Ritter Adjustments/Repairs

10/30/15       
Mitch Suber  Member

Website: subercustomshutters.com

I have a 13 spindle borer, which is a Ritter R-19F. We had it made so the spindles are on 2" centers, not the usual 32mm, for drilling wood shutter stiles. Lately it has not been dropping the head and bits to complete the drilling of all holes, to their desired depth. The drop speed is correct, and it will quickly drill the 1/4" holes down the first 3/8" of an inch, but then it just seems to hang there, and takes forever to finish the last 3/8" of the hole depth. It is a pneumatic machine, with a foot pedal, however pushing down on the head will help some. We have adequate air pressure, in volume to the machine, brand new bits with the proper rotation on all spindles. The adjustments allow for the proper drop down rate, and the correct return rate. When no material is being drilled, it cycles correctly, every time. All slides and glides are clean and well lubricated. It has the same problem with most species of wood, but is some better on softer woods. The only other thing is that sometimes after finally drilling the wood, the head hangs in the down position and will not return to the up position. Shutting off the air to the machine, and back on, causes it to return back up.

10/30/15       #2: Ritter Adjustments/Repairs ...
Bruce H

I'd clean the air valves. Most likely will have to take it apart. I am guessing one or more of them has gunk in it and won't let the air pass as it should.

10/30/15       #3: Ritter Adjustments/Repairs ...
Mitch Suber  Member

Website: subercustomshutters.com

Bruce, I considered that once when this happened one time before. I disconnected the air lines, but really did not know how to take them apart. I blew them out, oiled them well, but that was about it. It didn't change anything, so they may still be full of gunk. After 25 years, I imagine they are. I found where I can buy them, not too expensive, so I will go that route. I was concerned about making the drill inoperable if I took them apart, at least right now we can still get our work done, even if it is slow. Have you taken them apart before?

10/30/15       #4: Ritter Adjustments/Repairs ...
Bruce H

I haven't taken the exact ones you have apart but have mine, whatever they are. Getting parts is tough, usually replacing the valves is necessary. I have found some of them on-line. Took my Ayen valves apart last week, cleaned and oiled them, they seem to be working. Whatever Ritter used shouldn't be all that hard to find. I am guessing your machine can be made to go another twenty five years.

11/3/15       #5: Ritter Adjustments/Repairs ...
Mark B Member

May also try disconnecting the line to one side of the cylinder and seeing if you can hear air bypassing the internal seal on the piston. Or doing a bit of a pressure test. If the cylinder builds, and holds, pressure then Id agree the valves are suspect.

Checking the cylinder would be a simple test to rule out you dont need a new set of seals in the drop cylinder.

11/28/16       #6: Ritter Adjustments/Repairs ...
Sam Nichols

Website: http://rittermachinerycompany.com

Just a heads up in case you guys are looking for more Ritter parts. We acquired Ritter's IP and we are now building machines and providing replacement parts out of our Holland, MI location. Hit me up if you need anything.

http://rittermachinerycompany.com


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory