The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Fastening finished ends on frameless wall cabinets

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Fastening finished ends on frameless wall cabinets

10/17/16       
Gene Davis

Our 3/4" melamine carcases are CNC cut with blind dado joinery, fastened together with zip-r screws.

To do the occasional finished end (no applied panel) we cut the end from prefinished plywood, finished side in, and shop-paint the outside. We cannot screw these because the screws would be seen.

We've been using urethane adhesive in the dado and applied to the blind side of the tenon, and so far so good. This requires overnight clamping.

We are considering changing to butted joints for these sides, and a combination of glued-in dominos and pocket screws. We have not the means of doing RTA fasteners.

What do you do for this joinery situation?

10/17/16       #2: Fastening finished ends on frameles ...
Dan cook Member

What about pocket screws. You could do them from the bottom outside and top outside answers a butt joint.

10/17/16       #3: Fastening finished ends on frameles ...
Mark V.

Pocket screws or biscuits or a combination of both, depending upon the job. But, from what I see, the Lamello Clamex would the perfect solution, if I did a lot of this work.

Mark

10/17/16       #4: Fastening finished ends on frameles ...
Gene Davis

Thanks for the responses. Turns out Titan and maybe others makes a KD/RTA fastener that can be prepped in CNC and not require an edge bore.

So we'll use it. Shown attached is a wall-cab with a finished end and three such fasteners at each joint. Are two sufficient?


View higher quality, full size image (719 X 859)

10/17/16       #5: Fastening finished ends on frameles ...
Bill Member

Gene you mean Titus not Titan correct?

10/17/16       #7: Fastening finished ends on frameles ...
Gene Davis

Yes, Titus. Sorry for the mistype.

These.


View higher quality, full size image (831 X 363)


View higher quality, full size image (1433 X 361)

10/17/16       #8: Fastening finished ends on frameles ...
cabinetmaker

These will work also

https://www.google.com/webhp?sourceid=chrome-instant&ion=1&espv=2&
amp;ie=UTF-8#q=modeez

Link

10/17/16       #9: Fastening finished ends on frameles ...
Mark V.

Gene,

Those Titus fasteners are similar to Hefele's Rafix connectors. Expect your joints to shift 1.0-1.5mm when tightening them. If you use them on the outside of the top and bottom, the top will shift one direction and the bottom will shift in the other direction, making matters worse. Their good for closets, but for frameless cabinetry...I don't know.

If you end up using them, please let us know how they work.

Mark

10/18/16       #10: Fastening finished ends on frameles ...
Pat Gilbert

Is it really a big deal to your customer that there are a few cover caps on the inside of the cabinet?

10/18/16       #11: Fastening finished ends on frameles ...
Chris Hofmann

As Mark mentioned, Lamello P-system connectors are perfect for this application and are designed to accomplish secure fastening of end panels with an invisible joint. The machining man be done easily with the Zeta P2 hand tool or with CNC integration. There is no "walking" of the connectors when they are tightened. You have 2-3mm of lateral adjustment before they are tightened in case your hand-machining is slightly off - it's all very easy. Clamex connectors tighten with nearly 200 lbs of clamping force. I'm the Lamello product mgr. at Colonial Saw if you have any other questions: 781.585.4364 x.206

Lamello P Systems

10/18/16       #12: Fastening finished ends on frameles ...
cabinetmaker

Gene

Do you have an option for doweling ?

We are using dowels with face frame and frameless with great success. About 60 minutes before we hang doors and stress

Good luck

10/18/16       #13: Fastening finished ends on frameles ...
Gene Davis

No option for doweling, but we have two others: biscuits and Festool Dominos.

A line of 5mm x 30mm dominos would probably be a better solution than the exposed fasteners.

10/18/16       #14: Fastening finished ends on frameles ...
Cabinetmaker

Domino would be great leave about an 1/8 or so for drops of glue on either end of the domino

10/19/16       #15: Fastening finished ends on frameles ...
Phill Hunt

Website: http://www.dreamclosets.org

We have used the rafix and the Lamello. The Lamello works extremely well and is fast and easy. I would recommend looking into that connector.

10/19/16       #16: Fastening finished ends on frameles ...
JM

Maybe a stupid question, but can you not just glue the blind dado with titebond?

10/19/16       #17: Fastening finished ends on frameles ...
Mark V.

Gene,

Why would you use the dominos over biscuits? They both require glue and clamps and from what I have seen on youtube, the process to mill, glue and assemble a domino joint is much longer than the biscuits joints.

Mark

10/19/16       #18: Fastening finished ends on frameles ...
Mark V.

Phill,

Are you using the Clamex fasteners for your closet systems? And, if so, is one person easily able to install by themselves?

Mark

10/19/16       #19: Fastening finished ends on frameles ...
Phill Hunt

Website: http://www.dreamclosets.org

We use the Rafix from Hafele for our closet systems. We do a variety of frameless products for other companies so when the situation calls for an invisible conection such as Gene refers to, we use the Lamello. It is simple and one person can handle it.

10/19/16       #20: Fastening finished ends on frameles ...
Brad

Lots of videos at lamello for Zeta P2.

http://www.lamello.com/en/home/join-wood/p-system/clamex-p-medius-1410.html

10/19/16       #21: Fastening finished ends on frameles ...
Kerry Fullington

Gene,

Since you are using eCabinets Software for design, you could use the Lock Dado with Pocket Screw joinery and the machine will cut the screw pockets and peck the surface of the mating part.


View higher quality, full size image (1125 X 864)

10/19/16       #22: Fastening finished ends on frameles ...
Gene Davis

That's the best solution, Kerry, and thanks.

We can do just that, and it takes away the need for clamping if we went the biscuit or domino route.

10/19/16       #23: Fastening finished ends on frameles ...
Mark V.

Kerry,

Do you know anyone who is using this method? I remember when it came out, thinking that it was an awesome solution. But my tests proved otherwise, so now I am intrigued again.

Caveat, I don’t have a CNC, but I have a friend who has a Thermwood 43 and we were discussing the benefits of this system and I believe he told me that the pocket was similar to the one created with a Castle machine. I couldn’t leave it alone, so I took the pilot bit out of my Castle machine and made pockets in plywood and particle board. When I drove the screws, without a pilot/clearance hole, the core split apart. How is the CNC dealing with this? And, what is, “peck the surface of the mating part” doing if there is no way of judging where the screw will come through? Please help me understand this better. Also, do you have pictures of the parts off the CNC?

Mark

10/20/16       #24: Fastening finished ends on frameles ...
Kerry Fullington

Mark,

We have been using this joinery several years for the same purpose as Gene, to fasten finished ends of some Mella/Wood combination.
There is some swelling at the joint but auger point screws help. As usual a lot depends on the quality of the material core.
The pecking (which can be turned on or off) is mainly to remove the hard surface of the melamine where the screw is going to enter to expose the core.
The way Thermwood designed the pockets there is a tiny shelf in the center of the pocket to rest your screw point to get the angle correct since there is not pilot hole.

10/20/16       #25: Fastening finished ends on frameles ...
Gene Davis

The Thermwood router does not give one a through hole for the screw, the way a Kreg bit does.

I'm told by the shop that will cut this that when they do cab assembly of units with this detail, they predrill using an 1/8th-inch bit before driving the pocket screws. Not the part the screw will go into, but the part with the hole pocket.

So that's what we'll do, and we'll get some longer bits for the jobs.

10/20/16       #26: Fastening finished ends on frameles ...
Bill

We pocket screw on the cnc and pre drill as you describe. Works like a charm and saves lots of time.

10/20/16       #27: Fastening finished ends on frameles ...
Mark V.

Thanks guys!

Now the CNC pocket hole process is very clear.

Mark

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello