Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: wide belt sander snipe

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

wide belt sander snipe

7/29/15       
door shop guy

Hi Guys

I have a Powermatic 25" single head wide belt sander and i am getting just a tad bit of snipe that is only visible after finish. I am talking maybe jut a few thousandths. If enough time is not spent with the Dynabrade then it is noticeable. I have never recieved a complaint and dont even think most people notice unless it is sitting on a flat bench under light. However i would like to adjust to correct the problem. I just dont want to start adjusting without knowing what i am doing. So i am asking what causes snipe on a widebelt and what parts do i adjust to eliminate it?

7/29/15       #2: wide belt sander snipe ...
B

We have a powermatic 25" dual drum sander, so the adjustments may be similar.

Typically, ours will start to snipe if one of two things occur:

1. The feed rollers are too loose. If the material isn't held tightly to the rubber conveyor, it will hit the sanding belt too high, resulting in snipe.

2. The table becomes unparallel with the drums.

Even when these two issues are adjusted, severely bowed wood can still end up with snipe as the bow will not sit flat on the table surface. This may be less noticeable with a single head wide belt and a platen.

7/29/15       #3: wide belt sander snipe ...
Larry

Assuming you have set the bed level with the head and the pinch rolls per factory manual and that you don't have any slack in the bed supports, try feeding the doors through at slight angle so the rails don't hit the contact drum all @ once.

7/29/15       #4: wide belt sander snipe ...
door shop guy

I have had this sander for over 5 years used almost everyday and it is rock solid. The bed is 100% parallel with the head.
Feed rolls are tight and there is zero slippage of stock ever. I have not tried running doors at an angle but i can definitely see what you are saying Larry. Thanks i will try that.

I wonder if the platen is too low? Or not low enough? I dont know.

My sander was made in 1997 and since i have had it i have had zero problems.

8/10/15       #5: wide belt sander snipe ...
Adam West  Member

Website: http://www.surfprepsanding.com

Leading or trailing edge? Are you using both the platen and drum or just the drum. The part with the snipe will tell you what caused it. Just align the mark with the sanding contact and the edge of the part will correspond to the offending party.

Just be aware that narrow warped parts will have issues in your machine no matter what. Once the warped part clears the hold down rollers it will push itself into the head more than when it's being controlled.

8/11/15       #6: wide belt sander snipe ...
door shop guy

Hi Adam

Thanks for the reply. I looked into it more today and it is the trailing edge of the doors that have the snipe. It is about 2.5"from the end of the doors. So does this mean the outfeed rollers are too high?
I am using the platen.At least i think i am. I have always been happy with the sanded surface so i have never adjusted anything.

On a diffirent note, i do want to buy a SurfPrep sander sometime.

8/11/15       #7: wide belt sander snipe ...
door shop guy

Oh and i forgot to add i do not run any warped parts at all. I pride myself on a flat door. I flatten all parts on the jointer.

8/18/15       #8: wide belt sander snipe ...
Adam West  Member

Website: http://www.surfprepsanding.com

You want about .060" of pressure on the hold down rollers at most. Often I used .040" to .050", but I can't see your machine and feel the strength of the roller springs.

If you use a block of wood and bring the table up until you have light pressure between the block and the sanding drum, then you can drop the conveyor .060". Then you look for how much pressure you have on the rollers. They should be just lightly touching the block.

Usually your situation is from too much pressure on the front rollers. You can see the correlation between the sanding drum and the hold down roller from the length of the mark on the part.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello