Some mahogany variation would be my choice.

11/10/20       #8: Building plinths for load bearing w ...
David R Sochar Member

I have made these replacements about 20 times in my career.....

Mahogany (sweitania macrophylla), epoxy.

How do you plan to vent the columns?

11/11/20       #9: Building plinths for load bearing w ...
Adam

We have always used SA mahogany for large paint grade plinths. It’s a good machining rot resistant wood.

What machine will you be running?

11/13/20       #11: Building plinths for load bearing w ...
Dan Member

I plan on using a table saw and some kind of jig to make half lap mitres...
Would using a biscuit and just plain mitres hold well enough?

11/13/20       #12: Building plinths for load bearing w ...
David R Sochar Member

When we build theses, the Square plinth is mitered, and then each miter is splined with cross grained mahogany. Spline cuts are usually 1/2" wide x 1-1/4" deep x as long as we can make it/close to the outer face of the plinth. You want to 'spline' about 1/3 of the miter's surface. 1/3 or more.

The round parts are hexagonal and with double splines, bandsawn and turned on a lathe or shaped on the big shaper.

Of course, the name of the game in that Plinth miter is surface area and glue. More surface area is better. It is worthwhile to do a few calculations to see just how much surface area /glue area different solutions might provide.

Biscuits are not waterproof and you will never get enough meat to hold the joint together.

Asking ".....hold well enough?" Well enough for what? To get paid? To get out the door? Your question implies doing as little as possible. The job requires a certain level of commitment and performance. If you are not willing or capable of exerting that level of work, then then please pass on the job and be honest with your customer. Respect the craft enough to know when to back away.

11/13/20       #13: Building plinths for load bearing w ...
Adam

We’ve done them brick laid and miter/spline. If the builder likes you they will allow you to place them before the columns are installed. Those can be brick laid.The vast majority we’ve done are replacements that are installed long after the columns were installed(100’s of years). So those were miter/splined.

My question was in regards to the profiling. We would make some custom cutters and run them on the shaper with a power feeder.

Are you routing and carving?

11/13/20       #14: Building plinths for load bearing w ...
Adam

We’ve done them brick laid and miter/spline. If the builder likes you they will allow you to place them before the columns are installed. Those can be brick laid.The vast majority we’ve done are replacements that are installed long after the columns were installed(100’s of years). So those were miter/splined.

My question was in regards to the profiling. We would make some custom cutters and run them on the shaper with a power feeder.

Are you routing and carving?

Biscuits are for alignment. Not very structural. Definitely use a high quality epoxy resin like West System or equivalent.

11/19/20       #15: Building plinths for load bearing w ...
Hastings Read Member

Hers how we tackled this recently. Octaganol sections finger jointed with epoxy. Four separate sections turned on a lathe and then joined with Dominoes and epoxy. Bottom section was Accoya, the others Red Grandis.


View higher quality, full size image (4032 X 3024)


View higher quality, full size image (756 X 1008)


View higher quality, full size image (4032 X 3024)

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!