Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Veneered exterior entry door

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Veneered exterior entry door

7/13/24       
Revel Woodard  Member

I am making a standard size slab style door from VG Douglas Fir. It will be hung in a trimless aluminum frame and will incorporate a rabbet detail on sides and top, final thickness will be 2". Located in San Fransisco, it faces north, and is recessed in an alcove.

Having read many of the door posts on this forum, I've settled on the following approach: Ladder frame with 5" stiles and 5 or so rails joined with stub tenons + xl dominoes (could do full M+T if need be. would rather not). Voids filled with rigid insulation, skinned with 1/8" marine ply. 1" rail applied on both long sides, lipping planed flush. 3/32" shop sawn veneer (or 1/16" from certainlywood) applied over that. Marine ply and veneer to be glued using west systems epoxy in a veneer press. Would rather not use resorcinol but could be swayed to a pre catalyzed urea resin glue or polyurethane glue.

Finish has not been decided, though I am leaning toward spraying something like GF Exterior 450.
As has been my experience in the past, client does not love the appearance of freshly milled fir, and is looking for a more amber tone. One thought I had was to leave unfinished door in the sun for an hour or two, another though was to let the sun do its work over time. I will also be supplying a small run of T&G siding to match door for the alcove, ideally sprayed with same finish.

Have made exterior doors, but never a veneered one. Have done plenty veneer work, but not exterior. Does this approach seem sound? If there are any other finishes you can recommend, or any other pointers or admonitions, much appreciated.

-Revel

7/23/24       #3: Veneered exterior entry door ...
joremiaszh Member

Your approach to building the slab-style door with VG Douglas Fir is solid: using a ladder frame with 5" stiles and rails joined with stub tenons or Dominoes, filling voids with rigid insulation, and skimming with 1/8" marine ply is a robust choice. Applying a 1" rail and lipping for a clean finish is smart, and using 3/32" or 1/16" veneer with West Systems epoxy will ensure durability. For an amber tone, exposing the unfinished door to sunlight can help, but a controlled stain might offer more consistent results. GF Exterior 450 is a good finish choice for durability, and spraying the matching T&G siding with the same finish will ensure uniformity. Test the finish on scrap wood first, and make sure all edges are sealed well to prevent moisture issues.

7/23/24       #4: Veneered exterior entry door ...
Revel Woodard  Member

thank you 'fir' your response, and the finishing advise is much appreciated.... only thing I'm worried about is the strength of those voids. once that foam is skinned (rigid pink XPS 1.5") it will effectively be a torsion box, but it would seem you could still kick / punch a hole through if so inclined. SO I'm wondering if a true torsion box would ameliorate this potential issue ala the way David Sochar and others have illustrated; egg crate construction with voids filled with foam. the marine ply is hydrotek, and closer to 3/16"... I would use a thicker skin, but was constrained by the foam thickness (either 1" or 1.5") and the overall door finish thickness (2"). Don't want to over think this door, but don't want to deliver a flimsy product. I suppose I could vac bag a prototype panel. Another little wrench in the gears is that now the client does not want a typical aka functional threshold, but rather wants no threshold. Told them how this was silly and we had a chat about water etc, and now we are looking into drop down door bottoms from pemko... but that won't solve the water shedding issue. Going to work on this a bit more

7/29/24       #5: Veneered exterior entry door ...
oliverosalie Member

Your approach to building a slab-style door from VG Douglas Fir sounds well-considered, especially with your detailed construction method. The use of marine ply and shop-sawn veneer with West Systems epoxy is solid. For a more amber tone, allowing the sun to naturally age the fir could work, but you might also consider using a UV-stabilized finish to maintain the desired hue over time. GF Exterior 450 is a good choice, but also consider spar urethane for added durability. Given your experience, your plan seems sound, but keep an eye on the moisture resistance of all materials and finishes used.

7/30/24       #6: Veneered exterior entry door ...
David R Sochar Member

Lastly, use winders to check your vacuum bag set up. It has to be flat, dead flat, or you will build a twist into the panel. Often, vacuum bags are temporary set-ups on horses or cobbled tables that may not be as flat as we need.


View higher quality, full size image (2592 X 1944)

7/30/24       #7: Veneered exterior entry door ...
David R Sochar Member

My apologies for trashing this post.
Management can delete it all, I’ll clean it up and repost.
The edit is a good feature, but I could not edit all of my post, only one paragraph.

7/30/24       #8: Veneered exterior entry door ...
Revel Woodard  Member

Thank you, David. I would be very curious to see the rest of your post. Our vac table is pretty dang flat, my colleague Tim just gave it some tlc. I was going to ask-would you ever consider using polyurethane glue for an exterior door? I think the answer is probably no, but just checking.

