Subject: Re: Wide Belt Sander for Veneer particle core panels

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Wide Belt Sander for Veneer particle core panels

6/9/21       
Mike  Member

Is anyone using a wide belt sander for sanding 5/8-3/4" Veneer particle core panels?
We have used a stroke sander in the past but had too many issues with sanding lines not blending together.
Wondering if a wide-belt would work. Taking way too long with orbitals.
thanks

6/9/21       #2: Wide Belt Sander for Veneer particl ...
Bill

Yes, you need a segmented platen sander. Works like a charm and stains more uniformly. Depending on your volume well worth the investment.

I got a quote on a 2 head recently and it was 90K new. It was specific to my needs and your needs may be different. The benefit of a two head for veneer is that you run the heads counter rotating and it sands in one pass. The alternative is a single head and you want to sand in both directions.

Sounds like you don't have a wide belt at all so a more appropriate machine would be a two head. First head Drum, second head combination head with a segmented platen. With the second head you can sand, drum only, platen only or drum and platen. Very versatile machine. You can level doors and frame, sand hardwood, sand veneered panels.

PM me if you want details on the quote I got.

6/9/21       #3: Wide Belt Sander for Veneer particl ...
Scott

Mike,
I am not sure what your application is, or your volume, but any decent widebelt sander with a platen will work fine. I have a twin head SCM widebelt with a platen and I run veneer panels through it with no problems at all. I will stipulate that mine is 37 inches wide and the widest panel I normally use would be a fridge gable so about 26 inches wide.
I have done some 3 ft veneered doors, but I ran the blanks through first before I veneered them so they were fitted to my machine.
I would be nervous sending through 4 ft sheets straight from a wholesaler on a wider machine with out a segmented platen.

6/9/21       #4: Wide Belt Sander for Veneer particl ...
Mike D  Member

Thanks guys, very useful info. Looks like these suggestions will work for our situation.
We'd be running 1-2 kitchens through per day. So saving time and manual grunt work is the goal.
Now to convince the owner.

6/14/21       #5: Wide Belt Sander for Veneer particl ...
Pdub Member

Are you talking commodity veneer or custom laid up veneer? Commodity is so ridiculously thin now that you have to be super careful.
We just got a 2 head Viet with a standard air platen (not segmented) and send veneer through it. The machine just needs to be really dialed in, which isn't that tough to maintain.
Keep in mind that you will still be using the orbital to get rid of the scratch pattern from the widebelt.

6/14/21       #6: Wide Belt Sander for Veneer particl ...
Bill

With a segmented platen we can send commercial plywood through several times before it burns through. If you have a need to sand veneer I believe a segmented platen is worth it.

Why do you use an orbital after the wide belt? Have you done stain tests both ways?

6/14/21       #7: Wide Belt Sander for Veneer particl ...
Pdub Member

Because of the very linear scratch pattern a widebelt leaves on the surface?
If you do it right with your height setting at various grit belts, it's a very light pass with the orbital, but still necessary from my experience.

6/29/21       #8: Wide Belt Sander for Veneer particl ...
Adam West  Member

Website: http://www.surfprepsanding.com

Mike

If you look at basic machines like a drum/combi-head machine and want to sand veneer you want to be sure you buy a "dead shaft" machine with the ability to pop the drums out of the way without changing their settings. It is called air exclusion. Most Chinese and Taiwanese machines do not have this feature.

The platen MUST have the ability to pop down onto the part and up at the end. These types of plates will have either air or air bladders so they can float a bit. These can do a reasonable job.

Segmented platens are definitely the best but they cost big money.

I work with sanding machines for a living. Feel free to IM me if you need further assistance.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Lamello
    Today's Sponsors
    • MARTIN Woodworking Machines Corp.
      Quality Woodworking Machinery Engineered and Manufactured in Germany
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs
    • Impact Search and Placement
      Professional Employment Recruiting Specialists
    • The Millwork Studio
      Millwork Shop Drawings and Estimates
    • Unique Machine & Tool
      Industrial Machinery for Door and Drawer Production
    • ETK International
      New and Used Woodworking Machinery, Spare Parts and Superior Service
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Cabnetware Support
      Technical Support Forum for Cabnetware Users
    • OMEC/Macoser Inc
      Exclusive Importer of European Woodworking Machinery Since 1988
    • CabinetCRUNCHER
      3D Cabinet Design and Construction Software Powered by SketchUp and Excel, Precise Cut List Calculators with Highly Adjustable Construction Options for Cabinetmakers and Woodworkers of All Levels
    • J&P Machines
      Design and Production of Custom Equipment for the Manufacturing Industry
    • JKL Machinery
      US Exclusive Importer Casadei, Busellato, Vitap, Bonacin - Machinery Dealer representing New & Used Woodworking Machinery
    • WalzCraft
      Custom Doors and Wood Products

    Become a Sponsor today!