Hi everyone, I installed some kitchen cabinets and missed a depth detail for an under counter washer and dryer. I am used to the Asco models which are 22” deep, but this job required Miele and although they are listed as undercounted models , they require 25.375” clearance behind doors that will conceal them and my cabinets are 24” deep,
This was only realized after the stone and cooktop was installed. It’s a 2500.00 Miele integrated cooktop that is flush with the countertop. I offered to pay to redo the 3/4” stone top and we will move the cabinets 2” off the wall and counter will be redone, when the countertop people tried to remove the cooktop, which was siliconed in place, they cracked it. The designer says I am responsible for the cost of the counter and the cooktop. I have a policy that covers this but it’s a 5k deductible, so I am stuck with the total amount. Should the cost of the cooktop be my issue and is it normal to silicone it into the recessed cutout as it is an exact fit on all four sides? Any advice will be helpful. Thx

11/5/21       #2: Insurance liability issue ...
james e mcgrew  Member

Website: mcgrewwoodwork.com

Might not be what you want to hear and it never was for me. sometimes lessons are expensive yet are worth 100s of times over as time goes on. I learned long ago to be extremly diligent in specs, even so far as to not build anything untill i had a signoff or the appliance in sight.

mistakes happen, comes down to basically who was removing it and what their actual role was. if you hired the appliance installers then they should have known. anyone else is a crapshoot..

11/5/21       #3: Insurance liability issue ...
harold morantz

Website: http://morantzcabinets.com

i am only the cabinetmaker hired by the design/builder. the cooktop was not installed by me but the appliance company. it is a flush mount glass top set into a lazer cut rabbet in the countertop to come flush with counter. turns out it was siliconed in place which is not recommended by Wolf. It could not be removed without damaging the glass when it would need servicing. if the granite people had taken the time to call the appliance installer, this would be the appliance installers problem, but they were in a rush and tries prying the glass top loose. at least if they would have tried to push the mewtal part of the cooktop box from inside the cabinet, it might have come loose.

11/5/21       #4: Insurance liability issue ...
Mark B

Water under the bridge at this point but Id guess if they'd have blocked up under the cooktop and applied some decent pressure with shims (lifting the cooktop) and left it over night the silicone would have broken free.

Im sure at this point its going to boil down to how good a customer is this and is it worth losing them over $5k? Sadly, they are pretty well justified to say the entire scenario would not have occurred had the cabinets been correct.

Its a sucky one for sure but it seems like your at the bottom of the hill in the poop flows downhill scenario.

11/5/21       #5: Insurance liability issue ...
james e mcgrew  Member

Website: mcgrewwoodwork.com

Harold I have admired your work a long time, I know you know your stuff this is a hard call as to responsibility, sometimes the pain is lessened far sooner with acceptance

11/5/21       #6: Insurance liability issue ...
harold morantz

Thanks James. Your right of course and i beleive everything is ordained from above.
turns out the client, who i have already done three very high end apartments for in the same ocean front property does not want me to be the fallguy here, ecxept for the quartz counter portion which i was expecting anyway. i always say that id rather money was spent on physical stuff and not for sickness, etc. after 40 years in business, its just stuff:)
just turned 71 and someone is looking to buy my company with me staying on for two more years to teach them the trade, and i have noticed that i"m not as sharp as i used to be and this is the first time i messed up on an appliance spec, so after 40 years of being in this business, thats not a bad record:)

11/5/21       #7: Insurance liability issue ...
james e mcgrew  Member

Website: mcgrewwoodwork.com

I turned 65 wednesday. joined Woodweb in 1996 or so. Be nice to sell the shop. looking at a rleative who married in to take an interest

We been doing this so friggin long !

11/6/21       #8: Insurance liability issue ...
Keelhauled

I love the honest responses lads. In Ireland you dare not claim on your insurance until you really need to, you may as well sort it out of your own pocket because they'll get it out of you in the coming years. I too am 40 yrs at the bench albeit I'm 54 y.o. None of my family are interested in taking over but I'd like to cash out eventually to get some compensation for the long hours building the business. Maybe a seperate thread needed to see other people's opinions???

11/6/21       #9: Insurance liability issue ...
Harold morantz

Website: http://morantz about nets.com

That’s a great idea. Why not continue this one? I am sure there are plenty of guys from the boomer generation that are in the same situation.
I sold my 4 man shop in Montreal 17 years ago to relocate in Fort Lauderdale.,the move was a needed one for my wife who has several autoimmunity issues and the -30 winters were really hard on her. Neither of us are US citizens and it took awhile to get an investment visa to get into the country. Used the cash from the sale of our home,,small country home and business to do it.,bought all new machinery, an apartment on the ocean and drive down in our new minivan and restarted our lives. Kids were both married and we already had several grandchildren.
The Canadian dollar was .63 so we had a serious hit financially, but we got settled and business is thriving.
Still love running the business and going in every day, and I am in good shape but losing some of my edge for details and have to double check specs and dimensions carefully to avoid errors. I always take one of my guts with me to measure sites so I don’t miss stupid stuff.
My guys also double check my optimization sheets for anything I might have missed. Have an offer now to sell to someone thst is ready to grow the company and keep me in at my present reinbusment for two years to teach the ropes. This will give me the extra funds I will need to retire in the level I’ve lived on.
Anyone else with an interesting story of the desire to retire or the success or problems you have encountered? Would love to hear about it. Harold

11/9/21       #10: Insurance liability issue ...
Quicktrim

Nice to see a constructive , polite, thread on here with meaningful prose and thoughtful replies.

