Subject: Re: Curved benches

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Curved benches

2/16/21       
Michael Folan Member

Hi everybody
We landed this job of 100 linear meters of curved oak benches. It calls for 12 -15mm thick x 200mm wide pieces. Would you steam bend entirely or laminate and bend.
Thanks in advance
Mick


View higher quality, full size image (1080 X 2220)

2/16/21       #2: Curved benches ...
Adam

steaming bending an 1/2" x 8"(200mm) wide piece of oak in 3 bends as drawn would be a challenge with one piece. Impossible to replicate over 100m. Let alone 4 individual pieces.

This would definitely be a lamination job with a press. We would vac bag numerous ones side by side. It's a huge project . 500 pieces. whoa

2/16/21       #3: Curved benches ...
Michael Folan

Adam
Thanks a mill for swift reply. To compound matters theres a mixture of curved sections where each slat will need to be hand fitted after bending. In your experience will i need to source green lumber and how would i speed up the production with forms etc.
Mick


View higher quality, full size image (1080 X 2220)


View higher quality, full size image (1080 X 2220)


View higher quality, full size image (1080 X 2220)

2/16/21       #4: Curved benches ...
Bill

You didn't figure this out before you bid it?

Is it indoor our outdoor?

2/16/21       #5: Curved benches ...
Tom Gardiner

I would be searching for 2-3 mm veneers. Male and female forms in a big daylight press. I would imagine this would be ideally done with radio frequency curing but you will have to have a consult with an adhesives technical rep to ensure that the benches stay together
It would be worth the cost to buy a used press if you don't have one and probably the RF generator for the consistency and time savings.

2/16/21       #6: Curved benches ...
Michael Folan

Hi Bill
The benches are outdoor. We've been producing for years in european white oak with an oil finish. The vast majority are ex. 2" material. I figured in the price to include purchase of a RF generator as we have a heated daylight press. I also allowed in the costings to resaw 3mm veneers for bending. I'm meeting with a glue specialist and I'll mock up some samples and test before going into production. Thanks also Tom Gardiner for your input. I was thinking the same way.

2/16/21       #7: Curved benches ...
Bill

I believe an RF generator large enough to do that is in excess of $100K. I give you credit for taking that on.

2/16/21       #8: Curved benches ...
Mark B Member

Massive job but I dont see it as all that bad if you opt for even shop sawn veneer layup. Never solids. Looks like a fun one.

2/16/21       #9: Curved benches ...
Tom Gardiner

Can you produce shop sawn veneer at this price?

https://certainlywood.com/images-locator.php?item=1/10%20RF%20OAK%202011
4-6B

That's retail rift oak. I'm figuring you would see a substantial discount when ordering from a veneer mill the amount for this job. Core in seconds and faces AA matched. Or am I just lazy?
This will be a great challenge to work on. Good luck.

2/16/21       #10: Curved benches ...
David R Sochar Member

This path was first tread by Charles and Ray Eames about 90 years ago. Resorcinol glue, male and female forms and RF generators.

Wait, is that smoke I smell?

2/16/21       #11: Curved benches ...
Mark B Member

I was on the same trajectory as David without the RF but youd have to have the time to leave them in the forms. In todays world you could cut a set of forms to clamp those parts, perhaps double sided, (two clamped at once) and ditch the RF, ditch the bag, and go on.

2/16/21       #12: Curved benches ...
rich c

I'm with Bill. How did you land the job and not have a system ready to build it? Maybe that's why you got the job, you were the low bidder.

2/16/21       #13: Curved benches ...
BH Davis  Member

Website: http://www.bhdavis.net

To me this seems like a good opportunity to at least check into the use of compressed wood. Given the volume of work and equipment investment the compressed wood might be both a better cost and labor option.

Below is one source. Do a search for "compressed wood bending" for other options.

BH Davis

Compwood

2/16/21       #14: Curved benches ...
Adam

Michael,

We have done tons of similar work. Never in any quanity of that sort. Maybe 10-20 ft jobs a mix of regular chair types as drawn. As well as a couple of jobs like your tapered/scribed chairs that go in a curve.

Those parts are time consuming, with test pieces. Typically the first mold needs a fair amount of work and rework to get the exact finished product. Its more like building fiberglass boat molds than traditional woodworking.

Personally, I would have spent a day making one myself using the vac bag technique, just to see if its an acceptable product. If its good then figure out a mass production model using a press or a big vac bag form 20 at a time ( 25 layups). You would need a skilled crew dedicated to this process.

The metaphor would be somebody walking in asking me to build (500) basic curved door jambs which is the simplest version of your design. I have built probably built that many jambs in my entire 30 year career.

Quoting a project like that without doing some extensive testing and maybe not enough experience especially with the qty is not wise.

The financial risk vs reward of that project is scary simple because of the quantity. You guess 4hrs per part except it takes 5hrs. 1hr x 500 units = 500 hrs x $100 shop rate = $50000

That's if it goes reasonable with a big buffer. The whole project could go sideways and then the math is scary.

