Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Gluing solid wood to walls

6/2/17       
Dave Member

Hi. I am in the process of making some decorative hardwood tiles that are going to be adhered to a wall (gypsum/drywall). These tiles are going to be made from kiln dried (7-9%) solid wood (cherry, ash, maple, walnut)panels that have been ripped (2-3" max widths) and edge glued using the rip/flip process of alternating growth ring orientation. They are then going to be cnc milled with some patterns on them and then cut to final dimension of 6" (max) square. They will be finished with a water based laquer/urethane (Emtek or similar) The glue is going to be a urethane glue (no water content)3/16-1/4" v notch trowel. I am specifying a hairline gap (1/64") between all tiles but should I also: bevel the edges slightly (5-7 degree) to allow for more expansion allowanace and or relief cut the backs to reduce any potential cupping? These are interior only and specified for low moisture areas (not kitchen backsplash or bath room). Example tile image attached.
Thanks.


View higher quality, full size image (4168 X 3352)

6/2/17       #2: Gluing solid wood to walls ...
Bill

Would you consider that glue a flexible glue line? I would use something flexible so you won't have problems with splitting or adhesion as the wood expands and contracts.

6/2/17       #3: Gluing solid wood to walls ...
Dave Member

I would consider that glue line to be flexible. The urethane glues to the best of my knowledge are flexible and would allow for some movement of the wood.
Thanks

6/2/17       #4: Gluing solid wood to walls ...
Alan F.

I would glue or fasten the tiles to a piece of 1/4" PB or MDF and glue that to the wall w construction adhesive. Makes for a quicker and better install.
That's what we try and do with reclaimed wood. You can't tell when the install is done.


View higher quality, full size image (2385 X 3346)

6/2/17       #5: Gluing solid wood to walls ...
rich c.

You can specify any gap you want, but that won't guarantee the installer will do it. They when 12' of these expand an inch in a high humid section of the country, what happens when they pop off the wall? The owner will also be unhappy when they shrink enough that you could see white lines between them when they are installed around a fireplace. You'll have to apply the same thickness of finish on the back as the front for any kind of chance, but I see a fair number of problems for you.

6/3/17       #6: Gluing solid wood to walls ...
Blair

I would out a tongue on the north and west sides and a groove on the south and east side of each tile. That would ensure that you wouldn't ever see the substrate if the shrink and then you could spec a larger gap to make sure they never expand and come off the wall.

6/4/17       #7: Gluing solid wood to walls ...
B.H. Davis Member

At 6" square you are looking at 1/32" to 1/16" cross grain seasonal movement per tile. That means that a 1/64" gap spacing is not going to be large enough. Without climate control within the installation area I think you are going to have tiles popping regardless of the adhesive used.

BH Davis

6/4/17       #8: Gluing solid wood to walls ...
Adam

I would not rely on the waterborne finish to provide moisture stability. Nothing against WB. We primarily use it. I wouldn't trust any other finishes.

The only thing that truly prevents moisture from entering wood is epoxy resin. The West System boys have done all the testing. The epoxy does not need to be thinned with acetone or alcohol. The best moisture barrier is straight resin.

I would not use West System regular 205/206 hardeners. They cause blushing (contamination) and are very amber.

West System makes a hardener specifically for wood.

You can bond the epoxy/wood parts to the wall with any bonding agent.

West System 207 Special Clear Hardener

6/4/17       #9: Gluing solid wood to walls ...
Pat Gilbert

Alan

No seams, did the pieces overhang the substrate? Did you use panel clips?

I see this fraught with problems.

I like Blair's idea. I also like Alan's idea.

But still likely to be trouble.

6/5/17       #10: Gluing solid wood to walls ...
Dave Member

Thanks for all of your responses. Alan if I glue the tiles to a backing (PB or MDF) am I not inhibiting the seasonal movement and will make the tiles more prone to checking? I like the idea of the tongue/groove application that Blair has suggested. Would be relatively easy with CNC. Urethane adhesive is an elastomeric adhesive that allows for movement but has a strong bond. If I can acount for expansion/contraction I may do it. Otherwise may need to look at a panel clip system. Most of my information has come from the flooring industry so far and they use urethane glues to adhere wide plank flooring to subfloor. This is industry accepted practice. I have attached an application of a similar product where they are gluing (I presume a yellow glue) to a 1/2" baltic birch plywood backing plank. I have resisted the urge to do this because anything that restricts wood movement in my mind was bad. Am I wrong in thinking this? Appreciate immensely all of the feedback.


View higher quality, full size image (1276 X 783)

6/5/17       #11: Gluing solid wood to walls ...
Keith Newton

Dave, I think your plan is about right. I like your adhesive choice, but think gluing to drywall may lead to problems. the paper face will be pretty easy to tear away as it fails within. I'd use MDF, or industrial PB even over baltic, which leaves you trusting the glue of the face veneer.

Then, I think I would like to see about 1/10" gap, which could be caulked and fingered off forming a fine little cove that could handle and hide any movement, and better than looking into a gap.

6/5/17       #12: Gluing solid wood to walls ...
Alan F.

Dave,
The picture is T&G flooring, reclaimed wood, no real finish. There is room for movement. It is in a relatively stable environment with not a lot of change in humidity or temperature. We have been using that technique for reclaimed woods and flooring for awhile. We don't want an installer putting hundreds of pieces up in the field 1 at a time and we don't want to adhere right to the drywall. We use a mastic to adhere to the mdf /pb.

The panels are undersized so the boards lap when put together.

6/6/17       #13: Gluing solid wood to walls ...
kevin

Dave,

the tiles in the photo above are not real wood. thats why they are able to glue them to substrate without concern of movement.

you can tell they are fake by the repeat in the pattern. (look at the tile 2nd from the right on the top row. then count 8 tiles to left. its identical. look at any tile there that sticks out and count 8 tiles left or right)

6/6/17       #14: Gluing solid wood to walls ...
Dave Member

Kevin
I noticed that last night, but it is an actual product that is being produced and sold. That picture is rendered (quite well I might add) but they have actual installed photos on their website so I know it is getting installed. I know that climate control has been mentioned more than once on this thread. These tiles are only going to be specified for climate controlled areas so if someone wants to put them outside on a patio it would violate the warranty. I think I just need to plan on the movement of these tiles and use an adhesive with elastomeric properties and account for some gap with the tongue and groove method. I want to produce a quality product but if someone uses it improperly I don't feel that I can be faulted. That said I know that too much installation problems will fall back on me in terms of reputation. Anyways I am going to do some mock installs on a wall in my shop and see how it holds up. If anyone else has any more suggestions or knowledge they are willing to impart I do appreciate it.
Thanks.

6/6/17       #15: Gluing solid wood to walls ...
B.H. Davis Member

"Climate control" does not mean "indoors". It means controlled indoor temperature and humidity. Most homes don't have this nor I suspect do many commercial establishments.

My home has central heat and upstairs air conditioners.

In the winter the heat is on all the time but we don't pay much attention to maintaining a specific humidity level. Different types of heating systems create different moisture level condition in a home.

In the summer we will turn on the A/C on extreme temperature and/or high humidity days but again don't maintain a specific humidity level.

An indoor controlled climate will be maintaining a specific humidity level all the time.

BH Davis

6/6/17       #16: Gluing solid wood to walls ...
kevin

for what its worth... we did a bunch of huge entry portals and hallways in 3"x3" end grain mesquite squares. they were glued to mdf using Bruce all in one. then they were made into these large elaborate assemblies. I had the task of fiinishing these monsters. I used lots of epoxy thickened with fumed silica and colored with dye powder to match the wood. we spread this over the entire surface, filling the gaps and sealing the wood, then ran it thru our wide belt to get a smooth surface before topcoating it. ill try and find a few pics.


View larger image

6/6/17       #17: Gluing solid wood to walls ...
kevin

heres a pic i found.. we did ALOT of this stuff for this project.


View higher quality, full size image (791 X 636)

6/7/17       #18: Gluing solid wood to walls ...
rich c.

Mesquite is one of the most stable woods around. No surprise it works.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory