We need to have doors made to match existing vertical wood paneling, which is 5" wide tongue and groove rift oak. 8 feet tall, 30 inches wide, 1 3/4 thick.

The look is to have plank doors on both sides with perfectly aligned v-grooves - so six vertical planks, no edges, nothing. Similar to this.
https://www.trustile.com/sites/default/files/styles/content_slider/public/slider-v
g1000-01.jpg?itok=iChtl-Z0

But need to match existing paneling, so doors like pictured would not work.

I have read the Wood web database on plank doors, and saw suggestions on ladder style constructions. The problem is that the mill offers 5/8 inch thick planks and they can mill them square edge (with V added) or tongue and groove, but not willing to go to 1/2 inch thick. They are happier to offer 3/4 inch thick,

For 1 3/4 inch thick door even 5/8 thick panels on two sides leave only 1/2 inch for the center. These are all interior doors with humidity controlled space (well, there is a humidifier and dehumidifier).

For a ladder-style, would 1/2 thick really work?
Another suggestion was to glue to plywood but with 1/2 thick plywood even rift sawn oak seems iffy?

I am in a fairly remote area, so limited to what is locally available. What should I ask for? The wood people I talked to scratch their heads but are not experienced. But willing to try.

I would greatly appreciate your advice.

8/24/23       #2: Interior door construction question ...
RichC

Absolutely, never glue 1/2" solid wood to plywood.

8/24/23       #3: Interior door construction question ...
Nancy Member

The argument they make is that solid hardwood floor is routinely glued to plywood (but that is 3/4 inch thick hardwood) which on a face of it makes sense but still.

8/24/23       #4: Interior door construction question ...
RichC

I've never known anyone that glues solid hardwood floors down. Why do they insist on a gap around the room if the hardwood isn't going to expand. Gluing hardwood to plywood is never a good idea, no matter what the argument is. It contradicts the most basic law of woodworking.

8/25/23       #5: Interior door construction question ...
BH Davis  Member

Website: http://www.bhdavis.net

Can you cheat on the thickness and make these 2-1/4" thick? If so then you could make up the two sides independently by mounting the 5/8" thick boards to 1/2" plywood. No glue. Screws through the plywood into the backs of the boards.

Then you could vacuum or weight press the two plywood faces together and end up with a 2-1/4" thick door slab that should remain stable.

BH Davis

8/26/23       #6: Interior door construction question ...
Gary B

There are some door gurus on here that can give you a good answer. One even wrote the book on the subject. But I wonder, why not use a shop made veneer and vacuum bag this? If the v grooves need to be very deep, you could inlay a narrow solid wood strip before laminating. Just a thought.

8/27/23       #7: Interior door construction question ...
Matt Calnen

I made this door to do the same thing you need. 2 1/4” thick, 5/8” thick skins over a soft maple ladder frame. Groove to groove with a spline. I only glued half of the paneling width to the ladder frame so it could move a bit.


View higher quality, full size image (4032 X 3024)

8/27/23       #8: Interior door construction question ...
Pat Gilbert Member

Where is Dave?

8/27/23       #9: Interior door construction question ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com

I'd do a veneer thick enough to get my V into and plow those out on the cnc.

I'd also probably turn down that job as I've never been really happy with any pass doors I've made.

8/28/23       #10: Interior door construction question ...
tom gardiner

This was dicussed in a recent thread. Check out certainlywood.com for 1/16" rift oak veneer. If your v groove is large run dadoes in the substrate and glue in solid oak before pressing.
I would go with 1/2" particleboard skins and ladder the interior.

8/29/23       #11: Interior door construction question ...
Nancy Member

Matth, thank you for for the photo - that looks exactly like what we are looking for.
What did you use to fill the space in the ladder frame? We are trying to figure out if 2 1/4 doors would work, but that one looks the closest and simplest.

8/29/23       #12: Interior door construction question ...
Matt Calnen

Inside the ladder frame was hollow. I had planned to put 1” Ridgid foam in there(for sound dampening), but it got on the way of clamps. I did use stave cores for my ladder framing out of soft maple, and epoxy and domino’s for joinery. The “skins” are wire wheeled pine from the lumber yard, they were lightly sanded then painted for a textured look. Some integrated with existing wall paneling, some were Dutch doors and jambed and cased. These are in a wealthy persons party barn. A lot of open humid air in the summer, and heated dry air I. The winter. It’s been a year and a half since we built them and no call backs yet. I referenced Sochar’s book for construction ideas.

9/5/23       #13: Interior door construction question ...
Joe Calhoon Member

We make plank doors on a regular basis. Agree that if the 8’ tall door has to be 13/4” veneer with in set strips is the safe way. Ladder cores and 1/2” to 3/4” planking require thickness to be successful.
It’s OK to glue the planks to the ladder frame or ply core. Just don’t glue the planks together into one panel. Glued individually they can expand and shrink within their width. I leave 1/16” plus between the planks. Dry here and most everything shrinks. In a wet climate more gap would be required. Yours is interior so that makes things easier.

Just finished this hand planed distressed door for a hike in - skin in small cabin at timberline. 2 1/2” thick. 1” ladder frame with foam infill. Frame and planks are carefully faced material with grain alternating. The T&G is done at the shaper instead of the moulder to make alternating the grain easier to control I liked BH’s idea of screwing the planks on the exterior side in addition to glue. Don’t normally do this and never had problems with just glue but can’t hurt to add reinforcement to the exterior.
TB3 for everything.
The back door on my house is a 68mm thick plank Euro door with BB 1” fir plywood core made the same way with planks glued individually. All joints are still tight after 22 years. This door is to the weather and west facing. Needs refinish but everything still good.


View higher quality, full size image (960 X 1280)


View higher quality, full size image (960 X 1280)


View higher quality, full size image (960 X 1280)

9/16/23       #14: Interior door construction question ...
David R Sochar Member

Lots of good advice in the above responses.
A 1/2” ladder frame will work fine, and 5/8” faces will also be ok. If your wall paneling is 3/4, then the door faces need to be 3/4” to make the t&g look the same. Then your best bet is to build at 2-1/4”
You write as if you are trying to order things to certain sizes from a mill. I suggest you hire a professional woodworker and have him or her make the doors. This centers all the details in his/her shop, and the doors can be built properly.

9/21/23       #16: Interior door construction question ...
Nancy Member

We are ordering from the mill because we are also ordering paneling from them for the extension with matching T&G wall panels.

However some of the doors are sliding doors and 2 1/4 do not fit the openings (already framed), so I am back at needing 1 3/4 inch thick door.

If the ladder frame 1/2" and 5/8" faces work - that solves all the problems.
I do not have easy access to people who specialize in door construction, but they can build well if they know where they are heading (planning on getting a copy of Mr. Sochar's book for them).

To confirm - 1/2 inch with 5/8th face T&G quartered oak ladder frame would work for (1) sliding doors (both sides paneled T&G), (2) swing doors?

I also need one bifold door - again, with paneling on the side facing the room, but the "inward" can be anything. Can the ladder structure work for a bi-fold?
(And sorry - what does one use for the ladder frame - which wood? and what does one use to "fill in" - i see foamy thingies advised, but I dislike foam in all aspects. What can be used instead?)

Thank you.

9/22/23       #17: Interior door construction question ...
David R Sochar

The 1/2” thick ladder frame needs to have some nice long tenons, about .150” thick (1/3 the thickness of the frame) and 2” long, to hold it all square.

Plywood should be avoided. It does not have rigidity of hardwoods, and will show. Face the lumber to get it dead flat, then plane to 1/2”

The t&g that is go to 5/8” needs to be planed on the “back” only to preserve the t&g visual placement.

I think you feel you must build the doors as a carpenter would instead of using a competent, experienced door builder, all due to distance. A competent shop can make the doors and ship them to you complete. My shop shipped doors all over the US with no problems.

It is best to use the same species since it will show on the edges.

9/22/23       #18: Interior door construction question ...
Nancy Member

Thank you very much. I suppose I can bring the doors some distance. But how do you find non-local craftsmen?

My nearest metropolitan area is Detroit. How do I find a reputable door builders? I do need several doors.

9/22/23       #19: Interior door construction question ...
Matt Calnen

Where are you located? I’m in northern Michigan.

9/23/23       #20: Interior door construction question ...
David R Sochar

Acorn Woodworks is in suburban Indianapolis, and well qualified to do this kind of work.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!