2/17/21       #15: Curved benches ...
Michael Folan

Thanks Adam
Because of the scale of the job both the corten steel and stainless framing will be manufactured simultaneously in separate shops and come together at the end. We will both use prepared .dxf files so as on previous jobs the fit will be perfect. The cnc time to produce forms wouldn't be a problem.
I think ill stay away from Compwood for now as I'm certain we can get over the line with more traditional ways. Thx BH Davis.
As for the financial side of things the story is we priced this a year ago at the start of Covid. Then things went quiet in Ireland but is now full steam ahead playing catch up. It was all or nothing at the time. The full contract also includes 350 meters of our usual straight work in a mixture of Oak and Cumaru so rather than let the handy one go I took the lot. No matter what I'm covered.
Thx
Mick

2/17/21       #16: Curved benches ...
Alan F.

Ideally you can flatten out the parts or Slice it in 3-5 axis software so you can CNC the shape of the "pie" slices that are bigger on one side than the other rather than all the hand fitting, you still may need to trim them in but if spring back and elongation are consistent you might be able to create the shape, we have done that with veneer, never with solid, then forms.

A-

2/18/21       #17: Curved benches ...
Adam

michael,

Please post how this job turns out for you. I'll be interested in your fabrication methods. Good luck and I hope it goes well. Cheers

2/18/21       #18: Curved benches ...
Michael Folan

Good call Alan F on flattening the parts leaving minimal shaping afterwards. Any help on reducing distortion greatly appreciated.
Thx Adam I'll update this thread with progress pics

2/20/21       #19: Curved benches ...
Dave Edgerton  Member

I agree with the posts. If it were me I would make up a hot press form and use plastic resin adhesive. I had at one time done 2 km of bent handrail and that's what we did. A bit of setup but a guy could weld up a frame for a press pretty quick and use a firehose for the pressing pressure. You would have to keep the metal plates hot perhaps even manually when the press is open but that would work. The problem with vac bag is the cycle time though that would be ideal way to go. Perhaps a big enough setup to do 10 at a time. Heat is critical to speed up cycle time. What a fantastic project!

2/20/21       #20: Curved benches ...
Bill

You can use IR heaters and fants to cool and get a 40 minute cycle time in a Vacc press.

2/21/21       #21: Curved benches ...
Michael Folan

Bill
IR heaters sound good too. Can you expand more on your idea? Any links to specific heaters?
Thx
Mick

2/21/21       #22: Curved benches ...
Tom Gardiner

Heated platens and IR heaters are okay for veneering onto a core but here you will need to heat through 15mm so the cycle times will be long with only the surfaces being heated. This is where RF gluing shines. Ex Factory sold the perfect daylight RF press recently for $26k. A bit bitch to ship to Ireland though.

2/24/21       #23: Curved benches ...
Keith Newton

If I were doing this, I would be using veneers wide enough to get multiples cut after the cure. The veneer stack after the thickened epoxy was applied would go into the bag which is laid over the form, (not in the bag). A stiff platen clamped down on the top before the front and back is eased on down and clamped under platens, then ready to pull the vacuum.
When the form is not inside the bag, the form can be cheap and easily banged together. It only has to be strong enough to not collapse under the force to bend the slippery stack of veneers.
A tarp with a few insulation sheets can quickly turn any available space into a hot room to speed the epoxy cure with a space heater blowing into it.

Finally a jig to cut the front to back taper is merely a box with a door opening the same size as the diagonal front to back dimension. Then using a circular jamb saw like the flooring guys use, can then saw up one side, around the curve, across the top, then on around and down, indexing off the flat side of the jig/ fixture.
After the first cut on the end, the second cut becomes the first cut of the next piece just by pivoting the jig back and forth.
If your shop already has a CNC that uses a big vacuum pump, all you need to do is tap into the plumbing with a manifold for however many hoses and fixtures you want to gear up for.

2/24/21       #24: Curved benches ...
Bill

We use IR to laminate through 9mm pretty easily. It might add some time to go deeper but it will still shorten the cure time.

Industrial Heaters

2/27/21       #25: Curved benches ...
Jeff

Like others, I think these questions and ideas should have been hashed over before you ever bid the job.
Lots of amazing help and ideas from everyone, but not much of a game plan before the game quite often ends up being a bad game, or in simpler terms lots of lost $$$$.
All the best.

1/30/24       #26: Curved benches ...
Robert

Can anyone recommend a publication that would serve as an RF "bible" so to speak. Any recommendations/suggestions greatly appreciated.

1/31/24       #27: Curved benches ...
BH Davis  Member

Website: http://www.bhdavis.net
Fun to see this post come back to life. I'm sure everyone who participated in the discussion would like to hear how the project turned out.

I don't know of any RF drying guide but do a search for Workrite RF glue dryer and see what turns up. Also at IWF about 10 years ago someone was displaying a large RF dryer that could do something on the order of 4' diameter half round jambs.

The manuals for these machines would likely give useful information on techniques.
BH Davis

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!