I’ve been learning a lot from all of you over the years and now have just turned 45 and you guys make me feel young !

Thanks for that.

I think that the challenge is that in this business it takes so much to understand all the details that it’s quite hard for an outsider to come in and see the true value in what you have created. Mostly because what you have created has a lot to do with experience that can’t be sold or passed on. You can pass on the machines but how do you bundle your most valuable asset ,experience, and sell it to the new owner ?

That’s why a lot of shops end up on MachineryMax, several every week .

11/9/21       #11: Insurance liability issue ...
Harold morantz

Website: http://morantzcabinets.com

Quick trim, I think that to own and run any business requires attention to detail and a passion for what you want to accomplish.
In my case, it was the design and craft and the understanding of the processes that can create a product that satisfies that need and allows me to make a good living from it and excite others about my passions. It took me a long time to understand the financial aspects as I had no training in those areas.
When the frameless system of building cabinets first started to spread from Europe to America, Bob Buckley started the company True 32 to teach others about his passion for this new cabinet design and construction technique. He taught many of us and turned his cabinet shop into a learning experience for many and probably made a nice living doing so.
I sold my shop in Montreal of 4 workers and twenty four years of great clients with a steady clientele, to a young man who had just finished his rabbinic studies and wanted to buy an existing successful business. He spent a month shadowing my daily affairs with a deposit that was non refundable to see if he had the skills and desire to own a cabinet shop.
He did not know the difference between plywood and melamine , but the process intrigued him and he did buy my business, lock stock and barrel. That was 17 years ago and his trucks still carry my company name and I taught him how to successfully run a cabinet business.
With the funds, along with the sale of my home and country home, I was able to get a visa to move to Florida and haven’t looked back and had to learn new skills like marketing in a new and more diverse market.
I used the expertise of a great kitchen coach to help me adapt to this new market and the consults were worth every penny.
I hope to do the same thing in the next couple of years and pass this experience on. It can be learned but does require the initial investment of time and effort, taking over an established company thst had a good reputation and growing it bigger with more youth and determination can be very rewarding both emotionally and financially . As in the case of this error on my part of not checking the specs on an appliance , it’s all a matter of learning from errors and accepting the new challenges. Harold

11/10/21       #12: Insurance liability issue ...
Bruce H

I don't suppose you considered cutting a notch in the studs behind where the washer will go? Seems like recessing the washer a bit might have worked. Lots of my refrigerators are recessed into the wall cavity a couple of inches.

11/10/21       #13: Insurance liability issue ...
Harold morantz

Website: http://morantzcabinets.com

Concrete condo wall.

11/10/21       #14: Insurance liability issue ...
Bruce H

Well Harold, that makes it tough. I feel your pain though.

11/10/21       #15: Insurance liability issue ...
Harold morantz

Website: http://morantzcabinets.com

Thanks Bruce. Jobs done and chalked up to you experience. Won’t do that again😜
It’s been a dynamite year and in the end it’s better than having to spend it on doctors or the IRS😜

5/4/23       #16: Insurance liability issue ...
Johnny Woods Member

You didn't think to make a slot for the washer in the studs, did you? It seems like making the washer smaller could have helped. Many of my fridges are set back a few inches into the wall cavity.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • TradeJobPlacement.com
      Individualized Placement Services, Specializing in Millwork Design Engineers
    • OMEC/Macoser Inc
      Exclusive Importer of European Woodworking Machinery Since 1988
    • Fabrica CRM by Epure Millwork
      CRM for Custom Fabrication Shops
    • Impact Search and Placement
      Professional Employment Recruiting Specialists
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • ULTI-BOARD
      The Ultimate Spoilboard - ULTI-BOARD - Specifically Engineered and Formulated for the Ultimate in Spoilboard Performance - Not Your Ordinary Sheet of MDF.
    • TradeSoft
      Seamless Management Software to Improve Estimating, Job Costing, Scheduling, Purchasing, Shipping, and Shop Floor Data Collection
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • Parts Cutter CNC
      CNC Cabinetry and Closet Parts
    • WOODWEB, Inc.
      The Information Resource for the Woodworking Industries
    • WoodJobs.com Search Consultants
      Free Employment Service for Woodworking Related Job Seekers

    Become a Sponsor today!