TimG

A contractor asked me how to do this mortice in a rafter might be made. The architect specified a 1/4'' x 2'' x 7'' deep mortice to hide a metal plate . Too deep for a router or chisel mortiser,or even by hand. I thought perhaps a chain mortiser but I have zero experience with those.

8/20/20       #2: How to do this ...
rich c.

Not too deep by hand. Extra long drill bits are easy to find, as well as extra long paring chisels. You'd spend big bucks for a chain mortiser for that job. But if there is 50 rafters, then not such a bad expense.

8/20/20       #3: How to do this ...
perley bowen

A timber framer might be able to help you.
Perley

8/20/20       #4: How to do this ...
Keith Newton

I started to suggest that maybe the material could be mortised in the shop on a chain-mortiser, but I just went out and checked my PM, and the bar isn't that long, and I'm not sure how much travel it has in the plunge depth.

I've got a carving bar for a small chainsaw around here somewhere. I would be thinking about pairing that up with some sort of slide.

8/20/20       #5: How to do this ...
TonyF

TimG:

Not sure of the size, quantity or material, but is there any chance that the mortise could be routed out as a recess on a portion of the rafter thickness, and then the rest of the rafter thickness laminated on to make it full thickness? Otherwise, what Rich said.

TonyF

8/20/20       #6: How to do this ...
PAT GILBERT

What is the purpose?

8/21/20       #7: How to do this ...
TimG

The purpose is I'm guessing structural. I have a pdf he sent but I don't know how to post just the section,and don't want to post the entire thing as the architect firm is on it.It's at the ridge miter,I assumed they didn't want the plate seen from the outside. The contractor is wanting to know what he's in for before he bids. So far I came up with a Makita chain mortiser that is good to 7 1/8'' x 1 15/16'' x 9/16'' with the narrowest chain. It would require the plate to be thicker than drawn, but the rafters are 4'' thick so I don't see why a bigger plate won't fly but who knows. I'm retired now so it won't be me doing the work, I'm just the consultant. I wish these architects would have someone on staff who could vent some of these things they come up with before they get to this point.

8/21/20       #8: How to do this ...
TimG

OK,I did a screenshot of the section.


View higher quality, full size image (1920 X 1506)

8/21/20       #9: How to do this ...
PAT GILBERT

This seems superfluous, why not just strap it across the top, if it is necessary at all?

8/21/20       #10: How to do this ...
Scott

I think like another poster mentioned, the best option would be a chain mortiser. All the timber framers use them , I would suggest something like the one made by Makita.


View higher quality, full size image (825 X 1074)

8/21/20       #11: How to do this ...
TimG

Yes Pat,I quite agree.Scott,that is the one I mentioned in my above post.

8/21/20       #12: How to do this ...
Keith Newton

Now that I can see what your needing, I’m with Pat , using a strap over the top .

Another suggestion would be to use a long drill through the ridge and out the top side of both rafters, with all-thread and nuts over large rafters, if this is in a hurricane permit zone.

What the architect may not Understand, is that Gravity keeps the rafters to ridge under compression. The bottom end detail shown in detail 10 where the rafter and chord intersect is under much more tension, and it seems to me that lag bolt isn’t sufficient since there isn’t any bird’s mouth cut or pegged M&T.

8/21/20       #13: How to do this ...
Alan F.

Are we talking about details 8, 11 and 13?
that looks like 1/4 x 2 x 5" deep to me (14" strap -4" beam /2).

Has a structural engineer seen this detail? I don't see what a single plate does structurally, there is no connection to the beam and the wood will shrink and move. Once you run fasteners through its visible.

You can blind fasten one side as well as connect through the crown of the rafter.

If its snow load that's one issue, if its uplift for wind that's another issue. I don't see this solving either issue well.
A-

8/21/20       #14: How to do this ...
Scott

I looked at the details and it looks pretty, but I would seek clarification on the purpose of those plates?

Hangers on the ridge board would be a better solution than those plates.

Gussets on the ridge board would be a better solution than the plate at the splice on the ridge board.

The only reason I can see using the plates and bolts has nothing to do with structural, it would strictly be for the aesthetics or a look.

8/22/20       #15: How to do this ...
PAT GILBERT

Show this to the architect

Show this to the architect

9/17/20       #16: How to do this ...
Bruce H

Have the architect figure out how to achieve what he/she has drawn. Just because it was drawn doesn't make it practicable.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!