Perry Member

In the process of making some 2" thick exterior doors and wondering if anyone can see a problem with this method. I don't have shaper tooling that will allow me to cope rails beyond the stub tenons. One of these doors will be south-facing with no overhang and so dowels are out. It needs all the strength it can get.

Obviously, loose tenons is a way to get around that, but this got me thinking.

What about running the loose tenons all the way through like after the fact stave core?
The process would be
Cut to length and cope rails on the shaper
Run a dado 2.5" deep where the panel slot will be. 1" on this door.
Glue in staves that extend to the desired tenon length.
Then run edge profile, fit tenons, and Bob's your uncle.

Can anyone see a problem with this method? Other than a decent waste factor from milling out a lot of solid stock.

3/23/25       #2: Entry door staves/ tenons method ...
FRED R FREHNER

Website: http://www.rivercity.ca

Hi Perry,

Don't know your geographical location but i think the south facing no overhang is you biggest problem.
For our exterior doors Sun and UV are hard on the finish worse if you got no overhang for shade. If you got a dark finish on them they basically heat up, the wood dries and checks. the finish cracks and glue joints will separate, panels will split.
this will happen regardless of your construction.
We had good results using Accoya on black south facing doors, but even they had a proper overhang.
No overhang we would not recommend wood.
We like to use Loctite PUR glue for anything exterior that gets heat.

3/25/25       #3: Entry door staves/ tenons method ...
Dave Sochar Member

I would avoid loose tenons at all costs.Right away, you double your joinery labor. And extra parts to make and fit. Tenons should be 3" long.
Do not use TB glue. 2 is not really waterproof, just water resistant. 3 will fail if the door gets warm, Looses more than half at 210 degrees.
Use epoxy for all your joints.

3/25/25       #4: Entry door staves/ tenons method ...
Perry Member

Yeah, it has all the "no no's". But it is a historic house, everything is period correct. The client is aware it will fail at some point. Couldn't talk them out of painting it black either.
But the real crime is how dark they want to stain this gorgeous 30 ring an inch heart pine that is the interior half.

Outside is all Sapele. Grandis stave core. All quartersawn.
Have been using epoxy for everything, and will peg the tenons as well.

Fred, on the panels- an idea I had this morning was to use PVC trim board to make the exterior floating panels since the outside is getting painted. I know it moves a lot more than wood, but I can account for that with panel slop.
The current door has failed primarily from the floating panels splitting. I figured using something that wouldn't split would give it a little longer lease on life.

So the panels would be heart pine on the interior side, 1/2" xps in the middle, and then PVC on the outside

Any reasons that would be a bad idea?

Thanks
PF

3/27/25       #5: Entry door staves/ tenons method ...
Dave Sochar Member

The panels should be a seven ply, all wood construction. Use 1/16" cross bands to stabilize the panel. Core of 1/2" man made wood stable - ply wood, MBO, etc. with solid wood, same thickness both sides, then crossbands, then faces.
Same species, balanced construction. Glued into the frame.

Exterior doors with one species on one side and a different species on the other will fail. Soon. They are done that way at the whim of a person that knows little about wood, and respects it even less. Usually a designer or similar. Your job as a professional is to speak responsibly about the respect for the craft, and that you don't wish to make work that will be unsightly and unusable. You are trading a small bit of your life for some money. Don't waste either.

3/28/25       #6: Entry door staves/ tenons method ...
Perry Member

Thanks for the input Dave,
I understand that the dual-species sandwich would fail. Especially in this application. Total exposure, south facing. And the outside must be painted black. In the south. This thing will get hot.

A spot all of us would professionally reccomend not putting a wood door. But the added constraints of the historic house and oddball size make it the logical solution.

But do you still see the different species interior and exterior as a problem with a stave core?
Again, the staves and veneers are all quarter sawn.

The current door is all heart pine and the exterior has been through many painter hack filler jobs since it first failed a number of years ago.

My respect for this 24 Karat heart pine that is the interior is why I am trying to figure out the best way to give it the longest lease on life.
While the interior must all be heart pine, I have the freedom to play around with the exterior and I'm always trying to make a new mouse trap. Hence the pvc idea for exterior raised panels since it machines well. It is a tall profile about 3/4, thicker than I would be comfortable veneering to something that won't move.

3/28/25       #7: Entry door staves/ tenons method ...
Fred Frehner

Website: http://www.rivercity.ca

Hi Perry,

We had used this product in the past and it worked out well. For paint grade profiled exterior Panels.

https://packardforestproducts.com/products/wood-composites/extira/

I
t is prone to chipping on sharp corners and edges but it does not look like it takes on water.

Due to our Climate and heating requirement's we prefer to have an interior and an exterior panel.

There is also Tricoya for a higher price. I have never used it and at times it is hard to get in our region.

4/7/25       #8: Entry door staves/ tenons method ...
Dave Sochar

Perry -What are you? Just a dumb carpenter or something? Do these people not recognise you as a real professional? Do you not recognise yourself as a true professional? Assert the best principles you know and leave it at that. I assume you can walk, but don’t recognise when that might be the thing to do. If there is a problem with doors you build using all wacky doodle stuff dreamed up by others, that failed previously, who do you think they will blame?
Respect yourself. Respect the craft. Respect a lifetime of experience. Respect over 500 years of frame and panel construction. Stand your ground. There is lots more work down the road.

4/11/25       #9: Entry door staves/ tenons method ...
Dave Sochar Member

And, as for terminology, "staves" are thr vertical members of a barrel. There are no staves in a door.
This is the tip that there is no professional architectural woodworker involved. Whomever is calling out the species and materials knows little to nothing about proper door construction. and you are in the same boat. Just because someone wants something does no mean you are obligated to build it.
May I suggest you buy two copies of the book "Small Shop Production of Custom Wood Doors" (Amazon or other online sources) - One to give the project manager so he can learn why you cannot do his project, and the second copy for yourself.

4/13/25       #10: Entry door staves/ tenons method ...
Joe Calhoon

Dave,
Perhaps you should Google stave core before going off on a rant.
Joe

4/14/25       #11: Entry door staves/ tenons method ...
Perry Member

Well, Dave, I am illiterate, so I guess that does make me a dumb carpenter. Thus, buying your book wouldn't be particularly helpful unless it has good pictures.
Fortunately, you don't have to read to be able to shave a perfect fitting tenon with a Stanley 78.
A great lesson passed on to me in grad school years ago was to never waste time arguing with someone who has a lower opportunity cost of time than you. So I won't touch the traditional vs engineered materials (which you also claim to use) debate. I have a shop to run.

4/19/25       #12: Entry door staves/ tenons method ...
Dave Sochar Member

Website: http://www.acornwoodworks.com

My apologies. I am retracting my rude and offensive comments regarding staves and the folks that use the term or build method. I was wrong, and wrong headed.

Often, in my efforts at improving the lot of my fellow woodworkers, I go overboard on real or imagined problems. I want to see us all moving up professionally instead of endlessly toiling in a cloud of dust, only to find we are going nowhere. It is that directive that can push me past the line of respect and openness that I normally function within. My work - the shop, the people, the life - has been a source of satisfaction and joy for over 50 years, and continues past retirement. I want others to experience a lifetime of joy and success through their work.

Thanks for the correction. I appreciate the fact that you all take the effort to straighten me out as needed. Feel free to kick me around if I get off track. Woodworkers are the finest people around.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!