Safety Speed Cut Thermwood Corporation ECabinet Systems

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: 1.5" Birch Butcher Block counter Tops

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

1.5" Birch Butcher Block counter Tops

3/30/23       
Chris Member

Hey All,
Looking for some advice/help. I have 35 "L" shaped kitchens to build. I also have to cut and install the tops "on-site".
The Inside corner will be a 45+- miter cut. Does anyone have any experience using the Festool 75 plunge saw with track? Will it hold up running through 1.5" Birch about 70 times without burning up the saw or the wood, will it give me a nice plumb/straight cut?
If you-all have any better ideas, suggestions, anything at all... I appreciate any help!

Thank You,
Chris C.

3/30/23       #2: 1.5" Birch Butcher Block count ...
ScottO

Wow, that is a good question, I have never used a Festool T75, but I do own a T55, my feeling is it would cut that no problem, it will be easy to set up the saw and clamp the track so you get perfect cuts.
Use some sort of alignment fasteners like biscuits, dominoes or splines and some joint fasteners and you are done.
I did a bunch of those many years ago before they had the dedicated track saws, we cut all our mitered corners on a 10 ft sliding table saw. We used a fence and a router to make any small changes on site.
Have fun!&#128526;

3/30/23       #3: 1.5" Birch Butcher Block count ...
Dave Edgerton  Member

First iisue is you probably shold not do butcher block at 45 but that is none of my business. We have a makits setup like this and has worked great for years on butcherblock tops. Keepa very sharp handplane with you for touchups

3/31/23       #4: 1.5" Birch Butcher Block count ...
Tom Gardiner

I think you are in for a load of trouble with mitred corners on the counters. The joints will open up with seasonal movement of the wood. It is exaggerated with mitres. You would be way better off by butt joining with dominoes no glue in the front. Bonus is you will save 2' of material per kitchen.

3/31/23       #5: 1.5" Birch Butcher Block count ...
Joe W. Member

I have used both the T75 & T55 for years. I refer to the T75 as the beast. I use it for solid surface countertops and thick material such as the butcher block. Never had issues.

It was fine, but you need to have a good feel and understanding for the saw's abilities and make sure to use the proper blade, saw speed, and feed rate. All can cause problems if you don't.

I too don't recommend a 45 degree miter though.

Good Luck.

3/31/23       #6: 1.5" Birch Butcher Block count ...
Chris Member

Agree 100% on the mitered joint. Thank You for confirming my suspicion. I have a good feel for saw speed & feed don't think that will be a problem. Can you recommend a Blade for the Festool 75?
I would like to make this a one cut deal, I thought about trying to take two shallow cuts but I am pretty sure it will just increase the the chances of a torn-up kerf. I do have a sharp plane to clean any rough areas up.
More fun... No Backsplash other than a Stainless Steel sheet. So the butt Joint will make it a bit simpler to scribe backs to wall.
Thank You Guys, I really do appreciate your input and experience.
Chris

3/31/23       #7: 1.5" Birch Butcher Block count ...
Chris Member

Made the changes to the top, (Miter Vs. Butt), as stated above I have saved over 70' of butcher block therefore I can justify more tools! We are a cabinet shop so of course we have a biscuit joiner but not a Domino Joiner so I am looking at the Festool XL DF 700.
So what do you-all think, Can I use the big domino's without tie-bolt fasteners? I can use pipe clamps to pull the pieces up tight while sitting on the new cabinets and allow glue to set. Issue is getting under the counter to access the fasteners is going to be difficult at best.
Another issue... I have to finish the tops in-house. Contract does not allow on-site finishing so no sanding & matching of tops.

Again Many Thanks,
Chris C.

3/31/23       #8: 1.5" Birch Butcher Block count ...
Thomas Gardiner

Glue the dominoes into one side of the joint. Glue only the one closest to the wall on the other side of the joint. Over width slots for the other domino positions to allow movement. Hold pieces together with screws and washers through oversize pilot holes in the cabinets. Remember you are allowing for movement in the x and y planes of the joint.
Full waterproof finish on the joint faces before assembly

3/31/23       #9: 1.5" Birch Butcher Block count ...
Chris Member

Thank You all for your responses. I do feel more confident with all of your help.
Chris C.

3/31/23       #10: 1.5" Birch Butcher Block count ...
ScottO

No matter what kind of joint you make you are going to get seasonal movement across the grain. I agree about not using glue, I live in a super dry climate and we used a spline and joint fasteners with no glue, the joints opened a bit, but very minimal. What Thomas said about finishing your joints before is a fantastic idea.

3/31/23       #11: 1.5" Birch Butcher Block count ...
Adam

The general feeling about mitered tops is to not do them. There are occasions when you must do them to accommodate the Architect, Builder, Customer or your own personal goals.

There is a very simple way to make the miters work. You need to make the miter bomb proof. That could be a combination of splines, dominos, and a good adhesives like epoxy. Basically if you assembled you miter and left it on the work bench it would be there forever.

The trick is how you fasten it to your cabinets or table legs. You've got two options. You can either fasten one leg of the L hard to the cabinets, then fasten the other leg loose(3/4" holes with 1 1/4" fender washers) is the most fool proof way. Use a screwdriver to tighten the screws. Leave them a little loose. The counter is effectively sitting there under its own weight.

The other option is to fasten the mitered joint area (2" either side) hard to the cabinets. Then do the fender washer loose install on both of the legs. This reduces the visible movement 50% by sharing it on both legs.

You need to design the with cabinetry such that the minute movement over time is not apparent to the casual observer. Good thing is most countertops have a decent amount of overhang.

Please do not say this will not work, unless you have seen it fail. I've done this on 6 different projects over 30 years with no problems whatsoever. I would do it in my own house.

3/31/23       #12: 1.5" Birch Butcher Block count ...
Adam

For instance if you had a 4'/4' L countertop you would typically fasten the miter hard and let the ends move. If you had a 4'/8' L counter top you would fasten the 8' length hard and let the 4' leg wander with the seasons.

3/31/23       #13: 1.5" Birch Butcher Block count ...
Jeff

Adam, I am not disagreeing with you that you have done it and it worked. However what you said in your last message that you fasten the miter and let the ends float has me confused as that is not how wood moves. The majority of the movement will be in the width of the countertop, there is very minimal movement in the length of the countertop.

4/1/23       #14: 1.5" Birch Butcher Block count ...
Adam

The movement happens out at the ends of the legs. Depending on the length they will move laterally back & forth as the changes in moisture change the miter angle.

If you think about how a door casing moves throughout the seasons. When you install it the miters are tight and 45 degrees. As the moisture decreases(winter heating) the miter gaps at the bottom, which means the miter angles are 44.5. If you only nailed the header and left the legs unfastened the miter would hold(if you biscuited it) and the legs would move towards the middle of the door.

4/4/23       #15: 1.5" Birch Butcher Block count ...
Dave Edgerton  Member

Ypu dont want to glue the 2 tops together at 90 degrees, the cross gain one will rip apart if you use dominos. The wood will shink and expand at a rate of 3/32" per foot. X 2' equals just under a quarter inch if you are lucky. Spline joint, no glue, butterfly fasteners underneath.

4/6/23       #16: 1.5" Birch Butcher Block count ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com

This has worked stupid well for me


View higher quality, full size image (502 X 512)

4/6/23       #17: 1.5" Birch Butcher Block count ...
Chris Member

Wow! That is really nice. Just don't think I can do that on site, Really nice looking joinery. Can you tell how you were able to make the joint.

4/6/23       #18: 1.5" Birch Butcher Block count ...
Dave Edgerton  Member

Chris that return email did not work. Resend to me. Thanks!

4/7/23       #19: 1.5" Birch Butcher Block count ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com

Chris, I cut those on the cnc. Left and right tooling, and I made a sweet parametric program to make everything adjustable.

4/7/23       #20: 1.5" Birch Butcher Block count ...
Warren E Member

All solid other than a ply under the solid cherry. The moulding under the solid top was on the plywood.
Top was one slab then cut lamelloed and clamped well. In bolting down was bolted to the front tight. If it was going to shrink it would pull at the back. Nothing opened anywhere years down the road. Same as when it was made last time I saw it. The stuff on top of the top was just sitting for a photo but located with lamelloes then on site fastened tight from below.


View higher quality, full size image (1289 X 697)

4/8/23       #21: 1.5" Birch Butcher Block count ...
Chris Member

Hey All,
We have a Thermwood CNC, that was my first thought. Not that I was going to try a dovetail but just a way to get a clean square miter cut + cut outs for the Zipbolt fastners. Our table is 5X8 so each leg would fit. I suspect you had to clean up the Dovetail inside corners, then press the legs together, that must have been very satisfying! I would just make templates, CNC build and finish at shop then install finished product. But I am restrained due to closed "U" shape of kitchen walls. So on site, a mitered corner would be difficult to put together, a butt joint on site is do-able. Dave 's mention of using Dominoes & having issues with the ends coming apart does have me concerned. So maybe no Dominoes or glue, just a spline w/Zipbolt's... Thank you guys for the advice.


View higher quality, full size image (1766 X 944)

4/8/23       #22: 1.5" Birch Butcher Block count ...
Chris Member

This would be a butt joint + zipbolts & a spline.PIA on-site but again do-able.
Chris


View higher quality, full size image (1766 X 945)

4/8/23       #24: 1.5" Birch Butcher Block count ...
Warren E Member

for what you are doing id do the butt joint youve shown

4/8/23       #25: 1.5" Birch Butcher Block count ...
Jeff

I would be way more concerned with a sink in the butcher block than how much movement will be in the joint.
At least that looks like a sink unit.

4/8/23       #26: 1.5" Birch Butcher Block count ...
Chris Member

Yes it is a sink cut-out. Not my problem, plumber gets to deal with that. I just made an abstract cut out, I have no idea of sink size or placement Fore & Aft. Just goes in that cabinet.

4/8/23       #27: 1.5" Birch Butcher Block count ...
Chris Member

Having said that I bet they very well may ask me to do the sink cut out. Done this many times just not in 1.5" thick lumber. I would normally cut four 2" holes in the corners then skill saw the rest. I for sure will lay the polyurethane onto the edge. But I was just wondering what would be the best cutter to use for the 2" holes? Hole saw would just smoke + there not deep enough, Spade bit, I dunno I think it would tear it up, Forstner might take awhile & probably smoke it too, Auger ehh maybe just hang on :-)
Any thoughts

4/9/23       #28: 1.5" Birch Butcher Block count ...
Tom Gardiner

I template and cut the sink with the cnc. Sand and seal the cut. Overkill maybe. Give the client the sink cutout as a cutting board.
Impressed by the mitres holding together. I guess it is testament to good fit and strong glue.

9/10/23       #29: 1.5" Birch Butcher Block count ...
Chris Member

Hey All,
This job is getting close so I started looking for a festool TS75 saw, in my search I came across the Mafell KSS 60 18M bl Cordless Cross-Cutting System, with a guide extension should work for the tops. Have any of you all worked with or own one? I do wonder about the stock thin blade to make a clean 90* 1.5" crosscut.
Any thoughts about this cordless beast :-)
Thanks Again, Chris

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • VortexTool Co. Inc.
      Manufacturers of Custom Cutting Tools, and Distributors of Major Cutting Tool Brands
    • Colonial Saw
      North American Supplier of Striebig Panel Saws, Lamello Specialty Tools and a Wide Range of Saw and Tool Grinding Machinery
    • Simantech
      New & Used Machinery, Supplies, Tooling, Parts, and Abrasive Products
    • Mereen-Johnson Machine Company
      Manufacturers of High Production Woodworking Machinery
    • Carter Products
      Band Saw Guides, Blades, Wheels, Tires, Line Lasers and 2D Projectors, Wide Belt Sanding Accessories, Vacuum Holding Systems and More
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • Elias Woodwork & Manufacturing
      Solid Wood Cabinet Doors, Furniture, Dovetail Drawers, Mouldings, and Related Items
    • American National Knife
      Manufacturer of HSS and Carbide Tipped Woodworking Knife Sets for Planers, Jointers, Molders, Shapers
    • KCD Software
      Powerful 3D Cabinet/Closet Design Software with Built-In Touchscreen Mode for Mobile Use with Best Production Practices Including Direct to Cut List, Cabinotch and/or CNC Machining
    • Cabinetshop Maestro
      Web-Based Project Management Software for Custom Cabinet Shops - Manage Jobs from Prospect to Punchlist Through Scheduling, Task Management, Time Tracking and Communication
    • OMEC/Macoser Inc
      Exclusive Importer of European Woodworking Machinery Since 1988
    • Cab Parts
      Pre-manufactured Components for Easy-to-Assemble Cabinet Boxes
    • TotalFinishingSUPPLIES.com
      Solutions and supplies from spray tips to spray booths for all your woodworking needs

    Become a Sponsor today!