Subject: Re: MC Changes & Wood Movement Due to High Humitity

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

MC Changes & Wood Movement Due to High Humitity

3/3/17       
Eric

Being in the custom moulding and trim milling biz, I'm always concerned about my wood and trim's MC content. Even though my shop does everything we can to keep things in line, the problem is after its delivered and before the warranty expires.

Last spring I milled and delivered a rather large trim order. We delivered and stacked it into the new construction house where the trim carpenters (not my guys) would do the install. Now I find out that because of lack of room, after delivery the trim is moved outside and covered loosely with a tarp where it stayed, loose packed for a month as they used it.

In the spring, in a high humitity enviroment, loose packed and barely covered, how much MC gain do you think unfinished poplar would gain in 30 days??

Well, now guess what????

3/3/17       #2: MC Changes & Wood Movement Due ...
Leo G

Looks like you need to add another line to your warranty. Must be stored in a conditioned area. Outbuildings and outside void the warranty.

If they admitted they stored it outside I'd just use that as the reason to void the warranty. Any carpenter worth his salt knows that you need the moldings to acclimate to the normal conditions in the house before you start the install. Flooring is the same way.

3/4/17       #3: MC Changes & Wood Movement Due ...
David R Sochar Member

I used to run into this all the time when the housing market was exploding, and registered idiots were building 2m McMansions. They would put the trim in the garage. The one with no door.

There were too many jobs to track, so I learned to read the miters after install and the real house HVAC was turned on. Open at the toe meant it was swelling, gaining MC. Open at the hell meant if had absorbed MC, but was now giving it back.

We merely added a doc to all estimates and ship tickets that explained proper molding storage. The lumber salesmen were then trained, so they could give warnings to the alleged builder.

3/4/17       #4: MC Changes & Wood Movement Due ...
rich c.

Do they store the hardwood flooring outside too? Tell them it needs the same treatment. Wood is wood. And because this was the way I first read the title, I'd like to petition for the title to be changed to; "due to high humility"!

3/5/17       #5: MC Changes & Wood Movement Due ...
Geoff

Sorry to hear about this issue you are dealing with. That's a bummer. Sometimes it's a fine line between keeping the customer happy, keeping your reputation and not having to accept responsibility/loss $.

I would caution that just saying,"material needs to stored indoors" is not enough.
I had some millwork ruined because it was put on heated slab floor with no protection. some door casing had a 2 1/2" edge bow in 8'. Basically the boards got baked on one side.

3/5/17       #6: MC Changes & Wood Movement Due ...
Eric

Thanks for the responses and info, but:

What do you think would be the MC gain in poplar trim sitting outside in a spring, humid southern state for a month????

I realize this would be a guess, but if I can come up with something close, I can then use the worksheet in Woodweb to determine the amount of swell/swrinkage

3/5/17       #7: MC Changes & Wood Movement Due ...
Leo G

What did it start out at? The drier it was, the more it will gain. Naturalization of wood outdoors would be in the area of 12-16%MC. Indoors it's suppose to be 6-8%.

IN a month I'd say you could gain 2-4% points.

3/5/17       #8: MC Changes & Wood Movement Due ...
rich c.

In some sections of the country, during the rainy season, I bet the outer boards will gain 10% or more. Some will likely have water sitting on them.

3/5/17       #9: MC Changes & Wood Movement Due ...
Eric

Thanks again for all the info and replies. Seams like everyone is on the same page.

Anyone have a good disclaimer they would share concerning this problem that they put at the bottom of their bill or invoice???

3/6/17       #10: MC Changes & Wood Movement Due ...
Geoff

My rule of thumb is most species of flat sawn wood will change 1% in width for every 4% change in moisture content (MC).

If you delivered the wood at 7-8% MC that means your shop was 40% relative humidity (RH) at 70F.

The big unknown is what were the conditions when the wood was stored outside. You can go online and look up charts on average temperature and RH in your area. But the conditions that month could be much different.

If the RH was 75% at 70F , when stored outside, the MC of the wood would increase to approximately 14%. That is a 7% change in MC. If wood moves 1% for every 4% in MC that is about a total of 2% change in width. Therefore a 12" board would move about 1/4" (12"x.02=.24").

I don't know if that helps, good luck.

3/6/17       #11: MC Changes & Wood Movement Due ...
Alan F.

Lots of issues
Really hard to quantify the damage caused or to determine the cause (legally)
Most contracts have a notification clause
Most have a "best practices" or grade rule clause.
Most contracts have indemnification and warranties (indemnification you pay to defend the GC).

See attached; they don't sign something similar we don't deliver.

If 30 houses fail and 30 home owners sue, cost to defend is huge, insurance may not defend,

IF the GC does an liability wrap that covers everything then the indemnification and insurance may not matter.


Click the link below to download the file included with this post.

Release_and_Waiver_of_Claims_Revised.pdf

3/6/17       #12: MC Changes & Wood Movement Due ...
Vic

I was thinking this:
"All trim must be stored inside, off the floor, kept dry, humidity controlled between 45 & 55% during storage, install and afterwards. Allow trim to acclimate for 5 to 7 days before install. Central Humidification Systems are highly recommended when extensive millwork is being installed."

3/6/17       #13: MC Changes & Wood Movement Due ...
rich c.

"Central Humidification Systems are highly recommended when extensive millwork is being installed."

You suggest adding humidity? My experience is the opposite. From plaster or drywall mud drying, curing basement concrete, gallons and gallons of latex paint, etc....Humidity around home construction is sky high!

3/6/17       #14: MC Changes & Wood Movement Due ...
Eric

Yes, sometimes I think the humidity needs raising. We know the humidity needs to be between 45 and 55%. I've seen some houses where the humidity was 30%, and this was in Arkansas.....

3/7/17       #15: MC Changes & Wood Movement Due ...
David R Sochar Member

I would visit all the jobs as trim was being delivered - within a day or two. I'd mention to the carpenters that they were "mitering at their own risk" since no matter who gets blamed, they would be doing the reworks and fighting to get paid. This was after the paper explanation of not putting finished wood products on site before the site had dried out sufficiently.

I would use a sling hygrometer and a moisture meter and record info as I walked around the job.

This would send the carpenters to the builder or project manager. They would mention the hardwood guys - checking subfloors for moisture contented waiting until the real HVAC is on and the place drops below 40% RH. They would mention me and my 'instruments' as one put it.

If the carpenters did not do my work for me or were somehow ignored, I would then send my temp and RH data to the builder, framed in a simple scientific format, and could easily show that they were inviting problems. This always did the trick. I did have angry builders make calls and get all upset because of this. I would point out this was not a subjective call on my part (made to cause him problems), but an objective call based upon fact.

I became 'the expert' on the topic and was asked about flooring, tile and other things I knew nothing about. I did keep on hand a couple of mitered joints that had each failed - one to shrinkage, one to expansion - as a pass around that easily explained what I had discovered. This was considered the final step - tell them what you are going to tell them, tell them, then tell them what you told them.

No one had ever had anyone pay this much attention to their projects, so they became loyal customers. And the miters were tight, so the carpenters and everyone was happy.

We have three masters to serve in this work: the Owner, the Builder, the Carpenter. Each has their own goals and demands. Pleasing all 3 makes for a very successful project.

2/19/22       #16: MC Changes & Wood Movement Due ...
Angelo Thompson Member

If they admitted they stored it outside I'd just use that as the reason to void the warranty. Any carpenter worth his salt knows that you need the moldings to acclimate to the normal conditions in the house before you start the install. Flooring is the same way.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!