Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Exterior Wood Door Questions

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Exterior Wood Door Questions

7/23/17       
John G. Russell  Member

Website: http://www.johnrussell.com

Hi all, I've been asked to build 16 exterior wood doors. Reason is is that Simpson Door Co. said 12 weeks (they're all different sizes) and that was not going to work with schedule.
I know how to machine stave core and assembly etc. My questions are;
Best exterior wood glue to use?
I'm milling cope and stick with a 1/2" wide groove. What material could I use, similar to spacebars I use in cabinet doors to keep raised panels centered?
I need to install glass in some doors. What is best material to hold glass, Butyl? 16th 32nd?
Any advice and help would be dearly appreciated. I did try to do a search, but didn't get too much info.

http://www.russellwoodworks.com

7/23/17       #2: Exterior Wood Door Questions ...
John Member

I haven't built many exterior doors, but when I have I've used a different approach, a stub tenon on the stiles and a mating mortise in the end of the rails. The inner edges of the stiles also have a rabbet on both sides to produce a matching stub tenon as on the stiles. It looks like this - see photo. The frame can be glued up with any exterior rated glue. I use T-88 Epoxy, but a guy I know who has made 100's of doors for every one I have uses TB III. I use LVL stave cores for the doors with 3/16" thick veneer glued on with Weldwood Plastic Resin glue in a vacuum bag. There are many woods you could use for exterior doors, from Douglas Fir, to mahagony, to white oak, to the Sapele I used for this door. I use loose tenons to reinforce the stile/rail joint, but dowels are much faster and work just as well.

You capture the panel with moldings glued into those rabbets on both sides of the door. The panels are undersized just like you would for any frame and panel door. I use foam backer rod to hold the panels in the openings, just like space balls are used. This door has solid wood panels, back to back 3/4" panels, so the inside and outside panel can move independently, but you can install insulated glass panels the same way.

John


View higher quality, full size image (3648 X 2736)

7/24/17       #3: Exterior Wood Door Questions ...
David R Sochar Member

Glue? Do not use TBIII as it fails in temps as low as 170 F degrees. If the doors get a dark finish and direct sun, the skins will bubble, and even the stave joints can fail. I suggest Plastic Resin or epoxy.

Panels? If your panels are so loose they need spacers to locate them, then water will pass thru the panel/rail to the inside of the door, or just to the inside of the plow. Make the panels accurately and as a force fit into the stiles and rails, centered as you assemble. We like a very slight taper on our panel raising profiles to help get the panel in, then tighten as it goes into the groove. The length of the panels is just a few thousandths less that the vertical rail to help lock the panel in place. If there are no vertical rails, the rails above and below the panel are clamped up to tighten against the centered panel.

Glass? Talk to your IGU vendor.

I have taught about 12-15 people how to build doors over the last 45 years. It takes a good man 2 years just to learn the basics of all the custom variables. 5 years and they are capable to good. Beyond that they can be great.

Also, the method that John describes can be used on interior doors, but may not weather well on exterior doors. I have seen all those nice pieces 10 years down the road, after each has moved a bit, gotten wet, etc. Even the pins will rust, letting loose. Miters open, butt joints shift.

Think of that center 'stub tenon' as being integral and machines as part of the rail or stile. This will stop one part from moving, one major source of leaks.

It is always best to build doors with as few parts as possible - integral tenons, integral sticking, etc. This makes for fewer parts to fail, and everything will work to prevent water intrusion.

One never knows how exterior doors are to be used. Some are 15' under a porch roof and will never see rain or snow or sunlight. A door maker has more options open in that case than if the door is on the East side, no overhang, no shade, getting full sun and all weather. That door can hardly be warranted, and maintenance will be frequent.


View higher quality, full size image (1800 X 1477)


View higher quality, full size image (1800 X 1478)


View higher quality, full size image (1800 X 1478)

7/24/17       #4: Exterior Wood Door Questions ...
John Member

I hardly speak with the voice of vast experience, but the guy who taught me that method has built thousands of doors and claims to never have had a failure. I can't vouch for that, but he's sold and installed a lot of doors and he's given me no reason to doubt him.

Let me clarify a few things. I said TB III can be used to glue the door together because that's what he does. I use T-88 epoxy for assembly. The door skins are glued on to the LVL stave cores with plastic resin glue. Interestingly, he told me that a major door manufacturer uses nothing more than silicone caulking, which was shocking but, again, I have no reason to doubt him though I'd never consider doing it. The point is all the glue is doing is holding the parts together. The load is carried by the joinery, be it dowels, tenons, whatever. As such, there just isn't much load on those joints. You would never see 170°F on a door unless it was behind a storm door with direct sun exposure, in which case you are going to have all kinds of problems anyway.

The backer rod I use to hold the panels in place is used like space balls. The panels still fit snugly into the pocket created by the glued in moldings, no different then in a cope and stick door. It's just a different way of getting to the same end for a shop without a big shaper. All the backer rod does is keep the panel centered laterally in the door frame. I use solid spacers at the bottom to keep the panels at constant elevation.

Glued in moldings are no different than cope and stick if you believe glue is as strong as wood. I use T-88 epoxy to glue them in and clamp the moldings in place w/o pin nails, etc. It will last as long as any other construction.

The cheapest source of glass panels is to find one you like already used in a commercial door and order a replacement.

With no disrespect intended, building a durable door is no different than learning to build other wood structures. Learn from someone who's been there/done that, study current and historic practices to understand what works and what doesn't, use the best materials you can source and follow good workshop practices.

What I do works for me; larger shops couldn't afford the extra steps and time it takes for me to build doors. But the end product is just as durable, and likely better than some of the commercial doors I've studied and repaired. I offered the approach to the OP because he sounds like a smaller shop that doesn't build a lot of doors. He can take from it what he will.

John

7/25/17       #5: Exterior Wood Door Questions ...
David R Sochar Member

Fortunately, door building, like most of woodworking, has lots of options and paths to follow. With some awareness and diligence, many methods will work successfully. Materials, glues, methods, joinery are all variables that can intimidate even seasoned door makers.

We probably use about 6-8 different base construction types that we have developed over the years and know how to do, and can rely on some predictable outcomes. Only when we are done with a project, do we know 100% what we should have done - you know the story.

But we stick with the base methods because of their predictable results and known methods. Rail sizes, panel types, stub, offset, haunched or thru tenons, veneered faces, radius heads, all have known methods that make it easier than inventing new process all day, every day.

As a result, we have the confidence to offer a 5 year warranty. We have the confidence to jump in and cut up some expensive wood and come out with a good product at the other end. And some money in the pocket and the bank.

I don't know the OP, but he asks some good questions, and some that give me some concern. I don't think making exterior passage doors is like making cabinet doors. It is not a simple process, and should not be underestimated.


View higher quality, full size image (1350 X 1800)


View higher quality, full size image (1350 X 1800)

7/26/17       #6: Exterior Wood Door Questions ...
Jarin Smoker

David,

I love the picture of all the muntions, stiles and rails. That looks sweet. I am wondering if you would have a picture of the setup that you use for running those muntions? We are struggling to run those currently.

7/27/17       #7: Exterior Wood Door Questions ...
David R Sochar Member

Karin -

The muntins are the devil hisself. I have made changes over the years, and nearly everyone I have worked with has developed their preferred way. They all have their pros and cons. Safety and accuracy are the two paramount factors. Below is what we have evolved to.

Since they have to be cut to length and coped first, one often not only has narrow sticks, but short ones also.

We do not remove all the wood in one cut. While that can be done for massive stiles and rails, the muntins could explode or deflect or....whatever as 1/3 or more of their mass is removed in one cut. Scary stuff.

Our 9/16" Ovolo tooling (in the photos) is set up to remove 1/16" on a full thickness cut with top and bottom ovolos and a 1/2" wide x 9/16" deep (per one type of sticking) plow in one pass. The shaper fences are offset by 1/16" to support the cut. The cutters (brazed, by CG G Schmidt, designed by Acorn) are a set that can also do a glass rabbet or plows of different sizes. Confusing as a set of 7, but they make sense in that you have much more versatility than a single head. We have the complement in cope cutters, also. The photos show both set up and as parts. The color-codeded spacers and digital calipers are necessary.

For the muntins, we set up for a top ovolo, a 1/4" wide plow, then spacers to the bottom of the muntin and another 1/4" plow. The muntin is 1/8" wider than finish dimension going in, and coming out. If anything is less that 14" long or shorter, I like to run a 1/4" x 1/2" batten nailed to the fences that the uncut portion of the muntin can ride on. This prevents the dreaded overcut, or the little 4" ones from getting disappeared up the pipe. Even without the auxiliary fence, if a mutt creeps away from the fence, it can be run again. They can't be over cut, or undersized. Both sides get profiled. We use a power feeder for all that we can, and can make other holding apparatus as needed at the shaper.

Then the mutts are taken to the table saw and the waste is sawn out accurately. Side feather boards are used for the first cut, with the waste falling out left of the blade. The second cut is a bit tippy and hard to hold with feather boards, so we have a special fence we use to let the muntin ride on. The surface created in the first rip rides on the special fence - we call it a rabbet fence - to set the final thickness (critical) of the muntin blade. The sticking is just a hair above the rabbet fence, out of the way. We use good push sticks at every saw operation with muntins. And feather boards again. Be sure to save the cut-offs for spacing at assembly. If you don't now see the purpose of it, you will when you get to assembly.


View higher quality, full size image (1800 X 1350)


View higher quality, full size image (1800 X 1350)

7/28/17       #8: Exterior Wood Door Questions ...
Joe Calhoon

We do these a couple different ways.
Using the outboard fence we run one side taking the full cut and removing 1mm from the edge. Second cut we make 2 passes because the piece is getting thin. These are cut to length and tenoned or coped first. For short pieces we connect and make a train using slotted pieces between. If coped we dowel the joint and use dowels to connect.
I have seen shops run these on a moulder in lengths and tenon or cope after. It requires a good counter backup with clamp pressure against the workpiece.


View higher quality, full size image (1224 X 1632)


View higher quality, full size image (1632 X 1224)


View higher quality, full size image (1632 X 1224)

7/28/17       #9: Exterior Wood Door Questions ...
Joe Calhoon

Another method that works good on narrow mulls with 1/4" or less wide on the inside is to make it in 2 pieces. We cross lap the profile if square edge or cope and dowel if profiled. The flat piece is cross lap at the center joints and just butts to the stiles and rails. These can be tenoned if you want but I figure with the glass bead in and captured in the profile groove they are not going anywhere.


View higher quality, full size image (2016 X 1512)

7/28/17       #10: Exterior Wood Door Questions ...
John Member

I use the same two piece construction for divided light doors. This is an interior door, but it's the same process regardless. The rectangular frame is cross lapped, and the ends of the muntins have a tenon that fit into shallow mortises in the stiles/rails. The molded top pieces are full length in one direction, usually horizontally, and coped in the other. They are dado-ed on the bottom to fit over the lower frame, and are glued with no pins, dowels, etc.

This is all done on a router table as I have no shaper. The process works equally well on arched doors.

John


View higher quality, full size image (3648 X 2736)

7/28/17       #11: Exterior Wood Door Questions ...
Adam

As David mentioned there are many methods to making the skinny short muntins.

I did my first 3 years in a 6 man arch millwork shop. The boss was a very smart skilled old school guy. Doing custom highend doors was a big part of our work. We would do whole houses. 5000sq/ft plus int/ext doors & windows.

Back in the early 90's we had several big jobs doing divided light double insulated glass. I had 20 SA mahogany 15 lights a piece. That is a pile of muntins.

I started with wide short things that looked like rails. 10" wide 5" long roughly. Coped the ends on the sled. Ripped them 1/8" wider than finish width. Then I made two guides with followers. The first is 3" x 36" square edged. The 2nd is made by running a 3" x 36" that is coped on the edge not the end. You fasten a block on the end so nothing gets kicked out the back. Both pieces are fastened to a piece of ply. You now have two accurately made push block/sleds. You run the parts with one then the other. In both operations the part is fully trapped. It cannot move. The feeder thinks its running a stile.

My boss was very impressed. The jigs pumped out parts with a 99% success rate.
We used those for years.I'm not at the shop, so I've got no pics of those specific jigs.

7/28/17       #12: Exterior Wood Door Questions ...
John Member

I can't seem to post more than one picture. What's the secret double handshake?

John

7/31/17       #13: Exterior Wood Door Questions ...
David R Sochar Member

I like Joe's and John's two part muntin solution. A good example of problem solving.

I have thought of it a time or two, but opt for keeping things less complicated, fewer parts. If I can do it safely.

My mentor aways smiled and said "You want less parts, not more parts".

7/31/17       #14: Exterior Wood Door Questions ...
Adam

The advantage with our method is there are no changes to the head. The ability to hold onto the small part after the first profile cut is the key to the whole operation. The first time I pushed the part into the fully coped sled was a memorable moment. It holds the part so tightly that the cutter head never pulls it out.

We had tried to profile long sticks then cope them, but the reject rate was incredibly high. The guys had been using a small box with push sticks before I invented our profiling sled.

8/10/17       #15: Exterior Wood Door Questions ...
Joe Calhoon

This discussion inspired me to try something I have been thinking about for a while. Now that we have a feeder that quickly changes to feeding against the fence I think it is workable and only requires 2 passes with no jigs. Stegherr uses a similar setup on their shaper attachment for running TDL and SDL. Its sort of the reverse of Adam's method.

The add on zero fence removes 1mm from the edge. Made by running through the planer and droping the bed halfway through. I added a block the same depth as the rebate. 15mm in this case. It worked well.
The true test will be running short butted pieces and 2 1/4" thick material with the tall center of T.
First pass as always is no problem. Second pass I found worked better with 3 wheels feeding and going slower. I put the Aigner rollers on for more support but don't think they are needed. No snipe or tearout at the end. The only change in setup is moving the feed in closer for second passage.


View higher quality, full size image (2016 X 1512)


View higher quality, full size image (2016 X 1512)


View higher quality, full size image (2016 X 1512)

8/10/17       #16: Exterior Wood Door Questions ...
Joe Calhoon

More pictures


View higher quality, full size image (2016 X 1512)


View higher quality, full size image (1512 X 2016)


View higher quality, full size image (1512 X 2016)

8/11/17       #17: Exterior Wood Door Questions ...
David R Sochar Member

Joe - That looks very good, with a nice set up of holddowns. I used to do 1-3/4" thick muntins that way, and it worked pretty well. The short parts were the ones that always gave us trouble. We just made about 50% extra.

But the 2-1/4" muntins were just too much. For me, if not the machine. That is a lot of wood being removed - 30% in our case. The shorter the worser. A larger machine, heavier fences, and a good feeder tipped over would work for us. We use a SCM T130 with a 4 wheel Maggi. It is hard to tip that thing on its side.

8/15/17       #18: Exterior Wood Door Questions ...
Joe Calhoon

Hi Dave,
I am excited to try this on a real job. I think keeping constant pressure and backup on all parts of the mullion is the key to this. I think Adam's method does the same.
We don't do a lot of small grills or TDL except for historic work and that is usually only a couple doors or a few windows. We did have one large historic job for a ranch on the Santa Fe Trail. We ended up using the outboard fence with a lot of additional hold downs and backing blocks to get through that. Doweling or slotting and tenoning the small parts together we get almost no rejects.

I think a lot of small time door makers are faced with this and cannot justify owning the Stegherr type equipment to make the job easy. The biggest problem we had on the New Mexico job was IG. Whe had to send back over half the units because of sloppy edges. Wish I had known about Green Mountain Glass at the time.


View higher quality, full size image (1536 X 2048)

8/16/17       #19: Exterior Wood Door Questions ...
Adam

I think this thread should be added to the knowledge base.

Joe, those Aigner rollers are a nice piece of kit.

We like most shops rarely do the true divided light doors & windows. Its mostly restoration work or one entrance door. The accuracy is by the 1/64" when doing a 15 lite door. It adds up really quickly. Definitely caliper work. Multiply that by 20 doors and you are talking big dollars if it goes sideways. Especially in sa mahogany like we used in the 1990's.

Next time you are making a door without the little mullions/mutins try coping a dummy 2' stile. Then pattern a normal stile. They stick together like the big time. No glue required. This is how my sled works for the little guys.

8/16/17       #20: Exterior Wood Door Questions ...
Joe Calhoon

Adam,
I don't quite grasp your method with the 3" thick material and plywood, but thinking it might be similar to the picture below with a stop block added at the tail to keep the workpiece from kicking out.
We use this method for narrow pre squared window parts on the angle machine to keep from tipping.


View higher quality, full size image (2183 X 2913)

8/17/17       #21: Exterior Wood Door Questions ...
Kevin Member

Don't mean to hijack, but on those narrow mullions and muntins, how would you use IGUs without seeing the black sealant around the perimeter? I ask because I currently have three doors like this in the shop, mullions are 1" wide. I typically prefer to have 1/2" or so flat for the window to set in, but these I only have 5/16".

8/18/17       #22: Exterior Wood Door Questions ...
Adam

Joe,

Yes its essentially the same thing you've got in the pic.

I didn't describe the jig dimensions properly.

1 3/4 door. You take a 1 3/4" x 3" x 24" fake stile. Instead of patterning it. You cope the long edge. You then screw the thing to a piece of 3/4" ply. Screw a block on the end to keep it from throwing the parts. The feeder thinks this jig is a regular stile so its runs well. The part sits on the sled and is completely jambed into a coped edge. It cannot move.

9/7/17       #23: Exterior Wood Door Questions ...
Comfu Furniture Member

Website: https://www.comfu.furniture/

The method of focusing your search begins with the cabinet's door frame and the way the frame fits together, two ways to get involved in four pieces of the frame is called corn and stick and merging. To illustrate the difference, it is more informative to show pictures of these connecting methods. Here is a picture of a coop and stick frame before the assembly. We are also dealing in hotel furniture and hotel fit out.


View higher quality, full size image (640 X 480)

9/12/18       #25: Exterior Wood Door Questions ...
Paul

Website: http://www.prodoorbuilder.com

Nice finished product.

Paul
Www.prodoorbuilder.com

6/5/25       #26: Exterior Wood Door Questions ...
Monica Chou Member

Website: https://www.zonledoors.com/

1. About the selection of external woodworking glue
For outdoor wooden doors, the adhesive must have high waterproof performance and weather resistance. The following two types of glue are recommended:
Polyurethane glue (such as Gorilla Glue): It is highly waterproof, suitable for outdoor use, and can fill small gaps, but it has strong expansion and the amount of use needs to be controlled.
Structural epoxy glue (such as West System Epoxy): It has extremely high strength and good weather resistance, and is suitable for long-term outdoor exposure and structural connection.
At the same time, it is necessary to ensure that the bonding surface is clean and flat, fits tightly, and cures in a suitable temperature and humidity environment.

2. Recommended materials for raised panel spacing
You mentioned the "space bar" (i.e. panel support or positioning gasket) used in cabinet doors to keep the raised panel centered. It can also be used in outdoor doors, but you need to choose a material that does not absorb water and can move flexibly. The following are recommended materials:
Silicone/rubber gasket: It can absorb the stress caused by the thermal expansion and contraction of the panel.
Butyl rubber strip: It can not only space the panels, but also waterproof to a certain extent.
Teflon/PTFE gasket: Highly weather-resistant, suitable for removable panels.
Try to avoid using ordinary MDF or wood chips as spacers, which are not suitable for outdoor use.

3. About the selection of glass installation and fixing materials
When installing glass, the material needs to ensure sealing, waterproof and allow the glass to expand and contract slightly. The following are feasible solutions:
Butyl rubber tape or strip: This is a very commonly used sealing material, soft and durable, very suitable for wooden door glass installation.
Silicone sealant (Exterior Grade Silicone Sealant): Used to seal the edges to prevent water vapor from penetrating.
Thickness of the sealant: The question of choosing 16 inches or 32 inches may be a misunderstanding. If you mean the glass size support, the thickness of the glass and the sealant strips needs to be customized according to the size of the door opening. The commonly used butyl tape thickness is about 1/8" (about 3.2mm). Reserve a 2-3mm expansion joint around the glass, and then add sealing materials.
The recommended structure is: inner frame &#8594; butyl rubber strip &#8594; glass &#8594; another circle of strips &#8594; nailing &#8594; external glue sealing.

4, other suggestions:
All wood should be treated with anti-corrosion. It is recommended to use weather-resistant wood species such as red cedar, mahogany or teak.
When installing panels or glass, be sure to leave enough gaps for thermal expansion and contraction.
All glues and sealing materials should be clearly marked as Exterior Grade.
I hope these suggestions will help you with your door-making project.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!