7/30/24       #9: Veneered exterior entry door ...
Revel Woodard  Member

Oliver- regarding a UV stabilized finish, do you have any recommendations. I have not had great experiences when trying to stain fir so I assume that is out. The client does not like that fresh milled fleshy fir color, and I imagine the inside surface of the door will retain that hue for some time. However, since I am matching this door to the surrounding siding (which I am also making) am inclined to not use any color as it will ease refinishing down the road

7/31/24       #10: Veneered exterior entry door ...
Revel Woodard  Member

Slab glue up went ok, door has a 1/16" bow (not sure why, I'll double check that table) but no wind. I'll orient the concave side toward the lock jamb. Now for the veneering- Its all cut and thicknessed with the helical planer, somehow it didn't chew any of it up. I don't think I need to scuff sand it, and we don't have a wide belt but I'd run it through a friends if need be. I'm wondering how to veneer both sides of this at once
(I understand that is best practice with epoxy, as it shrinks a bit when curing?). Bottom side is a no brainer, then I have to veneer the top... I'm leaning toward edge glueing it first all first as that will take some variables out of the bag process. Wondering if edge glueing with epoxy is necessary, or if I can take a break from the stuff and use titebond 3 before I epoxy the resulting sheet onto the door core. Any ideas appreciated

8/11/24       #11: Veneered exterior entry door ...
Dave Sochar

No TB3, less you risk a failure. Heat causes failures in TB3, and those edges will hold the door up. TB2 or epoxy. And edges first is the way to do it. Both faces at once, tho that is hard to do.
You are smart to work with the bow. “Crowning” the door will hang the door with the concave side hitting the stops top and bottom first, then a bit more, and the latch snaps in and holds the door tight to the stops, no rattles, secure. If you are using the gawdawful compressible foam, all bets are off., and crowning is useless. Time was, all doors were crowned…….
And that errant photo. What is wrong with the elevation of that house?
Weekend in Branson if you guess correctly.

8/11/24       #12: Veneered exterior entry door ...
Quicktrim

David- would a core of solid flake board be acceptable? Not perticleboard but basically a large sheet of LVL type material? The local molding and door shop that I cnc parts for uses this method for their interior and exterior doors that they send to the mountains ( Vail high end and harsh environment ) .

It seems a very quick and easy method for slab doors , however they are very heavy , but everything we have machines for them was very flat and true. I have a couple slab doors to make coming up and wondering about the viability of this methodology.

8/11/24       #13: Veneered exterior entry door ...
Hen Bob Member

Shutters are backwards?

8/15/24       #14: Veneered exterior entry door ...
Revel Woodard  Member

I opted to epoxy the veneer to the door without edgeglueing; I did both sides of the door at once, and it went very well. Though it adds a step, I would probably edge glue the veneer next time, and not with TB3 -very interesting btw, David, I had heard that before but now I think it's sunk in!

Re: LVL core doors, I looked in to that. I've surmised that if you are very vigilant about MC it can work and is certainly a labor saver albeit heavy as you mentioned. Whereas it will stay flat, LVL is still wood based and thus prone to some swelling / shrinking.

...Maybe those shutters are on some sort of horizontal sliding hardware haha &#129315;

8/20/24       #15: Veneered exterior entry door ...
Tom Norton

This post is in regards to TB3 and my experience.
I have done repairs on my cedar trim with west facing exposure. And after 10 years the glued joint still is fine. Another little project was making a laminated handle for a snow shovel. That was a a lot of time! Butthat was 15 years ago and when not out it is under the barn with a south exposure. Still holding.
So curious about these other failures.
Thanks

11/12/24       #16: Veneered exterior entry door ...
Revel Woodard  Member

Meant to post some photos months ago- the door came out great. Install has been delayed but looking forward to that. I’ve sourced, milled and fillished some matching siding to surround the door in an alcove. I even saved veneer offcuts for the transom area. A fully trimless install, here’s hoping those walls are framed true as there’s nowhere to hide anything.


View higher quality, full size image (5712 X 4284)


View higher quality, full size image (5712 X 4284)


View higher quality, full size image (5712 X 4284)

11/16/24       #17: Veneered exterior entry door ...
Dave Sochar Member

Tom-I think it wise to err on the very safest side one can find. I also have a few projects around the compound glued with TB3 that have lasted for years.
However, this is no proof that the glue will pass for our commercial customers. Any failure in one of our products can result in thousands of dollars in repairs as well as a damaged reputation in the marketplace. Owning a small business is a gamble of its own. I do not need to add yet another variable to the mix.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!