Plastic laminate falling off millwork

5/1/23       
Dave Edgerton  Member

We did not do this work. However we have been asked to fix another company's work. The plastic laminate has fallen off every surface on the millwork in a reception area and office. It appears the glue did not adhere due to too much open time. The other milworker blamed low humidity in the office but i disagree personally with that. Could that be a factor? Millwork is only 4 years old.

5/1/23       #2: Plastic laminate falling off millwo ...
RichC

What is the substrate? Particle board and some MDF will move from season to season, but most office's maintain controlled temp and humidity.

5/1/23       #3: Plastic laminate falling off millwo ...
Dave Edgerton  Member

Rich, vertical is particle board the rest i will have to double check. The glue feels very thinly sprayed on. Even if these substrates move i dont recall seeing this much delamination in so many items.

5/2/23       #4: Plastic laminate falling off millwo ...
james e mcgrew  Member

Website: mcgrewwoodwork.com

Chances are Both surfaces were not sprayed, for a massive fail like this it would have to be a lack of adhesive, lack of adhesives on both surfaces, bad adhesive, wrong adhesive.
We have adhered hundreds of thousands of Plam to substrates without fail. Mdf and PCB are acceptable substrates if sealed correctly.
please bring pictures this is interesting to know.

5/2/23       #5: Plastic laminate falling off millwo ...
Tom Gardiner

I have witnessed two different mystery contact glue failures in 20 years. The first was my job where after about five years the laminate pretty well fell off. I am sure it was the glue. It was Dural and I only used it once.
The other was a job I was called in to look at. Good glue, the client had set up environmental monitors for temp and humidity. It turned out to be contamination of the p lam surface at the p lam facility. It took forever to find the cause with the adhesive chemists, p lam techs, cabinet shop and facility managers involved. This was about three or four years ago. I think the laminate was Arborite.

5/2/23       #6: Plastic laminate falling off millwo ...
Keith Newton

Were there any fire retardants used on this project?

5/2/23       #7: Plastic laminate falling off millwo ...
Dave Edgerton  Member

I will take pics and post. Its quite surprising actually how bad it is.

5/4/23       #8: Plastic laminate falling off millwo ...
Adam

When did it start failing in the last four years?

5/8/23       #10: Plastic laminate falling off millwo ...
adam

Sounds like 30 years ago when Wilson art came out with their blue water based glue, it stuck for about a year and then everything peeled off, would be nice to know what product was used so we will all stay away from it

5/8/23       #11: Plastic laminate falling off millwo ...
Ralph Kelley

Website: http://integralwindstormproducts.com

Re Adam: The first water based glue was terrible. it would fall off after a year. Many shops were using it since they did not have a spray booth with a fire hood. I worked for a company that had several kitchens that had to be removed, brought back to the shop, stripped and re-laminated with contact cement.
I agree and concur with your assessment and am now curious to see what the cause of this problem is.

5/11/23       #12: Plastic laminate falling off millwo ...
prunellaeelk Member

Err, Idk maybe you're right, but I have a different experience with the water-based glue used in kitchens. In my line of work, the glue adhered well and provided a durable bond over time. Ok, it's important to note that the success of any adhesive depends on various factors, and perhaps the problems you encountered were specific to certain circumstances or an issue with the specific brand or type of glue used...


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!