I have a project coming up and we're installing white oak treads on a system that has steel skirt boards. Will there be issues with warping if these are scribed tight to the skirt? Would it be better to leave a small expansion gap. I've included the drawing detail. I would love to hear people's experience with this situation or something similar.

Click the link below to download the file included with this post.

Stair_detail1.pdf



Click the link below to download the file included with this post.

Stair_detail2.pdf

12/14/21       #2: Wooden stair treads tight against m ...
RichC

You can have both bowing and splitting if you fasten it hard to the steel frame. Spec rift or quatersawn and that chance is greatly reduced.

12/14/21       #3: Wooden stair treads tight against m ...
Tom Gardiner

I would worry about black staining of the oak from tannin reacting with the iron.

12/15/21       #4: Wooden stair treads tight against m ...
nicko

I cant see where there would be a problem. Wood expands on the width not the length. I would scribe them tight to the skirt and drill the holes in the steel, either drill your center hole for the diameter of the screw and slot the front and rear hole to allow for some expansion both ways. Or drill the rear hole and slot out the middle and front hole so that all of the expansion moves to the front of the tread. If you wanted to leave a 32nd on either side of the tread to be safe you could.

nicko

12/15/21       #5: Wooden stair treads tight against m ...
Tom Gardiner

To surround a piece of solid wood in a welded frame of steel angle invites problems. It's fundamental. Wood expands and contracts across the grain with moisture fluctuations. Make these treads with wood at 8% MC and have them dry to 5-6 % during the winter and you could have splits where the screws attempt to constrain the movement. Make the same treads in the winter with 6% MC wood only to have them swell in the humidity of the summer - you may have cupping or at least severe wood compression within the steel frame.
This design ignores basic wood construction practices. If your area experiences humidity swings seasonally I would recommend an alternative construction or risk call backs for noisy or broken treads.

12/15/21       #6: Wooden stair treads tight against m ...
nicko

If you look at the drawing you can see that the treads are not surrounded by steel but sit on top of the steel

12/15/21       #7: Wooden stair treads tight against m ...
Matt Calnen

I agree with Nicko on fastening. If your worried about tannin bleed into the wood, fit, then remove and finish all sides before a final installation.

12/15/21       #8: Wooden stair treads tight against m ...
David R Sochar Member

Website: http://www.acornwoodworks.com

It is OK to sit on a metal frame.
It is OK to scribe tight against the metal.
It is OK to accommodate the treads' slight movement across it's width.
It Is OK to not worry about iron staining black, as long as it all is kept dry.

The tread will only require slightly slotted screw holes in the metal frame. Look at the Shrinkulator to determine how much, and have the metal shop modify their work to include that slot.

This may be an open riser design, but if the tread is to be tight against a (wood) riser, you will find it wise to rabbet the riser over the tread. Adjust the slot sizes in metal accordingly - no slot, hole only back by the riser -and max slot length at the most forward - away from riser - part of the metal support frame.

12/15/21       #9: Wooden stair treads tight against m ...
Tom Gardiner

I looked at the drawings again and there is a 1 1/2" angle iron welded pan that the tread drops in. That ain't good. Or maybe it's my eyes ain't good.

12/15/21       #10: Wooden stair treads tight against m ...
Nicko

The second drawing shows a hidden line which represents the angle under the tread. The last drawing shows the step tread from the bottom.

Nicko

12/15/21       #11: Wooden stair treads tight against m ...
Matt Calnen

Upon further contemplation(and a glass of wine), the possibility of someone spilling a drink on the stairs would have me say you should absolutely seal the treads all around to prevent tanin stain. I’d like to imagine my stairway will never see excess moisture, until one of my kids overflows the upstairs bath tub!

12/16/21       #12: Wooden stair treads tight against m ...
RichC

I don't see anywhere if this is residential or commercial. If it's commercial, people coming in the building will have snow on their shoes and water will certainly be a concern.

12/17/21       #13: Wooden stair treads tight against m ...
Mark  Member

What I see is:
There is a 4 pc, 1-1/2" angle iron frame between the steel stringers to place the tread into
The drawings call for 6/4 (1-1/2") treads, negating scribing the treads to the stringers ("skirtboards"); rather, a good fit to the angle iron frame would be required. I'd leave an 1/8"-3/16" gap at the back of the tread to the frame, tight to the fron, snug for length.
The designer/architect is paying attention- chamfer the underside egges to fit into the inside of the angle iron; drill oversize holes and fasten with Truss head screws- this alows for some movement
Rift stock would be best, but flatsawn will work. I'd probably glue up flatsawn to 3 pcs per tread
Simple job

12/17/21       #14: Wooden stair treads tight against m ...
Mark  Member

After a second cup of coffee, I reaized that if the treads are 1-1/2", set inside 1-;1/2" angle, then the treads would stick above the angle the thickness of the angle- which I'd guess would be 1/4" + -
So, if you rabbet the treads all the way around, you'd cover the angle iron, and be able to scribe to the stringer. But that 1/4" over at the nosing is a bad idea as it will eventually crack and break off.
Best to clarify with the architect/client

12/17/21       #15: Wooden stair treads tight against m ...
Adam

I'm not the original Adam poster

I agree with David. As long as you make allowances for the wood movement in tread width there should be no issues.

The good thing about the steel is it will not move as opposed to regular 2x house framing that shrinks & settles for a the year following construction.

I'm impressed by the Architect/Designers drawings including elongated holes and biscuit/domino's.

The steel rusting and tannins damaging the wood should be completely avoid by painting the steel and the finish on the stair treads.

It all looks well thought out to me, except the micro bevel in the bottom of the treads. You'll have to keep the glue out of them or run the finished treads on the router table with a regular v-bit, which wouldn't be hard. I guess you will be micro beveling everything anyways with a laminate trimmer.

12/18/21       #16: Wooden stair treads tight against m ...
Adam

I'm not the original Adam poster

I agree with David. As long as you make allowances for the wood movement in tread width there should be no issues.

The good thing about the steel is it will not move as opposed to regular 2x house framing that shrinks & settles for a the year following construction.

I'm impressed by the Architect/Designers drawings including elongated holes and biscuit/domino's(not that you need either)

Painting the steel & finishing the treads should prevent any staining.

2/23/23       #17: Wooden stair treads tight against m ...
David John  Member

Website: https://www.tendersleep.co.uk/

Wooden stair treads installed tightly against a metal skirt board provide a clean and seamless look to the staircase. The metal skirt board acts as a decorative cover for the structural portion of the stairs, and by placing the treads tightly against it, it creates a visually appealing and polished finish.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!