Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Exterior Wood Cladding - "Panels"

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Exterior Wood Cladding - "Panels"

10/23/23       
Max

I am planning to use 3/4" solid western red cedar cladding on a new house project in a tropical environment (south FL).

However, rather than expressed wood boards with a 1/8" joint between each board, I would like to glue the T&G boards into hairline joints onto some sort of substrate, effectively creating a panel that could then be applied like other facade cladding panels in a rainscreen system (panel sizes would be approx. 4'x8'). The desire is for a panelized look closer to an interior wood veneer panel rather than individual expressed boards.

On another project, an architect used 3/4" T&G teak glued and fastened into a 2-1/2" solid mahogany core and then another 3/4" T&G teak on the back side to balance. This was for a unique entryway condition - so ideally for this application, there is some other substrate that we could adhere and fasten to on one side since this will be detailed like a rainscreen.

Note - money is not an issue. My question is does this seem crazy from a functional / weathering perspective?

10/23/23       #2: Exterior Wood Cladding - "Pane ...
RichC

It's not practical for the life of the cedar. Wood moves from side to side during different weather conditions. Plywood doesn't. Cedar shingles live because the installer gets air behind the shingles and they dry out quickly. Your suggestion ignores the practices of centuries of success.

10/23/23       #3: Exterior Wood Cladding - "Pane ...
Max

I think what I am describing is akin to a cross laminated panel that are becoming more common as structural systems. Why could I not make a custom cross laminated, glued up sandwich panel and use it as a rainscreen?Lamboo has a bamboo wood product for exteriors that does this in principle.

10/23/23       #4: Exterior Wood Cladding - "Pane ...
Chicago Millwork

CLT panels do not get used in exterior applications, yes they are used for structures but then they are clad with something. Like Rich said what you are proposing simply will not last especially in a tropical environment. If you want cedar cladding look into rainscreen profiles.Even then I'm not sure about South Florida and cedar siding but I'm not an expert on coatings. History is not on your side with this idea.

10/24/23       #5: Exterior Wood Cladding - "Pane ...
RichC

Bamboo is grass, Cedar is wood. The cellular characteristics are much different when it comes to expansion and contraction.

10/24/23       #6: Exterior Wood Cladding - "Pane ...
RichC

If you don't like my advice, go ahead and do it. If money is no object, just bill them for replacement every few years.

10/24/23       #7: Exterior Wood Cladding - "Pane ...
Max

Appreciate the advice - I am by no means a wood expert. Just asking the question!

There is an example I saw at a museum in south florida - attached image below. It is teak cladding. Although not entirely exposed, it is set back under a roof, it is exterior. It was built in 2013 and I was there recently and the wood is holding up quite well, although it needs to be refinished. I've linked to an image below.


View larger image

10/24/23       #8: Exterior Wood Cladding - "Pane ...
Chicago Millwork

The overhang in the photo is massive and far from "normal" at that point it's almost inside. I get what you want to do ut it's not going to work how you envision it.

10/31/23       #9: Exterior Wood Cladding - "Pane ...
David R Sochar  Member

Website: http://www.acornwoodworks. nzs5z967fd com

You can make a panel with the look of solid cedar but it must be balanced - the same both sides. As simple as a three ply -face, core ,face - to a seven ply or more assembly. The cedar you see may be thin, like 1/16th inch thick, two panels thick,with each panel at five ply or more, with a core not more than 3/4” or so. Talk to Brett at Indiana Architectural Supply. They know the parameters.
LumberCore, for those over 65. Fabulous product. Five ply, if I recall.

7/16/24       #10: Exterior Wood Cladding - "Pane ...
RDBL

Website: http://rdbl.net/

In case you want to raise the smooth and strong reduction of your property, don’t overlook outdoor wood coverings. those bendy panels additionally create layout possibilities at the same time as present robust protection from the factors. wood outdoor pavers are flat, thin forums designed to guard the outdoor cracks of your private home. they come in a selection of styles, from traditional shiplap to fashionable tongue and groove art. These woods may be made from unmarried woods, which include cedar, alright and pine, every supplying a unique aesthetic and purposeful characteristic


View higher quality, full size image (1011 X 756)

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!